journal article·2024-01

Cavitation erosion resistance and tribological performance of PAI/PI/EP soft coating on 20CrMo

Xin Zhuo, Jun Cao, Haibo Huang, Li Liu, Xinkun Suo, Peiqing Ye, Zeshan Abbas

Wear· Volume 536-537
Publisher page

Abstract

A polyamide-imine/polyimide/epoxy resin polymer coating is prepared on the surface of 20CrMo steel by liquid spraying technology which is used to replace the CuPb24Sn copper alloy in valve plates for pumps. Tribological and anti-cavitation erosive experiments of the polymer coating, 20CrMo steel and CuPb24Sn copper alloy are carried out under oil, oil + seawater + silt mixed environment and seawater + silt environment. The results demonstrate that the deposition coating on 20CrMo steel can effectively replace copper alloy for the valve plate of the pump under oil lubrication, oil + seawater + silt environment. Under oil lubrication, the coating exhibits adhesive wear and its average frictional coefficient is 36.63 % and 8.57 % lower than that of the steel and copper alloy, respectively. Likewise, the coating mainly exhibits abrasive wear under the complex working conditions of seawater + silt + oil and seawater + silt. The soft coating reduces the three-body wear and the three-body frictional loss due to the embeddability. Under the complex conditions of seawater + silt + oil, the cavitation mass loss of the coating is 20 % and 35.48 % lower than that of the steel substrate and copper alloy, respectively. In addition, the cavitation mass loss of the coating is 53.6 % and 62.09 % lower than that of the steel and copper alloy under the condition of seawater + silt, respectively. The main influencing factors of the aforementioned results are the lipophilicity of the coating, the large ratio of hardness to elastic modulus (H/E) and the good corrosion resistance.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Tribology and Wear Analysis · Metal and Thin Film Mechanics · Lubricants and Their Additives

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (71)

Show source-provided references
1. In-situ fabricated bulk metallic glass/graphite composites with a 3D lubricating layer: tribological properties under dry sliding and in seawater10.1016/j.triboint.2020.106301 ↗
2. Effect of surface microtexturing on seawater-lubricated contacts under starved and fully-flooded conditions10.1016/j.triboint.2020.106339 ↗
3. 2023
4. 2023
5. Simultaneous enhancement of strength and ductility in a medium carbon low-alloy steel induced by secondary martensite and Cu-rich particles10.1016/j.msea.2023.144791 ↗
6. Microstructure and mechanical properties of annealed SUS 304H austenitic stainless steel with copper10.1016/j.msea.2011.02.019 ↗
7. Corrosion and wear properties of HVOF sprayed AlCoCrFeNi HEA coating in simulated seawater drilling fluid
8. Effect of N+ Cr ions implantation on corrosion and tribological properties in simulated seawater of carburized alloy steel10.1016/j.surfcoat.2020.125357 ↗
9. Synergetic effects of biomimetic microtexture with multi-solid lubricants to improve tribological properties of AISI 4140 steel10.1016/j.triboint.2021.107395 ↗
10. Experimental study on the influence of surface microtexture on the tribological properties of 45# steel friction pairs
11. Investigations of CrN+Cr2O3/TiO2 coatings obtained in a PVD/ALD hybrid method on austenitic 316L steel substrate10.1016/j.vacuum.2022.111653 ↗
12. Tribological performance and behaviour of CVD TiC/TiCN/TiN multilayer coating at elevated temperature10.1080/02670844.2020.1807813 ↗
13. Effects of ion nitriding on tribological performance of CrN coating by multi-arc ion plating
14. Effect of plasma carbonitriding on the high-temperature tribological properties of a TiAlCrN coating on 300M steel by multi-arc ion plating10.1080/14786435.2021.1887530 ↗
15. High temperature friction and wear performance of TiB2-50Ni composite coating sprayed by HVOF technique10.1016/j.surfcoat.2020.126766 ↗
16. Tribocorrosion behaviors of thermal spraying WC/Ni60 coated 316L stainless steel in artificial seawater10.1108/ILT-12-2017-0386 ↗
17. Effects of polymer composited lubricant coating on tribological properties of low-carbon steel surface
18. Tribological performance improvement of polyamide against steel using polymer coating10.1080/10402004.2019.1643517 ↗
19. Bubble behavior in cylindrical and square vessels under centric mechanical stirring10.1007/s42243-021-00609-y ↗
20. Observation of the formation of multiple shock waves at the collapse of cavitation bubbles for improvement of energy convergence10.3390/en15072305 ↗
21. Experimental study on the characteristics of microjets and shock waves of cavitation bubbles near elastic boundaries10.1016/j.oceaneng.2022.111664 ↗
22. Cavitation erosion mechanism of 2Cr13 stainless steel
23. Effect of WC-10Co on cavitation erosion behaviors of AlCoCrFeNi coatings prepared by HVOF spraying10.1016/j.ceramint.2021.02.070 ↗
24. Microstructure and cavitation erosion resistance of arc ion plating NiCrAlY coating on the 304L stainless steel10.1016/j.triboint.2022.107618 ↗
25. Microstructure and cavitation–silt erosion behavior of high-velocity oxygen–fuel (HVOF) sprayed Cr3C2–NiCr coating10.1016/j.surfcoat.2013.03.020 ↗
26. Slurry erosion behavior of F6NM stainless steel and high-velocity oxygen fuel-sprayed WC-10Co-4Cr coating10.1007/s11666-016-0515-4 ↗
27. WC-M coating to improve resistance of hydraulic turbines to cavitation erosion and abrasion
28. The tribological and mechanical properties of PI/PAI/EP polymer coating under oil lubrication, seawater corrosion and dry sliding wear10.3390/polym15061507 ↗
29. The investigation of microstructure and tribological properties of PTFE/PI-PAI composite coating added with VN
30. Friction and wear of PTFE—a review10.1016/0043-1648(92)90039-B ↗
31. Friction reduction of water based lubricant with highly dispersed functional MoS2 nanosheets10.1016/j.colsurfa.2018.11.047 ↗
32. Effects of Cu and WS2 addition on microstructural evolution and tribological properties of self-lubricating anti-wear coatings prepared by laser cladding10.1016/j.triboint.2021.106872 ↗
33. Effect of nano-CeO2 on microstructure and wear resistance of Co-based coatings10.1016/j.surfcoat.2015.06.014 ↗
34. Tribology of SiC ceramics under lubrication: features, developments, and perspectives10.1016/j.cossms.2022.101000 ↗
35. Dry sliding wear behavior of Al2O3/SiC particle reinforced aluminium based MMCs fabricated by stir casting method10.12693/APhysPolA.124.11 ↗
36. Friction and wear behaviors of Al‐SiC‐B4C composites produced by pressure infiltration method10.1108/00368791111155002 ↗
37. Cavitation-erosion behavior and mechanism of high-velocity oxygen-fuel sprayed CuAlNiTiSi medium-entropy alloy coating10.1016/j.surfcoat.2022.128096 ↗
38. Tribological performance of PTFE and its composite in wide temperature range
39. Cavitation bubble structures below a soft boundary in an ultrasonic field10.1016/j.ultsonch.2023.106500 ↗
40. Optical and electrical transport properties of ZnO/MoS2 heterojunction pn structure10.1016/j.matchemphys.2018.09.002 ↗
41. Structural and morphological evaluation of layered WS2 thin films10.1016/j.vacuum.2020.109570 ↗
42. Pore formation in polystyrene fiber by superimposing temperature and relative humidity of electrospinning atmosphere10.1016/j.polymer.2012.10.003 ↗
43. Relationships between hardness, Young's modulus and elastic recovery in hard nanocomposite coatings10.1016/S0257-8972(01)01714-5 ↗
44. Preparation, characterization, and applications of electrospun ultrafine fibrous PTFE porous membranes10.1016/j.memsci.2016.10.019 ↗
45. Expanded polytetrafluoroethylene/mxene nanosheet composites with hydrophilicity and lipophilicity for purification of oil spills and wastewater10.1021/acsanm.1c04166 ↗
46. Effect of oil temperature and counterpart material on the wear mechanism of ta-CNx coating under base oil lubrication10.1016/j.wear.2017.08.012 ↗
47. Effect of nano-Al2O3 surface treatment on the tribological performance of phenolic composite coating10.1016/j.surfcoat.2006.09.084 ↗
48. Wear mechanisms of a sintered tribofilm in boundary lubrication regime
49. The influence of different metallic counterparts on the tribological performance of nc-CrC/GLC in seawater10.1016/j.surfcoat.2017.07.021 ↗
50. Characterization and evolution of the coefficient of friction during pin on disc tribotest: comparison between C10200 Cu, AA6082-T6 Al and C36000 brass pins under varying normal loads10.1016/j.triboint.2019.06.013 ↗
51. Study on tribological properties of plasma thermal spraying Al2O3 coating sliding against counterparts with high hardness
52. Tribological properties of bronze–graphite composites under sea water condition10.1016/j.triboint.2012.04.023 ↗
53. Comparative tribological and corrosion resistance properties of epoxy composite coatings reinforced with functionalized fullerene C60 and graphene10.1016/j.surfcoat.2015.12.056 ↗
54. Preparation and tribological properties of polyimide/carbon sphere microcomposite films under seawater condition10.1016/j.triboint.2015.04.027 ↗
55. Enhancement of wear and friction characteristics of epoxy resin by multiwalled carbon nanotube and boron nitride nanoparticles10.1080/10402004.2014.998358 ↗
56. Study of tribological properties of polyimide/graphene oxide nanocomposite films under seawater-lubricated condition10.1016/j.triboint.2014.06.022 ↗
57. Three tribolayers self-generated from SiC individually work for reducing friction in different contact pressures10.1021/acs.jpcc.1c07668 ↗
58. Microstructure, mechanical properties and corrosion behavior of Ce doped TiN films10.1016/j.apsusc.2021.151770 ↗
59. Preparation of Ni-P-Ti3C2Tx-Ce composite coating with enhanced wear resistance and electrochemical corrosion behavior on the surface of low manganese steel10.1016/j.surfcoat.2022.128508 ↗
60. Effect of micro-texture on the friction and wear performance of copper-based self-lubricating composites
61. Fan · 2023
62. Excellent tribological and anti-corrosion performance of polyurethane composite coatings reinforced with functionalized graphene and graphene oxide nanosheets10.1039/C5RA10494G ↗
63. Galvanic corrosion performance of high-strength copper-nickel alloys in seawater10.5006/1.3319141 ↗
64. Comparison of the cavitation erosion and slurry erosion behavior of cobalt-based and nickel-based coatings10.1016/j.wear.2019.03.022 ↗
65. Cavitation erosion resistance enhancement of martensitic stainless steel via low-temperature plasma carburizing10.1016/j.wear.2019.03.009 ↗
66. Time-dependent corrosion behavior of electroless Ni–P coating in H2S/Cl− environment10.1016/j.ijhydene.2021.01.053 ↗
67. Unraveling the effects of CO2 and H2S on the corrosion behavior of electroless Ni-P coating in CO2/H2S/Cl– environments at high temperature and high pressure10.1016/j.corsci.2018.12.022 ↗
68. The coupling effect of immersion corrosion and cavitation erosion of NiCoCrAlYTa coatings in artificial seawater10.1016/j.corsci.2020.108635 ↗
69. Design of high-entropy alloy coating for cavitation erosion resistance by different energy-induced dynamic cyclic behaviors10.1021/acsami.2c19210 ↗
70. Cavitation erosion behavior of ceramic/organic coatings exposed to artificial seawater10.1016/j.surfcoat.2020.126133 ↗
71. Electrochemical noise analysis of cavitation erosion corrosion resistance of NbC nanocrystalline coating in a 3.5 wt% NaCl solution10.1016/j.surfcoat.2021.127133 ↗