journal article·2023-06

How the micro-mechanical stability of carbides in chromium-rich hardfacings influences the impact-abrasion resistance at elevated temperatures

H. Rojacz, C. Katsich, M. Varga, E. Badisch

Wear· Volume 522
Publisher page

Abstract

Abstract Highly loaded wear components in applications such as crushers or sieves suffer from combined impact and abrasive wear, in the worst case exaggerated by high operation temperatures. Hardfacings based on the system FeCrC with high hardphase content are promising candidates for such applications. Understanding of the influence of precipitated carbides or carbo-borides on the impact-abrasive wear resistance is therefore of high importance to increase the lifetime, decrease downtime as well as maintenance costs. In this study, two different FeCrC-based hardfacings were chosen for investigation, an FeCrC-alloy and a complex alloyed FeCrNbMoBC type. A thorough microstructural analysis was performed via scanning electron microscopy. Here, present hardphases, namely chromium carbides, chromium carbo-borides as well as niobium carbides were found. To evaluate the hardness H and Young’s modulus E nanoindentation measurements were performed and the plasticity indicating ratios H/E and H³/E² were derived. Scratch tests at elevated temperatures were performed identifying critical loads for carbide displacement and fracture. Those critical loads as well as the plasticity indexing parameters were correlated with the impact-abrasion behaviour of the two hardfacings via high-temperature cyclic impact abrasion tests up to 500°C. Results showed higher impact-abrasion resistance of the complex-alloyed FeCrC-based hardfacing due to better stability of the carbides as well as optimal ratios H/E and H³/E² indicating increased plasticity and thereby better impact resistance.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Metal Alloys Wear and Properties · Advanced materials and composites · Metal and Thin Film Mechanics

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (41)

Show source-provided references
1. Impact-abrasive wear resistance of high alumina ceramics and ZTA
2. Ceramic-rubber hybrid materials – a knowledge-based design concept10.1016/j.wear.2021.203735 ↗
3. Microstructure selection criteria for cast irons with more than 10 wt.% chromium for wear applications10.1016/S1044-5803(02)00260-7 ↗
4. Effects of ‘impact’ and abrasive particle size on the performance of white cast irons relative to low-alloy steels in laboratory ball mills10.1016/j.wear.2019.01.048 ↗
5. Abrasion wear of austenitic manganese steels via jaw crusher test10.1016/j.wear.2021.203726 ↗
6. The effect of retained austenite stability on impact-abrasion wear resistance in carbide-free bainitic steels10.1016/j.wear.2019.02.032 ↗
7. Role of fracture toughness in impact-abrasion wear10.1016/j.wear.2019.03.028 ↗
8. Wear mechanisms at high temperatures. Part 3: changes of the wear mechanism in the continuous impact abrasion test with increasing testing temperature10.1007/s11249-009-9534-3 ↗
9. Abdelbary · 2020
10. Stachowiak · 2005
11. Impact-abrasive wear of martensitic steels and complex iron-based hardfacing alloys
12. Influence of velocity on high-temperature fundamental abrasive contact: a numerical and experimental approach10.1016/j.wear.2018.12.013 ↗
13. Study of wear mechanisms at high temperature scratch testing10.1016/j.wear.2017.04.027 ↗
14. Microstructural changes and strain hardening effects in abrasive contacts at different relative velocities and temperatures10.1016/j.matchar.2016.05.027 ↗
15. Effect of carbide degradation in a Ni-based hardfacing under abrasive and combined impact/abrasive conditions10.1016/j.surfcoat.2011.07.064 ↗
16. Abrasive wear resistance of some commercial abrasion resistant steels evaluated by laboratory test methods10.1016/j.wear.2009.08.005 ↗
17. Wear behaviour of some low alloyed steels under combined impact-abrasion contact conditions10.1016/S0043-1648(01)00712-8 ↗
18. Surface deformation of steels in impact-abrasion: the effect of sample angle and test duration10.1016/j.wear.2013.01.006 ↗
19. Wear behaviour and wear mechanisms of different hardmetal grades in comparison with polycrystalline diamond in a new impact-abrasion test10.1016/j.ijrmhm.2020.105286 ↗
20. Mapping of impact-abrasive wear performance of WC–Co cemented carbides10.1016/j.wear.2015.02.031 ↗
21. The effect of retained austenite on the wear mechanism of bainitic ductile iron under impact load10.1016/j.jmrt.2021.01.122 ↗
22. B. Liu, W. Li, X. Lu, X. Jia, X. Jin, The effect of retained austenite stability on impact-abrasion wear resistance in carbide-free bainitic steels, Wear 428–429 (20019) 127-136.10.1016/j.wear.2019.02.032 ↗
23. Experimental setup for testing and mapping of high temperature abrasion and oxidation synergy10.1016/j.wear.2009.01.008 ↗
24. Wear mechanisms at high temperatures. Part 3: changes of the wear mechanism in the continuous impact abrasion test with increasing testing temperature10.1007/s11249-009-9534-3 ↗
25. Failure modes in scratch adhesion testing10.1016/0257-8972(91)90188-3 ↗
26. G. Pintaude, Introduction of the ratio of the hardness to the reduced elastic modulus for abrasion, in: J. Gegner (Eds.) Tribology, InTechOpen, London.
27. High temperature hardness of steels and iron-based alloys10.1016/j.msea.2016.06.058 ↗
28. Wear intensity evaluation in conveying systems–An acoustic emission and vibration measurement approach10.1016/j.triboint.2019.01.008 ↗
29. Development of impact energy distribution of various abrasives during cyclic impact/abrasion testing10.4028/www.scientific.net/SSP.267.234 ↗
30. Wear progress and mechanisms in high temperature sieves10.1016/j.engfailanal.2015.07.032 ↗
31. Wear mechanisms at high temperatures. Part 1: wear mechanisms of different Fe-based alloys at elevated temperatures10.1007/s11249-009-9421-y ↗
32. Introduction of a novel tribometer especially designed for scratch, adhesion and hardness investigation up to 1000°C
33. An improved technique for determining hardness and elastic modulus using load and displacement sensing indentation experiments10.1557/JMR.1992.1564 ↗
34. High temperature abrasive wear of metallic materials
35. M. Roy, Surface Engineering for Enhanced Performance against Wear, Springer Verlag, Berlin-Heidelberg.
36. The correlation of material characteristics and wear in a laboratory scale cone crusher10.1016/j.wear.2008.12.055 ↗
37. Roller crushers in iron mining, how does the degradation of Hadfield steel components occur?10.1016/j.engfailanal.2021.105295 ↗
38. Hammer premature wear in mineral crushing process10.1016/j.triboint.2017.06.025 ↗
39. Influence of welding current on carbide/matrix interface properties10.1016/j.jmatprotec.2009.10.001 ↗
40. Study on the cavitation erosion behavior of hardfacing alloys for nuclear power industry10.1016/S0043-1648(03)00144-3 ↗
41. Li · 2020