Effects of materials and solution temperatures on cavitation erosion of pure titanium and titanium alloy in seawater
Source abstract
Abstract
Abstract Cavitation erosion was studied for various pure titanium and titanium alloy samples using a rotating disk method in seawater at 303, 318, and 333 K. Their respective erosion resistances were evaluated in terms of Vickers hardness (HV). The resistance increased in order with increasing hardness: pure titanium samples of first, second, and third types, and titanium alloy (Ti–6Al–4V). The relative temperature was defined as 273 K for freezing temperature and 373 K for boiling temperature under pressurized water. The volume loss rate of test specimens increased with rising seawater temperature of 289–316 K of the relative temperature, as well as in cases using cavitating liquid jet and vibratory apparatuses.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Ultrasound and Cavitation Phenomena · Cavitation Phenomena in Pumps · Erosion and Abrasive Machining
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (10)
Show source-provided references
1. Novel development of material strength evaluation and new material application
2. Cavitation erosion of titanium alloy
3. Estimation of cavitation damage in seawater by a cavitating jet method
4. Katou · 1999
5. Influence of temperature on erosion by a cavitating liquid jet10.1016/j.wear.2005.08.001 ↗
6. Cavitation damage study with a rotating disk at the high peripheral velocities10.1080/00221689209498898 ↗
7. Titanium and corrosion prevention
8. Sverdrup · 1961
9. Evolution process of intense cavitation erosion in centrifugal pump
10. Temperature effects in cavitation damage10.1115/1.3425484 ↗