Scuffing behavior of 390 aluminum against steel under starved lubrication conditions
Source abstract
Abstract
Abstract The scuffing characteristics of 390-T6 aluminum–silicon alloy sliding against 52100 steel are examined under starved lubrication conditions. The evaluation is based on a shoe-on-disc geometry which simulates the plate/shoe contacts in an automotive air conditioning swashplate compressor. Four shoe geometries (flat shoe, crowned shoe, crowned shoe with a dimple at the center and crowned shoe with a groove) are tested against 390-T6 aluminum discs. All tests are conducted in a high-pressure tribometer (HPT) under R134a (tetrafluoroethane) environment with a base polyalkylene glycol (PAG) lubricant. The effects of degree of lubricant starvation, sliding velocity, geometry of contact, surface topography, and a tin coating on scuffing are evaluated. It is hypothesized that scuffing of 390-T6 Al alloy under starved lubrication conditions is due to macroscopic adhesions leading to plastic shearing of the bulk material.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Adhesion, Friction, and Surface Interactions · Mechanical stress and fatigue analysis · Brake Systems and Friction Analysis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (17)
Show source-provided references
1. Scuffing — a review10.1016/0301-679X(75)90056-0 ↗
2. Scuffing — a review10.1016/0301-679X(75)90029-8 ↗
3. Wear of aluminum–silicon alloys10.1016/0043-1648(75)90167-2 ↗
4. Wear characteristics of Al–Si alloys10.1016/0043-1648(94)90298-4 ↗
5. Friction and wear of Al–Si alloys
6. J. Ferrante, W. A. Brainard, Wear of aluminum and hypoeutectic aluminum–silicon alloys in boundary lubricated pin-on-disk sliding, NASA Technical Paper 1442 (1979).
7. Influences of silicon content and grain size of primary silicon crystals on the wear of high silicon aluminum alloys
8. Wear in Al–Si alloys under dry sliding conditions10.1016/0043-1648(87)90102-5 ↗
9. Wear and scuff resistance of aluminum 390
10. Wear and seizure of binary Al–Si alloys10.1016/0043-1648(94)90354-9 ↗
11. Mechanism of seizure of aluminum–silicon alloys dry sliding against steel10.1016/0043-1648(95)90182-5 ↗
12. Scuffing under dry sliding conditions: I. Experimental studies10.1080/10402009808983768 ↗
13. Scuffing under dry sliding conditions: II. Theoretical studies10.1080/10402009808983769 ↗
14. T.K. Sheiretov, Scuffing of aluminum/steel contacts under dry sliding conditions, PhD Thesis, Department of Mechanical and Industrial Engineering, University of Illinois at Urbana-Champaign, 1997.
15. A review of scuffing and running-in of lubricated surfaces, with asperities and oxides in perspective10.1016/0043-1648(84)90019-X ↗
16. W.L. Brown, Development of piston-ring coatings, SAE Technical Paper 690754 (1969).
17. Seizure failure of copper–lead with overlay and aluminum–tin connecting rod bearings10.1080/10402009608983520 ↗