Corrosion–erosion behavior of TiN-coated stainless steels in aqueous slurries
Source abstract
Abstract
Abstract The corrosion–erosion resistance of TiN-coated AISI 304 and AISI 420 stainless steels in aqueous slurries was studied. TiN films with a thickness of 0.6 μm were obtained by using the pulsed-arc plasma-assisted physical vapour deposition technique. The corrosion–erosion experiments were performed in a test machine in which the impingement velocity, impact angle, concentration of solids and pH of the solution were controlled. Polarization curves were simultaneously obtained to relate the electrochemical effects to the erosive wear mechanisms. The slurry used consists of quartz particles suspended in a mixture of sulphuric acid solution and 3.5% NaCl, with a pH value of 0.2. Measurement of critical and passive current densities showed that the behavior of coated materials differed according to substrate, but in a general way increasing impact velocity and changing from normal to grazing incidence led to a reduction in resistance to corrosion–erosion and liquid impingement corrosion. Surface analysis by SEM revealed formation of cracks in the coating and plastic deformation in both the substrate and the coating, especially when the mean impact velocity exceeded a critical value between 6.9 and 8.6 ms−1. Additionally, intergranular corrosion was observed in some specimens.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Erosion and Abrasive Machining · Metal and Thin Film Mechanics · Diamond and Carbon-based Materials Research
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (14)
Show source-provided references
1. Corrosion–erosion of nitrogen bearing martensitic stainless steels in seawater-quartz slurry10.1016/S0043-1648(01)00765-7 ↗
2. Erosion of steels in liquid slurries10.1016/0043-1648(84)90225-4 ↗
3. TiN coatings for protection against combined wear and oxidation10.1179/sur.1992.8.1.47 ↗
4. Erosion of PVD TiN coatings under simultaneous corrosion in sodium carbonate/bicarbonate buffer slurries containing alumina particles10.1016/S0257-8972(98)00463-0 ↗
5. Control of the corrosion resistance of TiN coated AISI 304 stainless steel10.1016/S0010-938X(97)81156-0 ↗
6. Microstructures of TiN films grown by various physical vapour deposition techniques10.1016/0257-8972(91)90128-J ↗
7. Review of cathodic arc deposition technology at the start of the new millennium10.1016/S0257-8972(00)00879-3 ↗
8. The corrosion resistance and wear resistance of thick TiN coatings deposited by arc ion plating10.1016/S0257-8972(01)01284-1 ↗
9. Slurry erosion characteristic of TiN coatings on Ti and plasma nitrided Ti alloy substrates10.1016/S0257-8972(99)00301-1 ↗
10. Impact angle, particle energy and mass loss in erosion by dilute slurries10.1016/0043-1648(95)07120-2 ↗
11. L. Prandtl, Guide a travers de la mécanique des fluides, Paris, 1952.
12. The influence of substrate material on the erosion resistance of TiN coated tool steels10.1016/0043-1648(95)07163-6 ↗
13. Effects of surface deformation on corrosive wear of stainless steel in sulfuric acid solution10.1016/S0043-1648(99)00019-8 ↗
14. The mechanochemical behavior of type 316L stainless steel10.1016/0010-938X(96)00008-X ↗