Roughening of metallic biomaterials by abrasiveless waterjet peening: Characterization and viability

S. Barriuso, M. Lieblich, M. Multigner, I. Etxeberria, A. Alberdi, J.L. González-Carrasco

Wear· Volume 270· Issue 9-10
Publisher page

Abstract

This study addresses the roughening of AISI 316 LVM and Ti6Al4V by waterjet peening (WJP) without abrasive particles, looking for rough surfaces free of embedded particles that could act as severe notches. Strong parameters have been selected to characterize and check viability of abrasiveless WJP; a water pressure of 360. MPa and two slow traverse velocities: 0.05 and 0.1. m/min. After processing, large number of pits with undercuts plus some larger intrusions are observed, which are more abundant and larger in the steel specimens and in those treated with the lower traverse speed. Cross sectional examination of 316 LVM reveals a significant grain size refinement in the subsurface zone, 10-20. μm wide, that exhibits a submicrometric/nanometric grain size, accompanied with a hardness gradient (50% increase) that extends to a depth of up to about 100. μm. The analysis of the magnetic hysteresis loops discards the presence of strain induced α-martensite. No hardness or microstructural gradient was developed in the Ti6Al4V alloy. The results indicate that in AISI 316 LVM the volume loss occurs through hardening of the subsurface, embrittlement, crack formation and erosion. In Ti6Al4V the material removal may take place first at the vanadium reach β-phase. © 2011 Elsevier B.V.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Surface Treatment and Residual Stress · Erosion and Abrasive Machining · High-Velocity Impact and Material Behavior

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (34)

Show source-provided references
1. Bone tissue response to commercially pure titanium implants blasted with fine and coarse particles of aluminium oxide
2. Biology of grit blasted implants
3. Osseointegration of grit-blasted and bioactive titanium implants: histomorphometry in minipigs10.4028/www.scientific.net/KEM.254-256.737 ↗
4. Fatigue and cyclic deformation behaviour of surface-modified titanium alloys in simulated physiological media10.1016/j.biomaterials.2005.08.012 ↗
5. Influencia del arenado de la aleación Ti6Al4V en la dureza subsuperficial y estado de tensiones residuales10.3989/revmetalm.0803 ↗
6. Mechanical surface treatments on titanium, aluminium and magnesium alloys10.1016/S0921-5093(98)01168-X ↗
7. Influence of the sandblasting on the subsurface microstructure of 316LVM stainless steel: implications on the magnetic and mechanical properties10.1016/j.msec.2008.11.002 ↗
8. The effect of sandblasting treatment on endurance properties of titanium alloy hip prostheses10.1046/j.1525-1594.2000.06486.x ↗
9. The effect of shot blasting and heat treatment on the fatigue behavior of titanium for dental implant applications10.1016/j.dental.2006.03.003 ↗
10. Peening by the use of cavitation impacts for the improvement of fatigue strength10.1023/A:1010947528358 ↗
11. Interrogations on the sub-surface strain hardening of grit blasted Ti–6Al–4V alloy10.1016/j.surfcoat.2009.02.003 ↗
12. L.L. VanKuiken, L.E. Byrnes, M.S. Kramer, High Pressure Water Jet Method of Blasting Low Density Metallic Surfaces, USA Patent No. 5,380,564, January 10, 1995.
13. Surface roughening of metallic substrates by high pressure pure waterjet10.1016/0257-8972(95)02528-6 ↗
14. Waterjet roughened surface analysis and bond strength10.1016/S0257-8972(96)02995-7 ↗
15. A novel approach for modelling of water jet peening10.1016/j.ijmachtools.2004.01.010 ↗
16. High-pressure water peening – a new mechanical surface-strengthening process10.1016/S0007-8506(07)60787-2 ↗
17. Abrasive waterjet peening: a new method of surface preparation for metal orthopedic implants10.1002/1097-4636(200009)53:5<536::AID-JBM13>3.0.CO;2-V ↗
18. Waterjet and abrasive waterjet surface treatment of titanium: a comparison of surface texture and residual stress10.1016/S0043-1648(01)00826-2 ↗
19. Improving fatigue strength of metals using abrasive waterjet peening10.1080/10910340600710105 ↗
20. The effect of particle hardness and shape when abrasive water jet milling titanium alloy Ti6Al4V10.1016/j.wear.2008.06.013 ↗
21. Abrasive water-jet controlled depth milling of Ti–6Al–4V alloy – an investigation of the role of jet-workpiece traverse speed and abrasive grit size on the characteristics of the milled material10.1016/j.jmatprotec.2004.07.069 ↗
22. Surface profiling of low-carbon steel with supersonic waterjets10.1016/S0043-1648(01)00699-8 ↗
23. Effects of materials and solution temperatures on cavitation erosion of pure titanium and titanium alloy in seawater10.1016/j.wear.2006.06.011 ↗
24. Abrasive waterjet peening with elastic prestress: a parametric evaluation10.1016/j.ijmachtools.2008.10.001 ↗
25. Boller · 1987
26. Strain hardening and plastic instability properties of austenitic stainless steel after proton and neutron irradiation10.1016/S0022-3115(01)00651-1 ↗
27. Compressive residual stress into titanium alloy using cavitation shotless peening method10.1023/B:TRIL.0000044497.45014.f2 ↗
28. Fretting fatigue behavior of cavitation shotless peened Ti–6Al–4V10.1007/s11249-009-9463-1 ↗
29. Local nanocrystallization in a Cr–Mn–N austenitic stainless steel caused by cavitation
30. Investigation of water cavitation peening-induced microstructures in the near-surface layer of pure titanium10.1016/j.jmatprotec.2008.12.006 ↗
31. Characterization of a water peening process10.1115/1.2812383 ↗
32. Cavitation erosion of titanium alloys
33. Effect of waterjet formation on surface preparation and profiling of aluminum alloy10.1016/j.wear.2007.09.008 ↗
34. Hydrodynamic profiling and grit blasting of low-carbon steel surfaces10.1016/S0301-679X(02)00009-9 ↗