journal article·2005-07

Wear of cast metal–metal pairs for total replacement hip prostheses

M.A.L. Hernández-Rodríguez, R.D. Mercado-Solís, A.J. Pérez-Unzueta, D.I. Martinez-Delgado, M. Cantú-Sifuentes

Wear· Volume 259· Issue 7-12
Publisher page

Abstract

Abstract The first metal–metal prostheses were implanted during the 1960s decade. Many of these implants showed unsatisfactory short-term results due to poor designs and inappropriate manufacturing methods leading to high friction and wear. However, in the cases where the implants lasted for 20 years or longer, it was found that they exhibited a highly polished surface finish, very small changes in dimensions and low wear rates. These findings brought a revival for the metal–metal implants, which at that time, were being progressively taken over by the metal–polymer, metal–ceramic and ceramic–ceramic pair materials. The present work evaluates the influence of dimensional and microstructural parameters upon the wear behaviour of metal–metal hip implants of a Co–Cr cast alloy by means of laboratory simulation. A total of 10 pairs (acetabular cup and femoral hemisphere) were manufactured with varying diametral clearances, carbon content (0.21 and 0.31 wt.%), and microstructures (as-cast, partial and complete carbide solutions) achieved by heat treatment. The pair specimens were subsequently tested in a newly developed hip simulator under severe reciprocating sliding conditions at a frequency of 1.5 Hz, a constant load of 2 kN and bovine serum solution as lubricant. It was found that pair specimens with large diametral clearances exhibited higher amounts of wear compared to those samples with smaller diametral clearances. In terms of microstructural parameters and carbon content, pair specimens with the as-cast and partial solution microstructures (with carbide volume fractions of about 10%) exhibited less amounts of wear than those with complete carbide solution microstructures (with carbide volume fractions of about 5%). This implies that a higher content of carbon enhances wear resistance only if the carbon is precipitated as carbides and not as solution within the matrix.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Orthopaedic implants and arthroplasty · Advanced materials and composites · Orthopedic Infections and Treatments

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (19)

Show source-provided references
1. The wear of metal-on-metal total hip prostheses measured in a hip simulator10.1243/0954411011536118 ↗
2. Metal on metal bearing in hip arthroplasty10.1097/00003086-199608001-00003 ↗
3. Total hip replacement- past, present and future10.1016/0142-9612(82)90001-1 ↗
4. The tribology (friction, lubrication and wear) of all metal artificial hip joints10.1016/0043-1648(71)90032-9 ↗
5. 20 years result of McKee-Farrar vs. Charnley prosthesis10.1097/00003086-199608001-00006 ↗
6. Experience with metasul total hip bearing system10.1097/00003086-199608001-00007 ↗
7. A comparative study of total hip replacement prostheses10.1016/0021-9290(73)90052-3 ↗
8. Observation of the long term behaviour of retrieved McKee-Farrar total hip replacements implants
9. Wear of retrieved metal-metal implants after two decades of clinical use
10. In vivo wear of three types of metal on metal hip prostheses during two decades of use10.1097/00003086-199608001-00013 ↗
11. Cobalt Chromium molybdenum metal combinations for modular hip prostheses10.1097/00003086-199608001-00004 ↗
12. Estimation of wear in total hip replacement using a ten station hip simulator10.1243/PIME_PROC_1996_210_411_02 ↗
13. German clinical results with metasul bearings
14. The effect of radial clearance on lubrication in a metal on metal joint tested in a hip simulator
15. Direct experimental evidence of lubrication in metal-on-metal total hip replacement tested in a joint simulator10.1243/0954406001522822 ↗
16. Elastohydrodynamic lubrication and wear of metal-on-metal hip implants
17. Elastohydrodynamic lubrication analysis of metal-on-metal hip resurfacing prostheses10.1016/S0021-9290(02)00422-0 ↗
18. F75-98 Standard Specification for Cobalt-28 Chromium-6 Molybdenum Casting Alloy and Cast Products for Surgical Implants (UNS R30075). ASTM Book of standards, vol. 13.01, September 2001.
19. Tribochemical reaction on metal-on-metal hip joint bearings: a comparison between in-vitro and in-vivo results10.1016/S0043-1648(03)00127-3 ↗