journal article·2014-09

The relationship between flake graphite orientation, smearing effect, and closing tendency under abrasive wear conditions

Rohollah Ghasemi, Lennart Elmquist

Wear· Volume 317· Issue 1-2
Publisher page

Abstract

Plastic deformation of the matrix during the wear process results in closing the graphite flakes. In this study, the relationship between the deformation of the matrix and the closing tendency of flake graphite was investigated, both qualitatively and quantitatively. Two representative piston rings, which belonged to the same two-stroke marine engine but were operated for different periods of time, were studied. Initial microstructural observations indicated a uniform distribution of graphite flakes on unworn surfaces, whereas worn surfaces demonstrated a tendency towards a preferred orientation. Approximately 40% of the open flakes of the unworn surfaces were closed during sliding, which may result in the deterioration of the self-lubricating capability of cast iron. Moreover, flakes within the orientation range of 0 to 30° relative to the sliding direction showed a maximum closing tendency when subjected to sliding. The closing tendency gradually decreased as the angle increased, approaching a minimum between 30 and 70°. A slight increase in the closing tendency was observed for flakes with orientations between 70 and 90°. A similar trend was observed on both rings. Furthermore, SEM and EDS analysis indicated substantial deformation of the matrix in the area around the flakes. An insignificant corrosion attack was observed on both worn piston ring surfaces.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Mechanical stress and fatigue analysis · Metal Alloys Wear and Properties · Tribology and Wear Analysis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (35)

Show source-provided references
1. Eyre · 1992 · 695
2. Wear characteristics of metals10.1016/0301-679X(76)90077-3 ↗
3. R.R. Fessler, G.R. Fenske, Multiyear Program Plan: Reducing Friction and Wear in Heavy Vehicles, 1999.10.2172/771210 ↗
4. Influence of chemical composition and microstructure of gray cast iron on wear of heavy duty diesel engines cylinder liners10.1016/j.wear.2007.01.091 ↗
5. B. Koppers Company. American Hammered Piston Ring Division, Engineers’ Piston Ring Handbook: A Practical Manual of Piston Ring Types, Specifications and Applications for Designers and Operators, 1941.
6. Cylinder liner wear in low speed diesel engines10.1016/0301-679X(78)90056-7 ↗
7. The influence of acid strength on the corrosive wear of grey cast irons in oil–sulfuric acid mixtures10.1016/0043-1648(88)90019-1 ↗
8. Wear in cylinder liners10.1016/0043-1648(83)90072-8 ↗
9. Glaeser · 1992
10. The effect of cast iron graphites on friction and wear performance I: Graphite film formation on grey cast iron surfaces10.1016/0043-1648(81)90115-0 ↗
11. On a multi-process wear model
12. Development of a methodology to predict cylinder liner scuffing in the 6V92TA engine lubricant10.1080/10402009908982208 ↗
13. The effect of cast iron graphite on friction and wear performance III: The lubricating effect of graphite under rolling–sliding contacts10.1016/0043-1648(82)90102-8 ↗
14. Wear characteristics of flake and nodular graphite cast iron10.1016/0043-1648(69)90247-6 ↗
15. Run-in and glaze formation on gray cast iron surfaces10.1016/0043-1648(69)90340-8 ↗
16. The mild wear mechanism of nodular iron10.1016/0043-1648(69)90255-5 ↗
17. Wear map for grey cast iron10.1016/S0043-1648(03)00100-5 ↗
18. Sliding wear response of a cast iron under varying test environments and traversal speed and pressure conditions10.1016/j.wear.2005.09.017 ↗
19. Wear behavior of alloyed hypereutectic gray cast iron10.1016/j.triboint.2009.10.004 ↗
20. The mechanism of changes in the surface layer of grey cast iron automotive brake disc10.1590/S1516-14392005000400020 ↗
21. Woodyard · 2009
22. Operational evaluation of piston ring wear in large marine diesel engines
23. Jackson · 1978
24. C.H. Jones, Marine fuels and international standards, in: Marine Fuels: A Symposium, ASTM International (1985).10.1520/STP878-EB ↗
25. Characterization and simulation of wear occurring in the cylinder bore of the internal combustion engine10.1016/0301-679X(90)90066-X ↗
26. Metallographic characterisation of transformation phases on scuffed cast-iron diesel engine components10.1016/S0041-2678(69)80249-6 ↗
27. Effect of phosphide and matrix microstructures on the dry sliding wear of grey cast iron10.1016/0301-679X(89)90084-4 ↗
28. The break-in stage of cylinder-ring wear: a correlation between fired engines and a laboratory simulator10.1016/0043-1648(87)90005-6 ↗
29. Stefanescu · 1990 · 100
30. Tribological characteristics of aluminum-50 vol pct graphite composite10.1007/BF02669612 ↗
31. Influence of grit size on the groove formation during sliding abrasion10.1016/0043-1648(68)90559-0 ↗
32. Zum Gahr · 1987
33. Sliding wear response of cast iron as influenced by microstructural features and test condition10.1016/j.msea.2006.12.009 ↗
34. Lubricating durability of two GF category engine oils10.1108/00368790510601725 ↗
35. Friction and wear performance of copper–graphite surface composites fabricated by friction stir processing (FSP)10.1016/j.wear.2013.04.023 ↗