High strain deformation of austenitic steel for enhancing erosion resistance
Source abstract
Abstract
Abstract Marine and off-shore components including propellers, pumps, valves, pipelines and other submerged surfaces are subjected to severe degradation by erosion. Impingement of solid particles mixed in a liquid, referred as slurry, leads to significant material loss and shortens the life span of components. Tailoring the surface properties of materials is an economical way for addressing their degradation. Surface modification through high strain-rate deformation is widely used to enhance functional properties of materials. However, surface modification, particularly at low temperature, is extremely challenging for high strength materials such as stainless steel and has not been investigated comprehensively so far. In the present work, high strain-rate deformation of austenitic steel, SS316L, was performed by innovative submerged friction stir processing technique. For comparative studies, friction stir processing was also performed under ambient cooling conditions. Electron back scatter diffraction studies showed significant grain refinement for the sample processed under submerged conditions. The erosion behavior of as-received and processed steel was investigated using slurry erosion tests. Erosion tests were performed at constant impact velocity of 20 m/s and particle size, while varying the impingement angles. The sample processed under submerged conditions showed nearly two times higher erosion resistance compared to as-received steel. The enhancement in erosion resistance is explained using structural rejuvenation achieved at high strain-rate deformation. All the samples showed similar erosion mechanisms with micro-cutting and ploughing being evident at acute angles and platelet mechanism at normal impingement angle. Erosion phenomena showed a strong correlation with material's hardness at oblique impingement angle while, erosion behavior at normal impingement is explained by the flow work given as hardness to elastic modulus ratio. The study provides fundamental insights into material design for advanced structural applications.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Erosion and Abrasive Machining · Advanced materials and composites · High-Temperature Coating Behaviors
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (43)
Show source-provided references
1. Fundamentals of fluid motion in erosion by solid particle impact10.1016/0142-727X(90)90036-B ↗
2. Erosion of hard surface coatings for use in offshore gate valves10.1016/j.wear.2004.03.035 ↗
3. Corrosion and synergy in a WCCoCr HVOF thermal spray coating—understanding their role in erosion–corrosion degradation10.1016/j.wear.2004.12.003 ↗
4. Wear and corrosion behaviour of thermally sprayed cermet coatings10.1016/S0257-8972(00)01141-5 ↗
5. Slurry erosion performance of Ni-Al2O3 based thermal-sprayed coatings: effect of angle of impingement10.1007/s11666-013-0013-x ↗
6. Zirconium based bulk metallic glass—better resistance to slurry erosion compared to hydroturbine steel10.1016/j.wear.2013.08.016 ↗
7. Friction stir welding and processing10.1016/j.mser.2005.07.001 ↗
8. Effects of friction stir processing on mechanical properties of the cast aluminum alloys A319 and A35610.1016/j.scriptamat.2005.03.040 ↗
9. Producing nanograined microstructure in Mg–Al–Zn alloy by two-step friction stir processing10.1016/j.scriptamat.2008.04.003 ↗
10. Enhancing the high-cycle fatigue strength of Mg–9Al–1Zn casting by friction stir processing10.1016/j.scriptamat.2009.05.023 ↗
11. Microstructure-property relationship for friction stir processed magnesium alloy
12. Tribological enhancement of AISI 420 martensitic stainless steel through friction-stir processing10.1016/j.wear.2013.01.007 ↗
13. Improvement of cavitation erosion resistance of a duplex stainless steel through friction stir processing (FSP)10.1016/j.wear.2012.10.005 ↗
14. Cavitation erosion of stainless steels10.1016/0043-1648(82)90278-2 ↗
15. Cavitation resistance, microstructure and surface topography of materials used for hydraulic components10.1016/j.triboint.2010.05.009 ↗
16. Cavitation erosion of sensitized UNS S31803 duplex stainless steels10.1007/s11665-016-2045-0 ↗
17. Corrosion and cavitation erosion behaviors of friction stir processed Ni-Al bronze: effect of processing parameters and position in the stirred zone10.5006/1070 ↗
18. Surface modification of hydroturbine steel using friction stir processing10.1016/j.apsusc.2013.01.006 ↗
19. Improvement in cavitation erosion resistance of AISI 316L stainless steel by friction stir processing10.1016/j.apsusc.2014.04.132 ↗
20. Improving erosion resistance of hydroturbine steel using friction stir processing10.1115/1.4027622 ↗
21. Prediction of the resistance of metals to erosion by solid particles10.1016/0043-1648(75)90084-8 ↗
22. Relationship between grain size and Zener–Holloman parameter during friction stir processing in AZ31 Mg alloys10.1016/j.scriptamat.2004.05.043 ↗
23. Effect of strain rate upon plastic flow of steel10.1063/1.1707363 ↗
24. High strain rate superplasticity in continuous cast Al–Mg alloys prepared via friction stir processing10.1016/j.scriptamat.2009.01.030 ↗
25. High strain rate superplasticity in a commercial 2024 Al alloy via friction stir processing10.1016/S0921-5093(03)00367-8 ↗
26. Continuous recrystallization in austenitic stainless steel after large strain deformation10.1016/S1359-6454(02)00013-7 ↗
27. Callister · 2007
28. Determination of elastoplastic properties by instrumented sharp indentation10.1016/S1359-6462(99)00011-1 ↗
29. Strength and ductility of ultrafine grained aluminum and iron produced by ARB and annealing10.1016/S1359-6462(02)00282-8 ↗
30. Wear-mode mapping for the micro-scale abrasion test10.1016/S0043-1648(03)00073-5 ↗
31. Effect of particle velocity and impact angle on the corrosion–erosion of AISI 304 and AISI 420 stainless steels10.1016/j.wear.2005.02.032 ↗
32. The martensitic transformation and strain-hardening behavior of austenitic steels during fatigue and tensile loading10.1007/s11837-014-0909-z ↗
33. The erosion of heat-treated steels10.1016/0043-1648(83)90107-2 ↗
34. The effect of stacking fault energy on the erosion behaviour of copper alloys at oblique impact10.1016/0043-1648(85)90129-2 ↗
35. Correlation of cavitation erosion behavior with mechanical properties of metals10.1016/0043-1648(90)90122-Q ↗
36. Erosion of work-hardened copper, nickel, and 304 stainless steel10.1016/0043-1648(91)90125-E ↗
37. Hutchings · 1992
38. Contact of nominally flat surfaces, proceedings of the royal society of London A: mathematical10.1098/rspa.1966.0242 ↗
39. Contact mechanics of rough surfaces in tribology: multiple asperity contact10.1023/A:1019186601445 ↗
40. Elastic deformation and the laws of friction, proceedings of the royal society of London A: mathematical10.1098/rspa.1957.0214 ↗
41. Some thoughts on the effect of elastic rebounds on the boundaries of the aqueous erosion-corrosion map10.1016/S0043-1648(97)00243-3 ↗
42. A method for optimizing the particle flux in erosion testing with a gas-blast apparatus10.1016/0043-1648(94)90099-X ↗
43. Interplay between erodent concentration and impingement angle for erosion in dilute water–sand flows10.1016/j.wear.2015.02.039 ↗