journal article·2019-02

Cavitation erosion behavior of Hastelloy™ C-276 weld by laser welding

Dongsheng Chai, Guangyi Ma, Siyu Zhou, Zhuji Jin, Dongjiang Wu

Wear· Volume 420-421
Publisher page

Abstract

Abstract Ni-based Hastelloy C-276 was chosen as the material of the stator and rotor cans of a nuclear main pump for its excellent resistance to corrosive environments and superior mechanical properties. In the present work, the cavitation erosion (CE) behavior of the Hastelloy C-276 thin sheet weld joint was tested. The results indicate that both the CE damages of the weld metal and the base metal initiate at grain boundaries preferentially. The solidification grain boundaries (SGBs) of the weld metal and the twin boundaries (TBs) of the base metal are more susceptible to CE. For the weld metal, due to the microstructure inhomogeneity, regions that show the highest damage intensity are located near the central line of the weld surface where the columnar dendrites interact with the nearly equiaxed dendrites. For the base metal, grains with more TBs are damaged faster compare to other grains. The surface roughness of the eroded surfaces increases with exposure time, and the surface roughness of the base metal increases faster than that of the weld metal. Overall, the resistance to CE of the weld metal is better than that of the base metal.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: High-Temperature Coating Behaviors · Nuclear Materials and Properties · Hydrogen embrittlement and corrosion behaviors in metals

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (34)

Show source-provided references
1. corrosion behavior of Hastelloy C-276 in supercritical water10.1016/j.corsci.2009.05.041 ↗
2. Improvement of wear resistance of Hastelloy C-276 Through laser surface melting10.1016/j.matdes.2012.10.024 ↗
3. A study on surface topography in cavitation erosion tests of AlSi10Mg10.1016/j.triboint.2016.06.007 ↗
4. Quantitative CLSM roughness study on early cavitation-erosion damage10.1016/S0043-1648(02)00003-0 ↗
5. Mesoscale plasticity anisotropy at the earliest stages of cavitation-erosion damage of a high nitrogen austenitic stainless steel10.1016/j.wear.2008.12.079 ↗
6. Influence of grain orientation on the local deformation mode induced by cavitation erosion in a CuSnNi alloy10.1016/j.wear.2014.04.010 ↗
7. Cavitation wear behaviour of austenitic stainless steels with different grain sizes10.1016/j.wear.2004.03.024 ↗
8. A comparison of the cavitation erosion resistance of TiNi alloys, SUS304 stainless steel and Ni-based self-fluxing alloy10.1016/S0043-1648(00)00443-9 ↗
9. Damage mechanism of cavitation erosion in austenite→martensite phase transformable Fe–Cr–C–Mn/Ni alloys10.1016/j.wear.2013.12.015 ↗
10. Effects of Ni and Mn on the cavitation erosion resistance of Fe–Cr–C–Ni/Mn austenitic alloys10.1007/s11249-013-0231-x ↗
11. Enhancement of cavitation erosion resistance of 316 L stainless steel by adding molybdenum10.1016/j.ultsonch.2016.10.015 ↗
12. Improvement of the cavitation erosion resistance of an AISI 304L austenitic stainless steel by high temperature gas nitriding10.1016/j.msea.2004.05.003 ↗
13. Comparison of Inconel 625 and Inconel 600 in resistance to cavitation erosion and jet impingement erosion10.1016/j.nucengdes.2010.07.021 ↗
14. Cavitation erosion behavior of Hastelloy C-276 nickel-based alloy10.1016/j.jallcom.2014.08.248 ↗
15. Cavitation erosion and corrosion behavior of copper–manganese–aluminum alloy weldment
16. Cavitation erosion behavior of as-welded Cu12Mn8Al3Fe2Ni alloy10.1179/026708301225000761 ↗
17. Ultrasonic cavitation erosion of 316L steel weld joint in liquid Pb-Bi eutectic alloy at 550 °C10.1016/j.ultsonch.2017.03.038 ↗
18. Pulsed laser welding of Hastelloy C-276: high-temperature mechanical properties and microstructure10.1080/10426914.2012.736652 ↗
19. The effects of pulse parameters on weld geometry and microstructure of a pulsed laser welding Ni-base alloy thin sheet with filler wire10.3390/met6100237 ↗
20. ASTM G32-10, Standard Test Method for Cavitation Erosion Using Vibratory Apparatus. ASTM, 2010.
21. Experimental study and analytical model of the cavitation ring region with small diameter ultrasonic horn10.1016/j.ultsonch.2009.12.006 ↗
22. Cavitation damage: theory and measurements–a review10.1016/j.wear.2016.12.009 ↗
23. An investigation of the tribological behaviour of a high-nitrogen CrMn austenitic stainless steel10.1016/S0043-1648(97)00273-1 ↗
24. Damages on steel surface at the incubation stage of the vibration cavitation erosion in water
25. Tensile properties of weld joint on thin Hastelloy C-276 sheet of pulsed laser welding
26. Effect of annealing twins on Hall–Petch relation in polycrystalline materials10.1016/j.msea.2003.09.100 ↗
27. Improving the weldability and service performance of nickel-and iron-based superalloys by grain boundary engineering[J]10.1007/s11661-998-0214-y ↗
28. C. Stein, S. Lee, A. Rollett. An analysis of fatigue crack initiation using 2D orientation mapping and full-field simulation of elastic stress response. Superalloys 2012: 12th International Symposium on Superalloys, pp. 439–444.10.1002/9781118516430.ch48 ↗
29. Crystallographic fatigue crack initiation in nickel-based superalloy René 88DT at elevated temperature10.1016/j.actamat.2009.08.022 ↗
30. Microstructural extremes and the transition from fatigue crack initiation to small crack growth in a polycrystalline nickel-base superalloy10.1016/j.actamat.2012.01.049 ↗
31. A. Cerrone, A. Spear, J. Tucker, C. Stein, A. Rollett, A. Ingraffea, Modeling crack nucleation at coherent twin boundaries in nickel-based superalloys. Montreal, Materials Science and Technology Conference and Exhibition, 164, 2013.
32. Fatigue crack initiation, slip localization and twin boundaries in a nickel-based superalloy10.1016/j.cossms.2014.06.001 ↗
33. High resolution mapping of strain localization near twin boundaries in a nickel-based superalloy10.1016/j.actamat.2015.07.016 ↗
34. Slip transfer and plastic strain accumulation across grain boundaries in Hastelloy X10.1016/j.jmps.2012.02.001 ↗