journal article·2017-06

Scale adhesion, scratch and fracture behaviour of different oxides formed on iron based alloys at 700 °C

H. Rojacz, F. Birkelbach, L. Widder, M. Varga

Wear· Volume 380-381
Publisher page

Abstract

Abstract The influence of different alloying elements in ferrous alloys on the cyclic high temperature oxidation kinetics at 700 °C and the mechanical stability (scratch resistance) of the oxides were examined. Formed oxide scales were investigated using different microscopic and analytical methods including scanning electron microscopy and X-ray diffraction. The mechanical stability and fracture behaviour were examined via scratch testing. Statistical analyses of the results indicate a high relevance of Cr, Ti and Si on the oxidation stability and scale adhesion, while Ni plays only a subordinate role within the oxidation of these ferrous alloys. The wear resistance is highly affected by the oxide layer structure, their mechanical properties and the ongoing cracking and spalling behaviour.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: High-Temperature Coating Behaviors · Advanced materials and composites · Metal and Thin Film Mechanics

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (64)

Show source-provided references
1. Bürgel · 2011
2. Young · 2008
3. Khanna · 2002
4. Gegner · 2006
5. Birks · 2006
6. ASM Handbook Committee · 2005
7. Richardson · 2014
8. Cyclic oxidation of heat resisting steels10.1007/s11085-005-8528-2 ↗
9. Yan · 2015
10. Effect of silicon on the steam oxidation resistance of a 9%Cr heat resistant steel10.1023/B:OXID.0000016280.81734.3f ↗
11. Khatak · 2002
12. Rice · 2007
13. Siebertz · 2010
14. Ramm: Optimization of the Scratch Test for specific coating designs10.1016/j.surfcoat.2011.08.051 ↗
15. DIN EN 1071:3, Advanced Technical Ceramics – Methods of Test for Ceramic Coatings - Part 3: Determination of Adhesion and Other Mechanical Failure Modes by a Scratch Test, 2005.
16. On the possibility of evaluating the resistance of materials to wear by ploughing using a scratch method10.1016/S0043-1648(00)00336-7 ↗
17. Studies on the adhesion of oxide layer formed on X10CrMoVNb9-1 steel10.1016/j.acme.2013.10.005 ↗
18. M. Larsson, M. Olsson, P. Hedenquist, S. Hogmark, On the mechanism of coating failure as demonstrated by scratch and indentation testing of TiN and HSS, submitted to Surface Engineering, 1996 (included in Uppsala Dr Thesis by Larsson, M., No. 191/1996).
19. K.L. Mittal, Adhesion Aspects of Thin Films. VSP BV, Utrecht, 2001.
20. Tribological contact analysis of a rigid ball sliding on a hard coated surface Part I: modelling stresses and strains10.1016/j.surfcoat.2005.03.040 ↗
21. Residual stresses in TiN, DLC and MoS2 coated surfaces with regard to their tribological fracture behaviour10.1016/j.wear.2009.01.004 ↗
22. Failure mode maps in the thin film scratch adhesion test10.1016/S0301-679X(97)00012-1 ↗
23. Zum Gahr · 1987
24. Chapter 7 – an overview of the potential of quantitative coating adhesion measurement by scratch testing10.1016/S0167-8922(06)80043-X ↗
25. I.A. Inman, P.S. Datta. H.L. Du, C. Kübel, P.D. Wood, High temperature tribocorrosion, in: Shreir’s Comprehensive Corrosion, Elsevier, Amsterdam, 2010.10.1016/B978-044452787-5.00020-2 ↗
26. Mechanisms for transitional friction and wear behaviour of sliding metals10.1016/0043-1648(81)90283-0 ↗
27. The dependence of the transition of severe to mild wear on load and surface roughness when the oxide particles are supplied before sliding10.1016/0043-1648(90)90054-E ↗
28. The role of oxide particles in the fretting wear of mild steel10.1016/0043-1648(91)90257-U ↗
29. Experimental simulation of high temperature sliding contact of hot rolled steel10.1016/j.triboint.2015.01.007 ↗
30. Welding parameters and their influence on the abrasion resistance of structural steels at elevated temperatures10.4028/www.scientific.net/KEM.721.461 ↗
31. Wear reducing effects and temperature dependence of tribolayer formation in harsh environment10.1016/j.triboint.2013.03.003 ↗
32. High temperature abrasion resistance of differently welded structural steels
33. High temperature corrosion of boiler steels in hydrochloric atmosphere under oil shale ashes10.1016/j.corsci.2013.12.016 ↗
34. High temperature oxidation studies of binary and ternary iron based alloys at 700°C10.2495/MC150341 ↗
35. R Development Core Team · 2008
36. Mehrer · 2007
37. Factors affecting chromium carbide precipitate dissolution during alloy oxidation10.1023/A:1018880019395 ↗
38. F.H. Stott, G.J. Gabriel, F.I. Wei, G.C. Wood, Materials and Corrosion, vol. 38, 1987, p. 521.10.1002/maco.19870380910 ↗
39. Chloridation and oxidation of iron, chromium, nickel and their alloys in chloridizing and oxidizing atmospheres at 400–700°C10.1016/S0010-938X(99)00142-0 ↗
40. Temperature dependence of oxide scale formation on high-Cr ferritic steels in Ar–H2–H2O10.1016/j.corsci.2011.02.031 ↗
41. Knacke · 1991
42. Grain-size effects on the high-temperature oxidation behaviour of chromium steels10.1007/s11085-010-9192-8 ↗
43. Brandes · 1998
44. Simultaneous measurement of Cr, Mn and Fe diffusion in chromium-manganese steels
45. Diffusion of Cr in alpha-iron10.2320/matertrans1989.31.255 ↗
46. Diffusion of nickel into iron10.1016/0001-6160(61)90138-9 ↗
47. Frost · 1982
48. The self-diffusion of Ni in NiO and its relevance to the oxidation of Ni10.1007/BF00647789 ↗
49. Diffusion of iron in silicon dioxide10.1149/1.1392548 ↗
50. Davis · 1997
51. The long-term, cyclic-oxidation behavior of selected chromia-forming alloys10.1023/A:1018874206733 ↗
52. Lide · 2008
53. Physical properties of iron-oxide scales on Si-containing steels at high temperature10.2320/matertrans.M2009097 ↗
54. Yang · 2002
55. Mechanical behaviour of iron oxide scale: experimental and numerical study10.1016/j.wear.2005.03.037 ↗
56. Mechanical properties of chromia scales
57. Microstructure and mechanical properties of chromium oxide coatings10.1557/JMR.2007.0445 ↗
58. Pysical properties of iron-oxide scales on Si-containing steels at high temperature10.2320/matertrans.M2009097 ↗
59. The mechanical properties of nickel oxide and their relationship to the morphology of thick oxide scales formed on nickel10.1007/BF00613090 ↗
60. Observations on the mechanical properties of nickel oxide scales10.1007/BF00572420 ↗
61. Inman · 2013
62. Friction and Wear Behavior of 30CrMnSiA steel at elevated temperatures10.1007/s11665-016-1969-8 ↗
63. High temperature three-body abrasive wear of 0.25C 1.42Si steel with carbide free bainitic (CFB) and martensitic microstructures10.1016/j.wear.2016.04.012 ↗
64. Some frictional features associated with the sliding wear of the nickel-base alloy N80A at temperatures to 250°C10.1016/0043-1648(94)90146-5 ↗