journal article·2019-04

Evaluation of surface modification in a steel track for the rubber tyred Metro

M. Moreno-Ríos, E.A. Gallardo-Hernández, M.J. Yáñez-Escoto, L.A. Márquez-Tamayo, E. Iturbe-Salas

Wear· Volume 426-427
Publisher page

Abstract

Abstract The rubber tyred metro is a very popular transportation system in some countries, like in Mexico City where 12 lines transport around 5.5 million people every day. The rubber tyre rolls over a steel track subjected under different sources of contamination. Firstly, the rubber tyre accumulates contaminants all over the tread tyre, such as: oil, water, tyre debris, wear particles from the braking and electrical systems, garbage from platforms and steel debris among others. Due to these facts, contamination problems and the rainy season, the metro system suffers severe problems of adhesion. Dangerously, the trains present skidding and slipping problems. The operator must approach and leave the station at very low velocity to prevent accidents. This problem causes delays in the system transportation and discomfort. As a remedy, to reduce the low adhesion, technicians from the metro system have machined grooves on the steel track, however the problem has not been considerably reduced. This work aims to improve the coefficient of friction (CoF) machining the steel track surface with different macro textures. Tests were carried out by using a pendulum friction tester in laboratory. The values indicated an increase in the friction because the grooves help to evacuate water on both sides of the steel track. In addition, the wear rate of some pads from the pendulum increased, indicating a potential increase of wear of rubber tyres due to texturing.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Tribology and Wear Analysis · Adhesion, Friction, and Surface Interactions · Lubricants and Their Additives

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (19)

Show source-provided references
1. Evaluation of friction mechanisms and wear rates on rubber tire materials by low-cost laboratory tests10.1016/j.wear.2015.04.001 ↗
2. Viscoelastic properties of elastomers and tire wet skid resistance10.5254/1.3538445 ↗
3. Wear and wet friction of steel tracks for rubber-tired metros10.1016/j.wear.2017.01.066 ↗
4. Metro CDMX. Twitter. Retrieved from 〈https:/twitter.com/search?Q=STC%20metro&src=typd〉, 2015.
5. Rubber steel friction in contaminated contacts10.1016/j.wear.2013.01.087 ↗
6. Friction and wear in Rubbers and Tyres10.1016/0043-1648(80)90291-4 ↗
7. SCT-Metro. Reporte Técnico Cómite para el analisis de los efectos de la lluvia en el tramo superficial de línea 2. México, D. F, 1993.
8. Wear and wet friction of steel tracks for rubber-tired metros10.1016/j.wear.2017.01.066 ↗
9. Influence of filler type on wet skid resistance of SSBR/BR composites: effects from roughness and microhardness of rubber surface10.1016/j.apsusc.2010.08.129 ↗
10. R. Lewis, S.R. Lewis, Y. Zhu, S. Abbasi, U. Olfsson, The modification of a slip resistance meter form measurement of railhead adhesion, Proc. IMechE. Part F: J. Rail Rapid Transit, 227, 196-200, 2013.10.1177/0954409712455147 ↗
11. Investigation of the isolation and frictional properties of hydrophobic products on the railhead, when used to combat low adhesion10.1016/j.wear.2013.11.024 ↗
12. An alternative method for the assessment or railhead traction10.1016/j.wear.2010.10.035 ↗
13. The mechanism of pedestrian slip on flooring contaminated with solid particles10.1016/j.triboint.2008.07.013 ↗
14. M. Moreno-Ríos, E.A. Gallardo-Hernandez, M. Vite-Torres, A. Peña Bautista, Field and laboratory assessments of the friction coefficient at a railhead, Proc. IMechE. Part F: J. Rail and Rapid Transit. Issue 1, 230, 313–320, 2016.10.1177/0954409714536383 ↗
15. British Standard 7976-1:2002+A1:2013, Pendulum testers, 2002.
16. Cooper Wessex, Pendulum skid tester manual, 2006.
17. M. Moreno-Ríos, Obtención de coeficientes de fricción con equipo péndulo en contactos rueda-riel de sistemas ferroviarios, México, D. F.: SEPI-ESIME-Zacatenco Instituto Politécnico Nacional, Ph.D. Thesis, 2015.
18. C.A. Quinto Saure, Erosión por partícula sólida de hielo seco (CO2) para la pista metálica de rodadura del neumático en el STC Metro. México, D. F.: SEPI-ESIME-Zacatenco Instituto Politécnico Nacional, Master Thesis, 2015.
19. M. Melgar Uresty, Programa de mantenimiento en las vías sobre neumáticos del metro de la Ciudad de México. ESIME-Azcapotzalco Instituto Politécnico Nacional, Tesis de Licenciatura, 2005.