Abstract
Abstract NiCr-Cr2O3-Ag-BaF2/CaF2 (PS304) and NiMoAl-Cr2O3-Ag-BaF2/CaF2 (PS400) coatings provide low wear and friction throughout temperatures ranging from 25 to 700 °C. However, one drawback of using NiCr as matrix component is the expansion observed in high temperatures, which can be detrimental for coating integrity in gas turbine applications. This expansion is caused by the formation of small precipitates, but the mechanisms of their formation are not fully understood since they are not observed in oxidational tests of pure NiCr. In the present study, PS304 and PS400 were sprayed by Atmospheric Plasma Spray and then heat-treated at 600 °C for 1, 24, 48 and 100 h to capture the initial moments of precipitate formation. The results have shown that the phase transformation occurring upon heat treatment is more complex than what is proposed in literature. Experimental evidence has shown that the precipitates are formed by fluorine that diffuses from the fluorides to the NiCr driven by the oxidation of the fluorides, which form BaCrO4 and CaCrO4. Wear and friction, however, show minor sensitivity to this reaction, at least under room temperature test conditions. Furthermore, PS400 coatings showed lower wear when compared to PS304, with negligible expansion and no significant change in microstructure upon heat treating, indicating superior thermal stability and wear resistance under the tested conditions.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: High-Temperature Coating Behaviors · Metal and Thin Film Mechanics · Vacuum and Plasma Arcs
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (32)
Show source-provided references
1. Wide temperature spectrum self-lubricating coatings prepared by plasma spray10.1016/0040-6090(79)90511-X ↗
2. Fauchais · 2014
3. The effect of compositional tailoring on the thermal expansion and tribological properties of PS300: a solid lubricant composite coating10.1080/10402009708983703 ↗
4. DellaCorte
5. Thrust-washer evaluation of self-lubricating PS304 composite coatings in high temperature sliding contact10.1080/10402000208982579 ↗
6. Thrust-washer tribological evaluation of PS304 coatings against Rene 4110.1016/j.wear.2005.02.051 ↗
7. Application of a high temperature self-lubricating composite coating on steam turbine components
8. The evaluation of a modified chrome oxide based high temperature solid lubricant coating for foil gas bearings10.1080/10402000008982337 ↗
9. Performance and durability of high temperature foil air bearings for oil-free turbomachinery10.1080/10402000008982407 ↗
10. Thermal processing effects on the adhesive stregth of PS304 high temperature solid lubricant coatings10.1080/10402000208982580 ↗
11. Phase identification of hard precipitates in PS304 coatings10.1179/026708410X12683118611301 ↗
12. The effects of substrate material and thermal processing atmosphere on the strength of PS304: a high temperature solid lubricant coating10.1080/10402000308982638 ↗
13. Stanford · 2004
14. Dimensional stability, microstructure, and cohesion strength of composite solid lubricant coatings after heat treatment10.1080/10402000802527781 ↗
15. Adsorption and diffusion of fluorine on Cr-doped Ni(111) surface: fluorine-induced initial corrosion of non-passivated Ni-based alloy10.1016/j.jnucmat.2016.06.027 ↗
16. Theoretical study of fluorine-induced surface segregation of Cr in non-passivated Ni-based alloys10.1063/1.5047225 ↗
17. First-principle atomistic thermodynamic study on the early-stage corrosion of NiCr alloy under fluoride salt environment10.1039/C8CP05045G ↗
18. Materials corrosion in molten LiF-NaF-KF salt10.1016/j.jfluchem.2008.05.008 ↗
19. Oxidation kinetics of BaF₂ single crystals10.1002/crat.19790140207 ↗
20. Oxygen penetration into single crystals of calcium fluoride10.1111/j.1151-2916.1963.tb11773.x ↗
21. Development of an in situ Raman spectroscopic system for surface oxide films on metals and alloys in high temperature water10.1016/j.nucengdes.2004.12.002 ↗
22. The Effect of Deposition Parameters on the Structure and Mechanical Properties of Chromium Oxide Coatings Deposited by Reactive Magnetron Sputtering
23. Monitoring Ag−Cr interactions in SOFC cathodes using Raman spectroscopy10.1021/jp804239t ↗
24. Friction and wear properties of hot-pressed NiCr-BaCr2O4high temperature self-lubricating composites10.1016/j.wear.2013.02.004 ↗
25. Pressure-induced structural phase transition in CaCrO4: evidence from Raman scattering studies10.1063/1.2117624 ↗
26. An in situ Raman spectroscopic study of pressure induced dissociation of spinel NiCr 2O 410.1016/S0022-3697(02)00328-1 ↗
27. Effects of lead on the initial corrosion behavior of 316LN stainless steel in high-temperature alkaline solution10.1007/s40195-018-0821-6 ↗
28. Chemical stability between NiCr₂O₄ material and molten calcium-magnesium-alumino-silicate (CMAS) at high temperature
29. Electrochemical and Raman spectroscopic investigations on the speciation and behavior of chromium ions in fluoride doped molten LiCl-KCl10.1149/2.1221910jes ↗
30. Fabrication of potato-like silver molybdate microstructures for photocatalytic degradation of chronic toxicity ciprofloxacin and highly selective electrochemical detection of H2O210.1038/srep34149 ↗
31. Thin films of MoO3-Ag2 O binary oxides - the high temperature lubricants10.1016/j.wear.2006.01.008 ↗
32. Spontaneous Raman spectroscopy of tungstate and molybdate crystals for Raman lasers10.1016/S0925-3467(00)00037-9 ↗