Effect of type and temperature of serum lubricant on VEXLPE wear and friction
Source abstract
Abstract
Abstract Multidirectional tests were carried out to study the influence of the type and temperature of serum lubricant on the wear and friction of vitamin E stabilized, extensively crosslinked ultrahigh molecular weight polyethylene (VEXLPE) against polished CoCr. To minimize the rates of protein denaturation and microbial growth, cold wear tests were performed for the first time so that the serum lubricant was at a refrigerator temperature of 4 °C. The highest wear factors and coefficients of friction were observed at the refrigerator temperature and the lowest at body temperature where the rates of protein denaturation and microbial growth were expected to be at their maximum. The VEXLPE mean wear factor in alpha calf serum (ACS) decreased by two orders of magnitude as the lubricant bulk temperature increased from 4 °C to 37 °C. Thermal analysis indicated that the contact temperature in the pin-on-disk test was less than 2 °C above the lubricant bulk temperature. It appears that a wide range of polyethylene wear rates and coefficients of friction can be obtained depending on the temperature. The type of serum also strongly affected the obtained wear rate at and above 20 °C.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Orthopaedic implants and arthroplasty · Tribology and Wear Analysis · Total Knee Arthroplasty Outcomes
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (32)
Show source-provided references
1. Frictional heating of bearing materials tested in a hip joint wear simulator10.1243/0954411971534728 ↗
2. Potential thermal artifacts in hip joint wear simulators10.1002/(SICI)1097-4636(1999)48:4<458::AID-JBM9>3.0.CO;2-B ↗
3. The effect of protein lubrication on the wear properties of materials for prosthetic joints10.1002/(SICI)1097-4636(1999)48:4<465::AID-JBM10>3.0.CO;2-Y ↗
4. Quantitative analysis of serum degradation and its effect on the outcome of hip joint simulator wear testing of UHMWPE
5. Effect of protein concentration and serum dilution on the wear rate of UHMWPE cups
6. A comparison of biological lubricants to bovine calf serum for total joint wear testing
7. The effect of frictional heating and forced cooling on the serum lubricant and wear of UHMW polyethylene cups against cobalt-chromium and zirconia balls10.1016/S0142-9612(03)00148-0 ↗
8. The effects of lubricant composition on in vitro wear testing of polymeric acetabular components10.1002/jbm.b.10077 ↗
9. Challenges associated with using bovine serum in wear testing orthopaedic biopolymers10.1177/0954411911416047 ↗
10. Calf serum constituent fractions influence polyethylene wear and microbial growth in knee simulator testing10.1177/0954411912444248 ↗
11. The effect of bacterial contamination on friction and wear in metal/polyethylene bearings for total joint repair—a case report10.1016/j.wear.2012.11.022 ↗
12. In vitro tests of substitute lubricants for wear testing orthopaedic biomaterials10.1177/0954411913481549 ↗
13. Effect of lubrication conditions on the wear of UHMWPE with noncyclic motion and load10.1080/10402004.2018.1506071 ↗
14. The origin of submicron polyethylene wear debris in total hip arthroplasty
15. Force track analysis of contemporary hip simulators10.1016/S0021-9290(03)00166-0 ↗
16. Frictional heating of total hip implants. Part 1. measurements in patients10.1016/S0021-9290(00)00188-3 ↗
17. 2014
18. Antimicrobial agents and low-molecular weight polypeptides affect polyethylene wear in knee simulator testing10.1016/j.triboint.2013.02.019 ↗
19. Wear testing of crosslinked polyethylene: wear rate variability and microbial contamination10.1016/j.jmbbm.2014.02.016 ↗
20. The biochemical characteristics of wear testing lubricants affect polyethylene wear in orthopaedic pin-on-disc testing10.1177/0954411914567930 ↗
21. A hip wear simulator with 100 test stations10.1243/095441105X34301 ↗
22. Characterization of irradiated blends of α-tocopherol and UHMWPE10.1016/j.biomaterials.2005.04.026 ↗
23. Vitamin E-stabilized UHMWPE for total joint implants: a review10.1007/s11999-010-1717-6 ↗
24. Biotribology of a vitamin E-stabilized polyethylene for hip arthroplasty – influence of artificial aging and third-body particles on wear10.1016/j.actbio.2014.02.052 ↗
25. High cycle in vitro hip wear of and in vivo biological response to vitamin E blended highly cross-linked polyethylene10.1016/j.biotri.2018.09.001 ↗
26. Hip wear simulator results of vitamin E-blended highly crosslinked polyethylene
27. Efficacy of vitamin E for mechanical damage and oxidation of polyethylene rim by stem neck impingement10.1016/j.clinbiomech.2019.05.024 ↗
28. Effect of contact pressure on wear and friction of ultra-high molecular weight polyethylene in multi-directional sliding10.1243/09544119JEIM146 ↗
29. A 12-station anatomic hip joint simulator10.1243/095441105X34419 ↗
30. Effect of random variation of input and various daily activities on wear in a hip joint simulator10.1016/j.jbiomech.2020.109831 ↗
31. Cold denaturation of proteins10.3109/10409239009090612 ↗
32. Performance analysis of an orthopaedic biomaterial 100-station wear test system10.1243/09544062JMES1626 ↗