Influence of substrate type and film thickness on the failures of Zr-based thin-film metallic glass under nanoscratch
Source abstract
Abstract
Nanoscratch experiments under constant and ramp loading conditions are performed to investigate the delamination, and spallation characteristics of Zr-based thin-film metallic glass (Zr-based TFMG, Zr 65Cu 15Al 10Ni 10). TFMGs with different film thickness = 200, 500, 1000 nm are deposited over hard and soft substrates via DC magnetron sputtering process. Coefficient of friction (COF) is measured to be less about 0.03 regardless of scratch mode and maximum normal load. The critical load for thin film delamination and spallation reveals that the deformation and failure mechanism of Zr-based TFMG significantly change with film thickness and substrate type. The failure mechanism is characterized by observing the scratch grooves via optical and scanning electron microscopes (SEM). The adhesion energy between thin film and soft substrate is calculated based on Burnett and Rickerby model, and an increase in adhesion energy with interfacial layer thickness is reported.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Metallic Glasses and Amorphous Alloys · High-Temperature Coating Behaviors · Surface Roughness and Optical Measurements
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (46)
Show source-provided references
1. Enhanced ductility in a Zr65Cu15Al10Ni10 bulk metallic glass by nanocrystallization during compression10.1016/j.matdes.2011.10.034 ↗
2. Indentation size effects of mechanical behavior and shear transformation zone in thin film metallic glasses10.1016/j.tsf.2017.11.029 ↗
3. Tribological behaviors of Zr-based bulk metallic glass versus Zr-based bulk metallic glass under relative heavy loads10.1016/j.intermet.2015.06.002 ↗
4. Influence of oxidation on the performance of Zr55Cu30Al10Ni5 BMG10.1016/j.intermet.2016.08.007 ↗
5. Fracture behavior of Zr55Cu30Al10 Ni5 bulk metallic glass under quasi-static and dynamic compression10.1557/JMR.2008.0217 ↗
6. Bulk metallic glass composite with good tensile ductility, high strength and large elastic strain limit10.1038/srep05302 ↗
7. Promising Ta-Ti-Zr-Si metallic glass coating without cytotoxic elements for bio-implant applications10.1016/j.apsusc.2017.08.065 ↗
8. Enhancement of mechanical and thermal properties in Zr-Cu-Ni-Al-N thin film metallic glass by compositional control of nitrogen10.1016/j.matlet.2015.07.019 ↗
9. Electrical and optical properties of Co75Si15B10 metallic glass nanometric thin films
10. Materials properties of ion beam sputtered Ti-Cu-Pd-Zr thin film metallic glasses10.1016/j.jnoncrysol.2017.01.008 ↗
11. Thermal, mechanical and electrical properties of Pd-based thin-film metallic glass10.1143/JJAP.40.5382 ↗
12. Thin film metallic glasses: properties, applications and future10.1063/1.5122884 ↗
13. Coating cutting blades with thin-film metallic glass to enhance sharpness10.1038/s41598-019-52054-3 ↗
14. Non-stick syringe needles: beneficial effects of thin film metallic glass coating10.1038/srep31847 ↗
15. Failure mechanisms of the coating/metal interface in waterborne coatings: the effect of bonding10.3390/ma10040397 ↗
16. Effects of coating thickness and interfacial roughness on cracking and delamination strength of WC-Co coating measured by ring compression test10.1088/1757-899X/61/1/012024 ↗
17. Characterization and analysis of metal adhesion to parylene polymer substrate using scotch tape test for peripheral neural probe10.3390/mi11060605 ↗
18. Quantitative peel test for thin films/layers based on a coupled parametric and statistical study10.1038/s41598-019-55355-9 ↗
19. Rust layer adhesion capability and corrosion behavior of weathering steel under tension during initial stages of simulated marine atmospheric corrosion10.1016/j.conbuildmat.2019.117393 ↗
20. Interface adhesion assessment of composite-to-metal bonded joints under salt spray conditions using peel tests10.1016/j.compstruct.2016.12.058 ↗
21. Scratch induced thin film buckling for quantitative adhesion measurements10.1016/j.matdes.2018.05.062 ↗
22. Influence of substrate and interfacial adhesion on the scratch resistance of poly(methylmethacrylate)10.1016/j.matdes.2020.108984 ↗
23. Mechanical properties study of a magnetron-sputtered Zr-based thin film metallic glass10.1016/j.surfcoat.2012.04.101 ↗
24. Micro-scratch study of a magnetron-sputtered Zr-based metallic-glass film10.1016/j.surfcoat.2009.05.017 ↗
25. Fabrication of new metallic glassy Ti40.6Cu15.4Ni8.5Al5.5W30 alloy powders by mechanical alloying and subsequent SPS consolidation10.1016/j.apt.2016.12.007 ↗
26. Characterization and properties of CuZrAlTiNi high entropy alloy coating obtained by mechanical alloying and vacuum hot pressing sintering10.1016/j.apt.2017.07.006 ↗
27. Formation of a silicon layer by electroreduction of SiO 2 nanoparticles in CaCl 2 molten salt10.1016/j.electacta.2012.01.008 ↗
28. Effect of modulation ratio on the mechanical behavior of multilayer-thin-film metallic glasses10.1016/j.jmrt.2021.11.160 ↗
29. Evaluation of mechanical properties of Zr-Cu-Al-Ni TFMG using nanoindentation10.1016/j.jmrt.2021.04.030 ↗
30. An improved technique for determining hardness and elastic modulus using load and displacement sensing indentation experiments10.1557/JMR.1992.1564 ↗
31. Structural and micromechanical properties of Nd:YAG laser marking stainless steel (AISI 304 and AISI 316)10.3390/ma13092168 ↗
32. Mechanical properties of low-temperature gaseous carburizated layer in 316L stainless steel based on nano-indentation and four-point bending tests10.1016/j.surfcoat.2020.125501 ↗
33. Study on tribological characteristics of Zr-based BMG via nanoscratch techniques10.1016/j.wear.2021.204067 ↗
34. Scratch-tip-size effect and change of friction coefficient in nano/micro scratch tests using XFEM10.1016/j.triboint.2018.01.003 ↗
35. Nanoindentation of zirconium based bulk metallic glass and its nanomechanical properties10.1016/j.jmrt.2019.10.034 ↗
36. A nanoindentation study of serrated flow in bulk metallic glasses10.1016/S1359-6454(02)00303-8 ↗
37. Tribological behavior of thermomechanically treated Al–Mg–Si alloy by nanoscratch measurements10.1016/j.triboint.2016.05.029 ↗
38. Influence of substrate hardness on coating-substrate adhesion10.4028/www.scientific.net/AMR.177.148 ↗
39. Indentation and scratching mechanisms of a ZrCuAlNi bulk metallic glass10.1088/0022-3727/41/7/074029 ↗
40. Shear band patterns in metallic glasses under static indentation, dynamic indentation, and scratch processes10.1007/s11661-007-9315-2 ↗
41. Study of scratching Mg-based BMG using nanoindenter with Berkovich probe10.1016/j.msea.2009.11.070 ↗
42. Investigation into nanoscratching mechanical performance of metallic glass multilayers with improved nano-tribological properties10.1016/j.jallcom.2018.10.270 ↗
43. Adhesion enhancement of DLC hard coatings by HiPIMS metal ion etching pretreatment10.1016/j.surfcoat.2018.04.090 ↗
44. The relationship between hardness and scratch adhession10.1016/0040-6090(87)90382-8 ↗
45. Adhesion evaluation of thin ceramic coatings on tool steel using the scratch testing technique10.1016/0257-8972(94)02396-4 ↗
46. Effect of interfacial SiO2 thickness for low temperature O 2 plasma activated wafer bonding10.1007/s00542-005-0038-2 ↗