Abstract

The use of connectors in electrical devices for automotive industry has significantly increased during the last decades. These connectors need to keep low and stable electrical contact resistance (ECR) otherwise disconnects may occur inducing critical failures. Close to the engine, these connectors are subjected to vibrations inducing fretting wear damage. The aim of this study is to investigate the influence of relative humidity and the presence of pollutant sulfurous gases (H 2 S, SO 2) on the silver-plated electrical contact resistance (ECR) behavior. The ECR fretting endurance Nc (i.e. when ΔR> ΔRth = 4 mΩ) displays a fast increase above RH th(Air)= 50%. The debris layer becomes more conductive so a larger wear volume is required to reach the ECR failure. At the same time, the debris layer becomes more cohesive and the wear rate decreases. Alternatively, synergic interaction between H 2 S, SO 2 gases and relative humidity above RH th(Air&S) = 60% leads to the formation of lubricating Ag 2 S sulphide and Ag 2 SO 4 sulphate tribofilm which, by decreasing the friction coefficient and the silver layer wear rate, sharply increases the ECR endurance. Finally, using simple explicit formulations, both ECR endurances under polluted and non-polluted air are formalized.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Electrical Contact Performance and Analysis · Mechanical stress and fatigue analysis · Adhesion, Friction, and Surface Interactions

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (34)

Show source-provided references
1. Electrical effects of fretting materials: a review10.1016/0043-1648(85)90101-2 ↗
2. Fretting corrosion of gold-plated connector contacts10.1016/0043-1648(81)90192-7 ↗
3. Degradation of power contacts in industrial atmosphere : silver corrosion and whiskers
4. Effect of intermetallic phases on the performance of tin-plated copper connections and conductors
5. Correlation between Wear and Electrical behaviour of contact interfaces during Fretting vibration
6. Influence of contact interface composition on the electrical and tribological properties of nickel electrodeposits during fretting tests
7. Effect of roughness on electrical contact performance of electronic components10.1016/j.microrel.2017.05.024 ↗
8. Normal force and displacement amplitude influences on silver-plated electrical contacts subjected to fretting wear: a basic friction energy – contact compliance formulation10.1016/j.wear.2018.12.010 ↗
9. Fretting behavior of Au plated copper contacts induced by high frequency vibration
10. Failure mechanism of sliding electrical contacts with various plated materials
11. Effect of grain size on the electrical failure of copper contacts in fretting motion10.1016/j.triboint.2017.02.043 ↗
12. Investigation on friction coefficient evolution for thin-gold layer contacts
13. Fretting corrosion of gold-plated connector contacts10.1016/0043-1648(81)90192-7 ↗
14. Fretting behavior of Au plated copper contacts induced by high frequency vibration
15. Stationary loading, fretting and sliding of silver coated copper contacts — influence of corrosion films and corrosive atmosphere10.1016/S0301-679X(96)00031-X ↗
16. Degradation of power contacts in industrial atmosphere : silver corrosion and whiskers
17. Introduction of an exponential formulation to quantify the electrical endurance of micro-contacts enduring fretting wear: application to Sn, Ag and Au coatings10.1016/j.wear.2011.01.058 ↗
18. The fretting sliding transition as a criterion for electrical contact performance10.1016/S0043-1648(01)00685-8 ↗
19. Gross plastic fretting mechanical deterioration of silver coated electrical contacts10.1016/S0043-1648(96)07259-6 ↗
20. Gross plastic fretting — examination of the gross weld regime10.1016/S0043-1648(96)07260-2 ↗
21. Prediction of the electrical contact resistance endurance of silver-plated coatings subject to fretting wear, using a friction energy density approach10.1016/j.wear.2014.12.006 ↗
22. Influence of humidity on the endurance of silver-plated electrical contacts subjected to fretting wear10.1016/j.surfcoat.2018.07.109 ↗
23. Quantification of fretting damage10.1016/S0043-1648(96)07306-1 ↗
24. In situ QCM and TM-AFM investigations of the early stages of degradation of silver and copper surfaces10.1016/j.apsusc.2006.08.005 ↗
25. Contact and rubbing of flat surfaces10.1063/1.1721448 ↗
26. A numerical simulation of fretting wear profile taking account of the evolution of third body layer10.1016/j.wear.2017.01.063 ↗
27. Tarnishing resistance of silver–palladium thin films10.1016/j.surfcoat.2005.10.020 ↗
28. Quantitative determination of surface composition of sulfur bearing anion mixtures by Auger electron spectroscopy10.1021/ac50051a021 ↗
29. XPS core level spectra and auger parameters for some silver compounds10.1016/0368-2048(91)85008-H ↗
30. A study of the modification of the friction and wear behavior of polyphenylene sulfide by particulate Ag2S and PbTe fillers10.1016/S0043-1648(98)00155-0 ↗
31. The role of filler deformability, filler–polymer bonding, and counterface material on the tribological behavior of polyphenylene sulfide (PPS)10.1016/S0043-1648(01)00799-2 ↗
32. On the mechanism of silver and copper sulfidation by atmospheric H2S and OCS10.1016/0010-938X(85)90060-5 ↗
33. Fretting corrosion behavior of electrical contacts with tin coating in atmosphere and vacuum10.1016/j.wear.2018.11.024 ↗
34. An investigation of fretting wear behaviour of nickel coatings for electrical contacts application in dry and lubricated conditions10.1016/j.wear.2013.01.076 ↗