journal article·2023-05Open access

Effect of substrate bias voltage on structural and tribological properties of W-Ti-C-N thin films produced by combinational HiPIMS and DCMS co-sputtering

S.A. Ataie, M. Soltanieh, R. Naghizadeh, A. Cavaleiro, M. Evaristo, F. Fernandes, F. Ferreira

Wear· Volume 520-521

Abstract

Protective multi-component thin films at the surface of cutting tools have been significantly developed to reduce wear and friction. The present work investigates the effect of substrate bias voltage on the structural-tribological relations of W-Ti-C-N thin films produced by HiPIMS and DCMS co-sputtering. Chemical analysis of the coatings is obtained and composite phase structure is revealed. Morphology of the coatings illustrates that defectless surfaces may be achieved. Topographical parameters are investigated by employing graphical software. Indentation, scratch and pin-on-disk tests (pin is AISI 52100 steel) are applied to study mechanical behaviors of the films. To produce a wear-resistant film, a median bias voltage (􀀀 60 V) and as a result, optimum content of tungsten concentration (19.2 at. %), grain size (42.8 nm) and average peak interval (188 nm) is required. Finally, a model based on the representative volume element is developed to show crack propagation and delamination.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Metal and Thin Film Mechanics · Advanced materials and composites · Diamond and Carbon-based Materials Research

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (67)

Show source-provided references
1. REACTIVELY SPUTTERED TiN COATINGS FOR TRIBOLOGICAL APPLICATIONS10.1016/0040-6090(80)90489-7 ↗
2. Tribological performance of titanium nitride coatings: a comparative study on TiN coated stainless steel and titanium alloy10.1016/j.wear.2019.01.029 ↗
3. Strategies for damage tolerance enhancement in metal/ceramic thin films: lessons learned from Ti/TiN10.1016/j.actamat.2022.117777 ↗
4. Microstructure and tribological performance of (AlCrWTiMo)N film controlled by substrate temperature10.1016/j.apsusc.2021.151677 ↗
5. Retrieval study of commercially available knee implant coatings TiN, TiNbN and ZrN on TiAl6V4 and CoCr28Mo610.1016/j.jmbbm.2020.104034 ↗
6. Correlation between stress and hardness in pulsed cathodic arc deposited titanium/vanadium nitride alloys10.1088/0953-8984/16/45/017 ↗
7. Magnetron sputtering of hard nanocomposite coatings and their properties10.1016/S0257-8972(01)01139-2 ↗
8. Influence of Si content on phase stability and mechanical properties of TiAlSiN films grown by AlSi-HiPIMS/Ti-DCMS co-sputtering10.1016/j.surfcoat.2021.127661 ↗
9. Wear behavior and machining performance of TiAlSiN-coated tools obtained by dc ms and hipims: a comparative study10.3390/ma14185122 ↗
10. Raman microscopic studies of PVD hard coatings10.1016/S0257-8972(99)00072-9 ↗
11. Different approaches to superhard coatings and nanocomposites10.1016/j.tsf.2004.10.053 ↗
12. The hardness and strength properties of WC-Co composites10.3390/ma4071287 ↗
13. Wide band gap and conducting tungsten carbide (WC) thin films prepared by hot wire chemical vapor deposition (HW-CVD) method10.1016/j.matlet.2016.07.132 ↗
14. Wear properties of carbon-rich tungsten carbide films
15. Influence of process parameters on properties of reactively sputtered tungsten nitride thin films
16. Tribological performance of GLC, WC/GLC and TiN films on the carburized M50NiL steel10.1016/j.surfcoat.2019.01.038 ↗
17. Wear resistant multilayer nanocomposite WC1-x/C coating on Ti-6Al-4V titanium alloy10.1016/j.triboint.2014.05.030 ↗
18. Effects of substrate temperature and reactive gas flow rate on the crystalline ceramic phases formation and tribological properties of W–Ti–Co–C–N thin films produced by co-sputtering10.1016/j.ceramint.2020.08.087 ↗
19. The effects of a third element on structure and properties of W-C/N10.1016/S0257-8972(01)01640-1 ↗
20. Mechanical behaviour of W-S-N and W-S-C sputtered coatings deposited with a Ti interlayer10.1016/S0257-8972(02)00622-9 ↗
21. Influence of Ti addition on the properties of W–Ti–C/N sputtered films10.1016/S0257-8972(03)00328-1 ↗
22. A study on the synthesis and microstructure of WC-TiN superlattice coating10.1016/S0257-8972(00)00808-2 ↗
23. High strength and deformation mechanisms of Al0.3CoCrFeNi high-entropy alloy thin films fabricated by magnetron sputtering10.3390/e21020146 ↗
24. Toughening mechanisms for ceramic materials10.1016/0955-2219(92)90026-A ↗
25. Toughening mechanisms in V-Si-N coatings10.1016/j.matdes.2021.109961 ↗
26. Toughness evaluation of hard coatings and thin films10.1016/j.tsf.2011.09.036 ↗
27. Study the effect of thermal annealing on adhesion strength of Silver-Tantalum Oxide thin film deposited by reactive magnetron sputtering10.1080/01694243.2018.1549770 ↗
28. Toughness measurement of thin films: a critical review10.1016/j.surfcoat.2004.10.021 ↗
29. Structure, mechanical, and micro-scratch behavior of Ta-Hf-C solid solution coating deposited by non-reactive magnetron sputtering10.3390/ma15134489 ↗
30. Fracture mechanisms of thin amorphous carbon films in nanoindentation10.1016/S1359-6454(97)00143-2 ↗
31. Hall-Petch analysis of dislocation pileups in thin material layers and in nanopolycrystals10.1557/jmr.2013.10 ↗
32. Growth defects in PVD hard coatings10.1016/j.vacuum.2009.05.018 ↗
33. Synthesis and structural properties of Mo-S-N sputtered coatings10.1016/j.apsusc.2020.146790 ↗
34. Indentation modeling study of temperature-dependent fracture toughness of brittle coating on ductile substrate based on microcrack formation theory10.1016/j.surfcoat.2016.12.016 ↗
35. Mechanics of crack propagation in delamination wear10.1016/0043-1648(77)90083-7 ↗
36. Tribooxidation as a way to improve the wear resistance of cutting tools10.3390/coatings8060223 ↗
37. Comparative study on the nanomechanical behavior and physical properties influenced by the epitaxial growth mechanisms of GaN thin films10.1016/j.apsusc.2021.152188 ↗
38. Energy consumption and material fluxes in hard coating deposition processes10.1016/j.surfcoat.2016.04.062 ↗
39. Contact fatigue behavior of CVD coated cemented carbides in dry and wet conditions
40. Precipitation-based grain boundary design alters inter- to trans-granular fracture in AlCrN thin films10.1016/j.actamat.2022.118156 ↗
41. Structural characterization of DC magnetron-sputtered TiO2 thin films using XRD and Raman scattering studies10.1016/j.mssp.2003.05.012 ↗
42. The ion energy distributions and ion flux composition from a high power impulse magnetron sputtering discharge10.1016/j.tsf.2006.04.051 ↗
43. The high power impulse magnetron sputtering discharge as an ionized physical vapor deposition tool10.1016/j.vacuum.2009.12.022 ↗
44. Effect of bias voltage on the growth of super-hard (AlCrTiVZr)N high-entropy alloy nitride films synthesized by high power impulse magnetron sputtering10.1016/j.apsusc.2021.150417 ↗
45. Effect of peak target power on the properties of Cr thin films sputtered by HiPIMS in deep oscillation magnetron sputtering (DOMS) mode10.1016/j.surfcoat.2014.09.020 ↗
46. Effect of substrate biasing on the structure and properties of tantalum coatings deposited using HIPIMS in deep oscillation magnetron sputtering mode10.3390/met10121618 ↗
47. Non-reactive HiPIMS deposition of NbC x thin films : effect of the target power density on structure-mechanical properties10.1016/j.surfcoat.2022.128674 ↗
48. CrN thin films deposited by HiPIMS in DOMS mode10.1016/j.surfcoat.2016.02.064 ↗
49. Tribological performance of DLC coatings deposited by DOMS in mixed Ar-Ne discharges10.1016/j.matlet.2020.129056 ↗
50. Tribological behavior of sputtered boron carbide coatings and the influence of processing gas10.1016/j.wear.2005.02.096 ↗
51. Influence of base pressure prior to deposition on the adhesion behaviour of carbon thin films on steel10.1016/j.apsadv.2020.100034 ↗
52. Influence of substrate temperature on the crystalline quality of AlN layers deposited by RF reactive magnetron sputtering10.1063/1.4906796 ↗
53. Effect of substrate temperature on the deposition of Al-doped ZnO thin films using high power impulse magnetron sputtering10.1016/j.surfcoat.2018.04.089 ↗
54. Effect of bias voltage on TiAlSiN nanocomposite coatings deposited by HiPIMS10.1016/j.apsusc.2016.09.028 ↗
55. Microstructure, mechanical and tribological properties of Mo–V–Cu–N coatings prepared by HIPIMS technique10.1016/j.ceramint.2021.12.285 ↗
56. HiPIMS pulse shape influence on the deposition of diamond-like carbon films10.1016/j.surfcoat.2021.128059 ↗
57. A critical evaluation of indentation techniques for measuring fracture toughness: I, direct crack measurement10.1111/j.1151-2916.1981.tb10320.x ↗
58. Measurement of thin film mechanical properties using nanoindentation10.1557/S0883769400041634 ↗
59. Measurement of mechanical properties by ultra-low load indentation10.1016/S0921-5093(98)00724-2 ↗
60. Computational modeling of dual-phase steels based on representative three-dimensional microstructures obtained from EBSD data10.1007/s00419-015-1044-1 ↗
61. XANES and XRR study on phase evolution of TiO 2 films developed using HiPIMS10.1016/j.mseb.2022.115827 ↗
62. Evaluation of carbon thin films using Raman spectroscopy
63. Vibrational properties of carbon nitride films by Raman spectroscopy10.1016/S0040-6090(98)00984-5 ↗
64. Contact analysis of non-Gaussian surfaces for minimum static and kinetic friction and wear10.1080/10402009608983609 ↗
65. Fracture toughness determinations by indentation10.1111/j.1151-2916.1976.tb10991.x ↗
66. Literature review on fretting wear and contact mechanics of tribological coatings10.3390/coatings9080501 ↗
67. Pelleg · 2013