Wear of hardfaced valve spindles in highly loaded stationary lean-burn large bore gas engines
Source abstract
Abstract
Abstract The technological evolution of more efficient natural gas-fuelled large bore engines aggravates the load situation within the engine and thus as well the tribological system valve spindle/seat ring. As a result of these changes, valve recession increases and component lifetime decreases, i.e. higher failure rates and more frequent service intervals. The tribological issues can be traced back to the cleaner combustion which demonstrably suppresses the formation of a protective layer on the sealing faces. In this work, Stellite® and Tribaloy®-hardfaced valve spindles with different operating hours and from the same gas engine were analyzed in terms of quantitative wear, oxidation and microstructural alterations in the wear scar. The observed wear mechanisms are based on microstructure fatigue and delamination, depending on the microstructure of the hardfacing. The severely worn sealing interfaces show no tribofilm at all, whereas a protective oxide layer is observed on the surface of the Tribaloy® hardfacing that features low wear. The second part of this work describes wear phenomena observed on specimens from laboratory experiments using a newly developed component test rig – the valve spindle tribometer. The authors describe their approach to investigate wear mechanisms by separated simulation of valve closure and peak combustion pressure depending on different key parameters such as valve closing velocity, temperature or atmosphere. From these preliminary results, probable wear mechanisms are derived and correlated with microstructural properties of the hardfacing alloys.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Metal Alloys Wear and Properties · Tribology and Wear Analysis · Mechanical stress and fatigue analysis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (19)
Show source-provided references
1. 〈http://www.eia.gov/forecasts/ieo/world.cfm〉, (Online).
2. The effect of operating conditions on heavy duty engine valve seat wear10.1016/S0043-1648(96)06945-1 ↗
3. R. Lewis, R. Dwyer-Joyce, G. Josey, Design and development of a bench test-rig for investigating diesel engine inlet-valve and seat insert wear, in: Proceedings of the 5th International Tribology Conference - Austrib'98, Brisbane, 1998.
4. A study of exhaust valve and seat insert wear depending on cycle numbers10.1016/j.wear.2007.02.006 ↗
5. Comparison and analysis of protective tribofilms found on heavy duty exhaust valves from field service and made in a test rig10.1016/j.wear.2013.01.061 ↗
6. Design and operation of a high temperature wear test apparatus for automotive valve materials10.1016/j.wear.2015.08.017 ↗
7. The influence of laser hardening on wear in the valve and valve seat contact10.1016/j.wear.2009.01.040 ↗
8. Development of a laboratory bench test to simulate seat wear of engine poppet valves10.1080/10402009308983204 ↗
9. Investigation of engine exhaust valve wear10.1016/0043-1648(67)90007-5 ↗
10. X. Liang, G. Strong, D. Eickmeyer, K. Myers, A study of valve seat insert wear mechanisms, SAE Technical Paper Series, no. 1999-01-3673, 1999.
11. Wear mechanism analysis of engine exhaust valve seats with a laboratory simulator10.1080/10402009708983647 ↗
12. Wear and wear mechanism simulation of heavy-duty engine intake valve and seat inserts10.1361/105994998770348043 ↗
13. The oxidation behaviour of metals and alloys at high temperatures in atmospheres containing water vapour: a review10.1016/j.pmatsci.2007.11.001 ↗
14. Wear mechanism study of exhaust valve system in modern heavy duty combustion engines10.1016/j.wear.2010.11.039 ↗
15. O. Lehmann, A. Renz, Valve wear in lean-burn large bore gas engines - from engine tests of components to a unique tribological test rig, in: Proceedings of the CIMAC Congress, Helsinki, 2016.
16. Consideration of lubricants for temperatures above 1000 F10.1080/05698195908972374 ↗
17. Sliding wear characteristics of molybdenum containing Stellite 12 coating at elevated temperatures10.1016/j.triboint.2015.06.006 ↗
18. The third body approach: a mechanical view of wear10.1016/0043-1648(84)90025-5 ↗
19. Wear, corrosion and cracking resistance of some W- or Mo-containing Stellite hardfacing alloys10.1016/j.msea.2005.06.062 ↗