Evaluation of synergistic effect and failure characterization for Ni-based nanostructured coatings and 17-4PH SS under cavitation exposure in 3.5 wt % NaCl solution
Source abstract
Abstract
Abstract The Ni/SiC nanocomposite and Ni nanocrystalline coatings were electrodeposited on a 17-4 precipitation hardening stainless steel substrate. The failure characterization of specimens as well as synergistic effect of cavitation and corrosion, and the influence of the mechanical, electrochemical, and microstructural attributions of the Ni-based nanostructured and 17-4 PH stainless steel substrate on their cavitation resistance were investigated. The surface morphology of 17-4PH stainless demonstrated the quasi-cleavage failure mechanism, and both coatings had the dimpled rupture morphology after the cavitation deterioration in both mediums. The results also represented that the synergism contribution of cavitation and corrosion was 29.5, 22.6, and 6.3% for 17-4 PH stainless steel substrate, Ni nanocrystalline, and Ni/SiC nanocomposite coatings, correspondingly.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Electrodeposition and Electroless Coatings · Corrosion Behavior and Inhibition · Metal and Thin Film Mechanics
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (41)
Show source-provided references
1. Cavitation erosion of materials10.1179/imr.1986.31.1.1 ↗
2. Cavitation erosion–corrosion behaviour of CrMnB stainless overlay and 0Cr13Ni5Mo stainless steel in 0.5 M NaCl and 0.5 M HCL solutions10.1016/j.triboint.2008.02.011 ↗
3. Ultrasonic cavitation erosion of gas nitrided Ti-6Al-4V alloys10.1016/j.ultsonch.2014.01.005 ↗
4. Cavitation erosion of plasma-sprayed CoMoCrSi coatings10.1016/j.triboint.2016.06.014 ↗
5. Cavitation protection by low temperature TiCN coatings10.1016/0257-8972(95)08265-4 ↗
6. Synergistic effects of cavitation erosion and corrosion for nickel aluminium bronze with oxide film in 3.5% NaCl solution10.1016/j.wear.2017.01.047 ↗
7. Different methods of measuring synergy between cavitation erosion and corrosion for nickel aluminium bronze in 3.5% NaCl solution
8. The synergistic effects of cavitation erosion–corrosion in ship propeller materials10.1007/s40735-015-0012-1 ↗
9. Implications of solution treatment on cavitation erosion and corrosion resistances and synergism of austenitic stainless steel10.1016/j.wear.2017.09.024 ↗
10. Laser-fabricated Fe-Ni-Co-Cr-B austenitic alloy on steels. Part II. Corrosion behaviour and corrosion-erosion synergism10.1016/S0257-8972(01)01292-0 ↗
11. Synergistic effect of cavitation erosion and corrosion of various engineering alloys in 3.5 % NaCl solution10.1016/S0921-5093(00)00899-6 ↗
12. Effect of ultrasonic cavitation erosion on corrosion behavior of high-velocity oxygen-fuel (HVOF) sprayed near-nanostructured WC–10Co–4Cr coating10.1016/j.ultsonch.2015.01.012 ↗
13. The synergistic effect of cavitation erosion and corrosion of nickel-aluminum copper surface layer on nickel-aluminum bronze alloy10.1016/j.jallcom.2018.03.103 ↗
14. Hong
15. Relationship between cavitation structures and cavitation damage10.1016/j.wear.2004.08.004 ↗
16. Correlation of cavitation erosion behavior with mechanical properties of metals10.1016/0043-1648(90)90122-Q ↗
17. Analysis of mechanical and chemical mechanisms on cavitation erosion- corrosion of steels in salt water using electrochemical methods10.1016/j.triboint.2018.04.012 ↗
18. Effect of heat treatment on the structure, cavitation erosion and erosion-corrosion behavior of Fe-based amorphous coatings10.1016/j.triboint.2015.04.039 ↗
19. Exceptional cavitation erosion-corrosion behavior of dual-phase bimodal structure in austenitic stainless steel10.1016/j.triboint.2019.01.018 ↗
20. Correlation of microstructure with cavitation erosion behaviour of a nickel-aluminum bronze in simulated seawater10.1016/j.triboint.2019.03.071 ↗
21. Cavitation erosion of electroplated nickel composite coatings10.1016/j.surfcoat.2008.02.004 ↗
22. 2010 · 1
23. Electrodeposition of nickel/SiC composites in the presence of cetyltrimethylammonium bromide10.1016/j.apsusc.2010.05.082 ↗
24. The effects of electrodeposition current density on properties of Ni-CNTs composite coatings10.1016/j.surfcoat.2007.11.032 ↗
25. The effect of SDS surfactant on tensile properties of electrodeposited Ni-Co/SiC nanocomposites10.1016/j.msea.2012.08.145 ↗
26. Electrolytic composite Ni-PTFE coatings: an adaptation of Guglielmi's model for the phenomena of incorporation10.1016/S0257-8972(02)00180-9 ↗
27. Kinetics of the deposition of inert particles from electrolytic baths
28. Effect of CTAB concentration in the electrolyte on the tribological properties of nanoparticle SiC reinforced Ni metal matrix composite (MMC) coatings produced by electrodeposition10.1016/j.colsurfa.2012.11.048 ↗
29. Electrodeposition of Ni-SiC nano-composite coatings and evaluation of wear and corrosion resistance and electroplating characteristics10.1016/j.colsurfa.2007.07.027 ↗
30. Bestimmung der Größe und der inneren Struktur von Kolloidteilchen mittels Röntgenstrahlen, Nachrichten von Der Gesellschaft Der Wissenschaften Zu Göttingen
31. Hussain · 2018
32. Symposium on internal stresses in metals and alloys
33. A study of the erosion-corrosion behaviour of engineering steels for marine pumping applications10.1016/0043-1648(95)07145-8 ↗
34. Impedance spectroscopy at interfaces of metals and aqueous solutions - surface roughness, CPE and related issues10.1016/j.ssi.2004.06.023 ↗
35. Evaluation of model and dispersion parameters and their effects on the formation of constant-phase elements in equivalent circuits10.1016/S0022-0728(98)00471-9 ↗
36. The analysis of electrode impedances complicated by the presence of a constant phase element10.1016/S0022-0728(84)80324-1 ↗
37. Electrochemical impedance spectroscopy study on silver coated metallic implants10.1016/j.electacta.2011.01.072 ↗
38. Cavitation erosion resistance and wear mechanisms of active screen low temperature plasma nitrided AISI 410 martensitic stainless steel10.1016/j.wear.2014.12.009 ↗
39. 2016 · 1–6
40. Influence of surface mechanical attrition treatment ( SMAT ) on the corrosion behaviour of AISI 304 stainless steel10.1016/j.corsci.2013.04.056 ↗
41. A study of cavitation erosion of cast iron10.1016/0043-1648(83)90271-5 ↗