Simulation and experiment based investigations of squat formation mechanisms
Source abstract
Abstract
Abstract In this work, possible formation mechanisms of squats were investigated based on field and laboratory measurements, full-scale wheel-rail test rig experiments and a newly developed simulation tool. Wheel-rail contact conditions were found, which can lead to cracks in or to outbreaks of a white etching layer (WEL) on a rail surface. Under certain condition this also can lead to cracks growing into the bulk material. Furthermore, according to the simulation results, geometrical deviations of the rail surface - as for example outbreaks of WELs - can remain at the rail surface and grow up to a size comparable to that of squats. It has been shown, that the crack initiation potential in the area of such permanent geometrical deviations can be increased.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Railway Engineering and Dynamics · Mechanical stress and fatigue analysis · Electrical Contact Performance and Analysis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (28)
Show source-provided references
1. Squats and squat-type defects in rails: the understanding to date10.1177/0954409711422189 ↗
2. Metallurgical aspects of surface damage problems in rails
3. Squat growth—some observations and the validation of numerical predictions10.1016/j.wear.2010.10.051 ↗
4. An investigation into the causes of squats- correlation analysis and numerical modeling10.1016/j.wear.2008.02.037 ↗
5. Zhao · 2012
6. “Studs”: a squat-type defect in rails10.1177/0954409711421462 ↗
7. The epidemiology of squats and related defects
8. The development of squat defects under high axle load operations
9. Early stages of rails squat formation and the role of a white etching layer10.1016/j.ijfatigue.2013.02.016 ↗
10. Metallurgical and physical understanding of rail squat initiation and propagation10.1016/j.wear.2012.02.013 ↗
11. Rolling contact fatigue of white etching layer: Part 1 crack morphology10.1016/j.wear.2007.01.003 ↗
12. Rolling contact fatigue of white etching layer: Part 2. Numerical results10.1016/j.wear.2007.01.002 ↗
13. Tribological characterization of rail squat defects10.1016/j.wear.2012.11.011 ↗
14. The squat condition of rail materials – a novel approach to squat prevention
15. Ein neuer Zugang zum besseren Verständnis von Squats
16. Bernsteiner · 2018
17. The determination of critical size for rail top surface defects to grow into Squats
18. Development of white etching layer on rails: simulations and experiments10.1016/j.wear.2016.03.028 ↗
19. Residual stresses generated by repeated local heating events – modelling of possible mechanisms for crack initiation10.1016/j.wear.2016.05.029 ↗
20. Kalker · 1967
21. Vollebregt · 2016
22. Plasticity in wheel-rail contact and its implications on vehicle-track interaction10.1177/0954409716673118 ↗
23. Meierhofer · 2015
24. Wear of wheel-rail surfaces10.1016/0043-1648(86)90060-8 ↗
25. Trummer · 2016
26. Modeling surface rolling contact fatigue crack initiation taking severe plastic shear deformation into account10.1016/j.wear.2016.02.008 ↗
27. Tribological properties of the surface of railway tracks, studied by indentation technique10.1016/j.wear.2004.02.017 ↗
28. Suh · 1977