Comparative analysis of fretting wear behavior of steel wire subject to tensile-torsional coupling forces in typical mining environments
Source abstract
Abstract
The complex mining environments can significantly accelerate the fretting wear among steel wires within wire rope, thereby diminishing its service life and posing severe risks to the safety of mine hoisting operations. To explore the fretting behavior of steel wires featuring complex contact structures in typical mining environments, a customized test rig was utilized to perform fretting wear experiments of steel wire under tensile-torsional coupling forces. The findings indicate that with increasing contact force, the coefficient of friction (CoF) between steel wires in different environments decreases, whereas the frictional force and wear degree increase significantly. The wear depth and wear coefficient under peak contact structure are markedly larger than those under valley contact structure. For the same contact force, the wear of steel wire without lubrication is the largest, the wear under water lubrication is the second, and the wear under grease lubrication is the least. The primary wear mechanisms of steel wire under grease lubrication are abrasive wear and fatigue wear. The presence of mineral particles in the grease can reduce the CoF, but it will exacerbate the wear and result in adhesive wear characteristics on the wear surfaces. Under no lubrication and water lubrication conditions, the wear mechanisms encompass abrasive wear, adhesive wear and fatigue wear. Furthermore, with increasing contact force, the fatigue wear of steel wire under no lubrication intensifies, while the abrasive wear characteristics become more pronounced under water lubrication.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Mechanical stress and fatigue analysis · Electrical Contact Performance and Analysis · Vibration and Dynamic Analysis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (31)
Show source-provided references
1. Comparative analyses of torsional fretting, longitudinal fretting and combined longitudinal and torsional fretting behaviors of steel wires10.1016/j.engfailanal.2017.12.002 ↗
2. Tribological behavior and mechanical properties of transmission wire rope bending over sheaves under different sliding conditions
3. Tribo-fatigue behaviors of steel wires under coupled tension-torsion in different environmental media10.1016/j.wear.2018.12.038 ↗
4. Friction and wear behavior of multiple steel wires with different corrosion extents under different lubrication conditions
5. Influence of different mineral particles in lubricating grease on the fretting behavior between steel wires under different contact forms
6. Studies on failure behaviour of wire rope used in underground coal mines10.1016/j.engfailanal.2016.09.002 ↗
7. Studies on friction and wear characteristics of wire rope used in multi-layer winding hoist during inter-circle transition under dry friction10.1177/13506501211009418 ↗
8. Sliding friction and wear behavior of winding hoisting rope in ultra-deep coal mine under different conditions
9. Influence of longitudinal vibration on the friction and wear characteristics of multi-layer winding hoisting wire rope
10. Tribological behavior of octadecylamine functionalized graphene oxide modified oil for wire rope in mine hoist
11. The friction and wear properties of steel wire rope sliding against itself under impact load10.1016/j.wear.2018.01.010 ↗
12. Fretting fatigue behavior of steel wires contact interface under different crossing angles10.1016/j.wear.2017.12.014 ↗
13. Fretting wear of thin steel wires. Part 2: influence of crossing angle10.1016/j.wear.2011.04.012 ↗
14. Fretting wear of thin steel wires. Part 1: influence of contact pressure10.1016/j.wear.2010.02.017 ↗
15. Comparative research on failure mechanisms of steel wire ropes during bending fatigue under constant and variable loads
16. Fretting wear behaviors of steel wires in coal mine under different corrosive mediums10.1016/j.wear.2011.03.028 ↗
17. Numerical study on wear evolution and mechanical behavior of steel wires based on semi-analytical method10.1016/j.ijmecsci.2018.09.030 ↗
18. Semi-analytical analysis of the interwire multi-state contact behavior of a three-layered wire rope strand10.1016/j.ijsolstr.2020.06.004 ↗
19. Fretting fatigue behavior of steel wires contact interface under different crossing angles10.1016/j.wear.2017.12.014 ↗
20. Effect of fretting frequency on tension-torsion fretting corrosion fatigue behavior of steel wire
21. Effect of torsion angle on tension-torsion multiaxial fretting fatigue behaviors of steel wires10.1016/j.ijfatigue.2017.09.021 ↗
22. Effects of tensile stress ratio and amplitude on tension-torsion fretting-corrosion-fatigue behaviors of non-perpendicularly crossed steel wires10.1016/j.engfailanal.2020.104839 ↗
23. Prediction of fretting fatigue crack propagation life of steel wire considering fretting wear
24. Fretting friction and wear of steel wires in tension-torsion and helical contact form
25. Fretting behaviors of steel wires with tensile-torsional coupling force under different wire diameters and crossing angles10.1007/s11249-020-01331-8 ↗
26. Fretting tribological behaviors of steel wires under lubricating grease with compound additives of graphene and graphite
27. Fretting wear behaviors of steel wires under friction-increasing grease conditions10.1016/j.triboint.2010.10.021 ↗
28. Experimental study on corrosion-fretting fatigue behavior of bridge cable wires10.1061/(ASCE)BE.1943-5592.0001642 ↗
29. Quantitative demonstration of wear rate and dissipation energy during tension-torsion cyclic loading of steel wires with fretting contact in different environmental media10.3390/app10186610 ↗
30. Effect of various kinematic parameters of mine hoist on fretting parameters of hoisting rope and a new fretting fatigue test apparatus of steel wires10.1016/j.engfailanal.2012.01.008 ↗
31. Vibration-worn characteristics of winding hoisting wire rope in mine under mineral dust environment