Effect of Ag nanoparticles on the tribological response of MAO coatings fabricated on plastically deformed titanium
Source abstract
Abstract
The effect of silver nanoparticles (Ag-NPs) concentration in the electrolyte during micro-arc oxidation (MAO) of plastically deformed titanium of commercial purity (cp-Ti) on microstructure, adhesion and tribological performance of produced coatings was investigated within the present work. Although the effect of the Ag-NPs on the antibacterial properties and biocompatibility of MAO coatings has been barely investigated, the tribological behaviors such as sliding and fretting wear have been studied in detail. The application of phosphate-based electrolyte allowed to effectively incorporate the Ag-NPs into the MAO coating, particularly on their upper surface, without agglomeration, and in the areas close to the pores. Such a distribution of the Ag-NPs influences the scratch and wear resistance, delaying the cracking of the coating (by increasing L C1 critical load) and acting as a solid lubricant decreasing the coefficient of friction, respectively. A reduction in sliding wear rate was observed for the MAO coatings with added Ag-NPs, with a lowest value recorded for the material with 1 g/l of Ag-NPs suspended in the electrolyte (1.34·10 -6 mm 3 /N·m) as compared with the reference material without NPs (2.57·10 -6 mm 3 /N·m). A slight increase in wear rate was stated for 2 g/l (1.86·10 -6 mm 3 /N·m). The tribological response of the MAO coating with conductive Ag-NPs is governed by two competing phenomena: increasing amount of solid state lubricant (Ag-NPs) but increasingly more porous coating at the same time (due to more intense micro-arcing in the electrolyte of higher conductivity) deteriorating the wear resistance. • MAO coatings with Ag-NPs were deposited on cp-Ti substrates • Ag embed into MAO coating in original form on its upper surface and near porosity • Addition of Ag-NPs, acting as solid lubricants, reduced the friction coefficient • Wear rate reaches a minimum for the MAO coating with 1 g/l of Ag-NPs • Soft Ag-NPs on the upper surface helped to delay crack formation and propagation
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Titanium Alloys Microstructure and Properties · Magnesium Alloys: Properties and Applications · Metal and Thin Film Mechanics
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (45)
Show source-provided references
1. Leyens · 2003
2. Titanium-based alloys and composites for orthopedic implants applications: a comprehensive review10.1016/j.matdes.2024.112850 ↗
3. Mechanical and clinical properties of titanium and titanium-based alloys (Ti G2, Ti G4 cold worked nanostructured and Ti G5) for biomedical applications10.1016/j.jmrt.2018.07.016 ↗
4. The tribological properties of nano-titanium obtained by hydrostatic extrusion10.1016/j.wear.2006.11.047 ↗
5. Research progress of laser cladding on the surface of titanium and its alloys10.3390/ma16083250 ↗
6. Optimized mechanical properties of the hot forged Ti–6Al–4V alloy by regulating multiscale microstructure via laser shock peening10.1016/j.ijmachtools.2024.104192 ↗
7. Enhancing the tribological performance of MAO coatings through hydrostatic extrusion of cp-Ti10.1016/j.jallcom.2024.178246 ↗
8. An alternative approach for producing electrolytic coatings to enhance corrosion resistance of biodegradable magnesium alloy10.24425/amm.2025.156238 ↗
9. Advancements in plasma electrolytic oxidation with particle suspensions: a novel approach for the direct incorporation of calcium carbonate10.1016/j.apsusc.2025.164360 ↗
10. Improved lubricating and corrosion resistance of MAO coatings on ZK61 Mg alloy by co-doping with graphite and nano-zirconia10.1016/j.jmrt.2024.09.232 ↗
11. Tailoring the corrosion resistance and biological performance of Mg-Zn-Y-Nd bioimplants with multiphasic, pore-sealed cerium-doped ceramic coatings via facile one-pot plasma electrolytic oxidation10.1016/j.jmst.2025.01.016 ↗
12. Influence of the micro-arc oxidation (MAO) parameters on surface properties of the hydroxyapatite and hydroxyapatite - carbon nanotube coatings formed on the Ti13Nb13Zr alloy10.2478/adms-2025-0014 ↗
13. Electrolyte-mediated incorporation of ZnO nanoparticles into TiO2 coatings on Cp titanium via PEO
14. Establishing the intrinsic connection between microstructure, 3D defects, and the corrosion behavior of selective laser melted WE43 alloys10.1007/s12598-025-03463-z ↗
15. Phosphate porous coatings enriched with selected elements via PEO treatment on titanium and its alloys
16. Enhancing fretting corrosion resistance of micro-arc oxidation coating with Y2O3 nanoparticles on biomedical Ti6Al4V alloy for hip implants10.1016/j.surfcoat.2025.132468 ↗
17. Comparative study on fretting wear behavior of micro-arc oxidation coatings formed in aluminate, phosphate, and silicate electrolytes on Ti6Al4V alloy10.1016/j.wear.2026.206512 ↗
18. Microstructure, mechanical properties and fretting corrosion behavior of micro-arc oxide coatings on biomedical Ti6Al4V alloy for modular hip implant: effect of Na2SiO3/KOH electrolyte concentration10.1016/j.matchemphys.2026.132068 ↗
19. Fretting corrosion behaviors and wear–corrosion synergistic interaction of bare and micro-arc-oxidized Ti6Al4V ELI in different fretting regimes10.1016/j.triboint.2025.111394 ↗
20. A review on the synthesis of the various types of anatase TiO2 facets and their applications for photocatalysis10.1016/j.cej.2019.123384 ↗
21. Green synthesis, characterization and medicinal uses of silver nanoparticles (Ag-NPs), copper nanoparticles (Cu-NPs) and zinc oxide nanoparticles (ZnO-NPs) and their mechanism of action: a review10.1016/j.bcab.2023.103006 ↗
22. The synergistic effect of MAO-treated and PAO–graphene oil on tribological properties of Ti6Al4V alloys
23. Comparative study on fretting wear behavior of micro-arc oxidation coatings formed in aluminate, phosphate, and silicate electrolytes on Ti6Al4V alloy10.1016/j.wear.2026.206512 ↗
24. Influence of alumina and zirconia incorporations on the structure and wear resistance of titania-based MAO coatings10.1016/j.surfcoat.2019.124900 ↗
25. Synthesis of zirconia-incorporated titania layer by microarc oxidation for biomedical applications10.1002/sia.5869 ↗
26. Improved lubricating and corrosion resistance of MAO coatings on ZK61 Mg alloy by co-doping with graphite and nano-zirconia10.1016/j.jmrt.2024.09.232 ↗
27. Effect of nano-ZrO2 particles on corrosive and abrasive performances of the micro-arc oxidized ceramic film on TC4 alloy surface
28. Review on the application of additives in micro-arc oxidation of titanium alloy
29. An electron microscopical study on the growth of TiO2–Ag antibacterial coatings on Ti6Al7Nb biomedical alloy10.1016/j.actbio.2011.02.037 ↗
30. In-situ formation of Ag nanoparticles in the MAO coating during the processing of cp-Ti10.1038/s41598-023-29999-7 ↗
31. Antibacterial activity of a porous silver doped TiO2 coating on titanium substrates synthesized by plasma electrolytic oxidation10.1016/j.apsusc.2019.144235 ↗
32. Surface modification of Ti6Al4V by micro-arc oxidation in AgC2H3O2-containing electrolyte10.1680/jsuin.18.00007 ↗
33. Effects of concentration of Ag nanoparticles on surface structure and in vitro biological responses of oxide layer on pure titanium via plasma electrolytic oxidation10.1016/j.apsusc.2015.04.161 ↗
34. Conductivity and flexibility enhancement of aerosol-jet-printed sensors using a silver nanoparticle ink with carbon nanotubes10.24425/amm.2024.149754 ↗
35. Tribological properties of PEO nanocomposite coatings on titanium formed in electrolyte containing ketoconazole10.1016/j.triboint.2016.06.013 ↗
36. Friction and wear characteristics of micro-arc oxidation coating on Ti6Al4V alloy—A review10.1049/bsb2.70000 ↗
37. Nanostructured oxide composites in PEO coating of β Ti alloys with low elastic modulus for biomedical applications10.1016/j.triboint.2025.110677 ↗
38. Effect of silicate-based/phosphate-based electrolyte on mechanism of incorporation of ZnO nanoparticles into MAO coating fabricated on titanium
39. Effect of Ag concentration on structure and wear behaviour of coatings formed by micro-arc oxidation on Ti6Al4V alloy10.1080/02670844.2020.1741211 ↗
40. Lubricating and conductive properties of modified graphene/silver nanoparticles under current-carrying friction conditions10.3390/lubricants13010038 ↗
41. Fabrication and tribological properties of polyelectrolyte multilayers containing in situ gold and silver nanoparticles10.1016/j.colsurfa.2012.08.044 ↗
42. Enhancing dry sliding wear resistance of pure Mg by plasma electrolytic oxidation ceramic coatings using silver addition
43. Comparative study on the fretting and sliding wear properties of micro-arc oxidation-treated aluminum alloy at different temperatures10.1016/j.triboint.2024.109847 ↗
44. Nanocomposite coatings for anti-corrosion properties of metallic substrates10.3390/ma16145092 ↗
45. The effect of Ag content modulation and frictional heat on the fretting wear resistance of Fe2O3-Ag composite coatings