journal article·2005-07

Low wear and friction of nanometer-thick Ag layers on Si(111) surfaces

F. Honda, M. Goto

Wear· Volume 259· Issue 1-6
Publisher page

Abstract

Abstract Tribological performance of sub-nano to nanometer-thick Ag layers deposited on Si(1 1 1) have been examined to understand the effect of surface thin layers to the wear and friction characteristics. The slider was made of diamond sphere of 3 mm in diameter. Sliding tests were carried out in an ultra-high vacuum environment (lower than 2 × 10−8 Pa) and analyzed in situ by Auger electron spectroscopy (AES) for the quantitative thickness-measurements, by reflection high-energy electron diffraction (RHEED) to clarify the substrate cleanliness and crystallography of the Ag films, and by scanning probe microscopy (SPM) for the morphology of the deposited/slid film surfaces. The Ag and substrate surfaces were atomically clean during the tribological tests so that the chemical effect of the Ag and Si surfaces appeared directly on the friction and wear processes. Experimental results of the sliding tests indicated that the minimum coefficient of friction (μ) was 0.007 for the 1–5 nm thick as-deposited films of Ag on a Si(1 1 1) surface. Beyond the minimum thickness region, μ increased to 0.01 or higher. Observations of the slid surfaces showed that the Ag(1 1 1) sliding planes orientate parallel to the sliding direction, although the surface morphology of the deposited surface was totally deformed by the slider on the track. The Ag crystallites were not, therefore, destructed crystallographically by sliding but the fine Ag(1 1 1) sliding sheets were rotated, sheared, and displaced layer by layer, to orientate the Ag(1 1 1) plane parallel to the sliding direction by the reciprocal movement of the slider. After 100 cycles of the reciprocal movements, no worn particles were found around the sliding track and the low friction sliding lasted over 1000 cycles of the reciprocal sliding. The observed results indicated that the atomic force between surface atoms, especially diamond C Ag chemical bond, Ag(1 1 1) interlayer bonding force, and also the orientation of the sliding planes strongly reflect to the friction force, in addition to the asperity of the surface. A sliding mechanism of very thin layers of Ag film of very low wear and friction is discussed.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Diamond and Carbon-based Materials Research · Force Microscopy Techniques and Applications · Metal and Thin Film Mechanics

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (10)

Show source-provided references
1. Film thickness effect of Ag lubricant layer in the nano region10.1016/S0043-1648(03)00530-1 ↗
2. Extremely low coefficient of friction of diamond sliding against Ag thin films on Si(111) surface under ultra-high vacuum10.1016/S0043-1648(02)00036-4 ↗
3. Nachweis grober Schmeltpunkts erniedigungen bei dunnen Metallschichten10.1002/pssb.19660150116 ↗
4. Adhesion and friction of single crystal diamond in contact with transition metals10.1016/0378-5963(80)90142-7 ↗
5. The effects of speed, film thickness, and substrate surface roughness on the friction and wear of soft metal films in ultrahigh vacuum10.1016/0040-6090(78)90226-2 ↗
6. Super lubricity of diamond sliding on the Ag monolayer/Si(111) and the effect of gas adsorption10.1016/S0039-6028(02)01408-5 ↗
7. The low friction of a diamond/H-terminated Si(111) sliding system10.1109/TMAG.2003.808918 ↗
8. The formation of hydrogen passivated silicon single-crystal surfaces ultraviolet cleaning and HF etching10.1063/1.341489 ↗
9. Surface structure and surface conductance during metal adsorption on semiconductors10.1142/S0218625X97001140 ↗
10. Correlation between atomic-scale structures and macroscopic electrical properties of metal covered Si(111) surfaces10.1142/S0217979293003504 ↗