journal article·2011-07Open access

Effect of low-temperature plasma carbonitriding on the fretting behaviour of 316LVM medical grade austenitic stainless steels

J. Liu, H. Dong, J. Buhagiar, C.F. Song, B.J. Yu, L.M. Qian, Z.R. Zhou

Wear· Volume 271· Issue 9-10

Abstract

Abstract An optimized low-temperature plasma carbonitriding process at 430 °C for 15 h was used to treat the surface of 316LVM medical grade austenitic stainless steel. By using a servo-hydraulic dynamic test machine, the fretting behaviour of both as-received and the surface-treated 316LVM plate samples against martensitic stainless steel balls was studied in the Ringer's solution at various displacement amplitudes. The experimental results demonstrate that the optimized low-temperature plasma surface treatment can produce a precipitate-free, C/N supersaturated S-phase layer. Such layer revealed a hardness of 5 times that of 316LVM substrate. The formation of S-phase can protect the 316LVM from corrosion in the Ringer's solution, and the hard surface-treated layer can significantly improve the fretting wear resistance of 316LVM material. When fretted in a mixed regime, a sharp drop of friction force was observed for untreated 316LVM after fretting for about 1000 cycles, which was mainly caused by the penetration of Ringer's solution into the contact area of the fretting pairs. As a comparison, no friction drop was observed through the fretting process on the surface-treated samples. Due to the high ratio of elastic modulus to hardness (E/H) of untreated sample, the main damage mechanism on untreated sample was adhesive and abrasive wear during the fretting process. However, because of the high hardness and low E/H ratio of the surface-treated sample, the main damage mechanism was mild abrasive wear. In conclusion, the low temperature plasma surface treatment can effectively improve the fretting wear properties of 316LVM stainless steel, which could pave the way to develop the high-performance, long-life body implants.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Metal and Thin Film Mechanics · Mechanical stress and fatigue analysis · Metal Alloys Wear and Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (18)

Show source-provided references
1. S-phase surface engineering of Fe–Cr, Co–Cr and Ni–Cr alloys10.1179/095066009X12572530170589 ↗
2. Friction, wear and microstructure of unlubricated austenitic stainless steels10.1016/0043-1648(80)90247-1 ↗
3. Surface property enhancement of Ni-free medical grade austenitic stainless steel by low-temperature plasma carburizing10.1016/j.surfcoat.2010.06.062 ↗
4. Fretting wear of stainless steels under variable temperature conditions: introduction of a ‘composite’ wear law10.1016/j.wear.2009.08.029 ↗
5. Characteristics of a plasma electrolytic nitrocarburising treatment for stainless steels10.1016/S0257-8972(01)01025-8 ↗
6. Study on CN ion implantation austenitic stainless steel
7. Tribological properties of plasma nitrided stainless steel against SAE52100 steel under ionic liquid lubrication condition10.1016/j.triboint.2005.04.030 ↗
8. Corrosion behavior of ion nitrided AISI 316L stainless steel10.1016/j.tsf.2007.08.072 ↗
9. Effect of surface treatment on the fretting wear behavior of medical grade austenitic stainless steels
10. S-phase in stainless steels: an overview
11. Study on surface performance of biomedical metallic materials implanted by nitrogen ion
12. Mixed fretting regime10.1016/0043-1648(94)07081-4 ↗
13. A general equation for fitting contact area and friction vs load measurements10.1006/jcis.1998.6027 ↗
14. Material effects in fretting wear: application to iron, titanium, and aluminium alloys10.1007/BF02667367 ↗
15. Improving the erosion–corrosion resistance of AISI 316 austenitic stainless steel by low-temperature plasma surface alloying with N and C10.1016/j.msea.2006.05.122 ↗
16. Quantitative characterization of scratch and mar behavior of polymer coatings10.1016/S0921-5093(01)01159-5 ↗
17. Effect of displacement amplitude in oil-lubricated fretting10.1016/S0043-1648(00)00323-9 ↗
18. Adhesion and abrasive wear resistance of TiN deposited on electrical discharge machined WC–Co cemented carbides10.1016/j.wear.2007.11.016 ↗