Interface adhesion during sliding wear in cast iron after hot deformation

Q. Zhang, Z.Y. Jiang, D.B. Wei, H.T. Zhu, Z.X. Chen, J.T. Han, G.L. Xie

Wear· Volume 301· Issue 1-2
Publisher page

Abstract

Abstract Interface adhesion between cast iron substrate and oxide layer formed during dry unidirectional sliding wear was studied by using thermo-mechanically processed 4.8Ni–1.5Cr cast iron. The purpose of the present work is to reveal the difference of the adhesion behaviour between martensitic matrix with a higher hardness and austenitic matrix with low hardness. The 4.8Ni–1.5Cr alloy was sandwiched as a middle layer with low carbon steel as outer layers and thermo-mechanically processed via (1) hot rolling (HR), (2) hot rolling and heat treatment (HT), and (3) hot rolling, heat treatment and hot compression (HC), respectively. The applied normal loads were 20 and 40 N, and the sliding speeds were 45 and 78 mm/s in sliding wear test. The durations of the wear test were 2 and 7 min, respectively for different testing rounds. It was found that the wear after running-in was always mild under the conditions of 20 N and 45 mm/s or 20 N and 78 mm/s for all the tested samples. Prior to the transition into mild oxidational wear, negative displacements of pins were observed for HT and HC samples when the applied load was raised to 40 N at the sliding speed of 78 mm/s. No similar response was observed for HR sample under the same testing condition. The possible mechanisms for the negative displacement of pin in the test are discussed in terms of the microstructure and phases of the testing samples. The effect of the hardness of the substrate on the growth and integrity of the oxide film formed during the sliding and the interface adhesion between the oxide film and substrate are also discussed.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Metal Alloys Wear and Properties · Mechanical stress and fatigue analysis · High Entropy Alloys Studies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (35)

Show source-provided references
1. Microstructure-property relationships in high chromium white iron alloys10.1179/095066096790326075 ↗
2. The formability of spray-formed, high-chromium content, white cast iron10.1023/A:1006685809567 ↗
3. The effect of processing route, composition and hardness on the wear response of chromium bearing steels in a rolling-sliding configuration10.1016/S0043-1648(96)07391-7 ↗
4. The effect of spray forming on the microstructure and properties of a high chromium white cast iron10.1023/A:1004573524282 ↗
5. The rolling/sliding wear response of conventionally processed and spray formed high chromium content cast iron at ambient and elevated temperature10.1016/S0043-1648(99)00053-8 ↗
6. Fabrication of high chromium cast iron/low carbon steel composite material by cast and hot rolling process10.1016/j.matdes.2010.01.014 ↗
7. Review of oxidational wear.1. The origins of oxidational wear10.1016/0301-679X(83)90086-5 ↗
8. The role of oxidation in the wear of alloys10.1016/S0301-679X(98)00008-5 ↗
9. The influence of oxides on the friction and wear alloys10.1016/0301-679X(78)90178-0 ↗
10. Self-formation of protective oxide-films at dry sliding mild-steel surfaces under a medium vacuum10.1016/0043-1648(94)07042-3 ↗
11. On the critical thickness of protective films at sliding interfaces10.1016/0043-1648(84)90115-7 ↗
12. The role of triboparticulates in dry sliding wear10.1016/S0301-679X(98)00027-9 ↗
13. Formation and wear mechanism of tribo-oxides and the regime of oxidational wear of steel10.1016/S0043-1648(02)00230-2 ↗
14. Effect of hot-spot temperatures on unlubricated wear of steel10.1080/05698196708972175 ↗
16. Development of wear-protective oxides and their influence on sliding friction10.1098/rspa.1980.0016 ↗
17. Origins and development of oxidational wear at low ambient temperatures10.1016/0043-1648(84)90053-X ↗
18. The effect of ΔT (oxidizing temperature minus cooling temperature) on oxide spallation10.1007/BF00612137 ↗
19. The role of hard second phases in the mild oxidational wear mechanism of high-speed steel-based materials10.1016/0043-1648(94)90262-3 ↗
20. The mechanism of oxidational wear10.1016/0043-1648(94)06569-1 ↗
21. High resolution observations of friction-induced oxide and its interaction with the worn surface10.1016/S0301-679X(02)00040-3 ↗
22. The unlubricated sliding wear of steels: the role of the hardness of the friction pair10.1016/0043-1648(93)90272-N ↗
23. Effects of the tribo-oxide and matrix on dry sliding wear characteristics and mechanisms of a cast steel10.1016/j.wear.2010.04.028 ↗
24. The effects of load and substrate hardness on the development and maintenance of wear-protective layers during sliding at elevated temperatures10.1016/S0043-1648(01)00601-9 ↗
25. Wear of metals at high sliding speeds10.1016/0043-1648(77)90089-8 ↗
26. Prow formation in the wear of cast iron10.1016/0043-1648(84)90090-5 ↗
27. Influence of hardness of the harder body on wear regime transition in a sliding pair of steels10.1016/j.wear.2008.11.019 ↗
28. Effect of temperature on the sliding wear performance of Al alloys and Al matrix composites10.1016/0043-1648(96)06923-2 ↗
29. Characteristics of wear results tested by pin-on-disc at moderate to high speeds10.1016/0301-679X(95)00097-N ↗
30. The dry wear of steels I. The general pattern of behaviour10.1098/rsta.1965.0001 ↗
31. Sliding wear of metals10.1146/annurev.ms.18.080188.001041 ↗
32. Analysis for wear behaviours of oxidative wear10.1007/s11249-010-9741-y ↗
33. Comments on the sliding of wear of metals10.1016/S0301-679X(96)00065-5 ↗
34. Surface aspects of unlubricated metal-to-metal wear10.1016/0043-1648(71)90073-1 ↗
35. Mechanisms of dry wear of some martensitic steels10.1016/0043-1648(75)90121-0 ↗