journal article·2015-05Open access

Role of atomic layer deposited solid lubricants in the sliding wear reduction of carbon–carbon composites at room and higher temperatures

H. Mohseni, T.W. Scharf

Wear· Volume 332-333

Abstract

High frequency reciprocating sliding wear behavior and mechanisms were investigated at 25, 150 and 400 °C for solid lubricant oxide coated carbon–carbon composites (CCC). Atomic layer deposition (ALD) was employed to infiltrate a trilayer nanolaminate coating of ZnO/Al2O3/ZrO2 into the porous CCC. The ALD coatings exhibited excellent conformality and pore-filling down to ~55 μm into the CCC, which cannot be achieved by other coating techniques. Compared to uncoated CCC, ALD infiltration resulted in a 64% improvement in the wear rate to 1.5×10−6 mm3/N·m at 25 °C, while a 31% improvement was determined during 150 °C sliding. Conversely, higher temperature sliding at 400 °C resulted in increasing wear rates by an order of magnitude due to combined oxidation of the steel counterface and exposed CCC. Cross-sectional focused ion beam-transmission electron microscopy (FIB-TEM) studies of the worn surfaces were performed to elucidate the solid lubrication mechanisms. It was determined that a highly deformed composite surface tribolayer of nanolaminate coating and amorphous C was responsible for improved sliding wear compared to the uncoated CCC that just exhibited an amorphous C tribolayer. Inside the deformed composite tribolayer, a high density of near surface ZnO (0002) basal plane sliding/shear-induced stacking faults was observed in comparison to unworn ALD nanolaminates. Activating subsurface basal stacking faults in ALD ZnO promotes intrafilm shear/slip and hence improves wear resistance. The slip of partial dislocations results from a dislocation glide process along the ZnO (0002) basal planes. Thus, ALD ZnO/Al2O3/ZrO2 nanolaminate coatings are potential candidates for providing wear reduction from low to intermediate temperatures in moving mechanical assembles, such as CCC bushings that experience fretting-type wear.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Metal and Thin Film Mechanics · Diamond and Carbon-based Materials Research · Tribology and Wear Analysis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (33)

Show source-provided references
1. Savage · 1993 · 85
2. Carbon-carbon composites: oxidation behavior and coatings protection
3. Fitzer · 1998
4. Stachowiak · 2005 · 621
5. Fretting fatigue and fretting wear10.1016/0301-679X(89)90081-9 ↗
6. Waterhouse · 1992 · Vol. 18 · 242
7. Stachowiak · 2005 · 419
8. Atomic layer deposition
9. Chemical vapor deposition and atomic layer deposition of coatings for mechanical applications10.1007/s11666-009-9364-8 ↗
10. Atomic layer deposition of ZnO/Al2O3/ZrO2 nanolaminates for improved thermal and wear resistance in carbon–carbon composites10.1116/1.3669518 ↗
11. Fundamental investigations of fretting fatigue: Part 5, the effect of relative slip amplitude10.1299/jsme1958.12.692 ↗
12. Chameleon coatings: adaptive surfaces to reduce friction and wear in extreme environments10.1146/annurev-matsci-082908-145259 ↗
13. Solid lubricants: a review10.1007/s10853-012-7038-2 ↗
14. Development and characterization of low friction coatings for protection against fretting wear in aerospace components10.1016/j.tsf.2007.07.056 ↗
15. Fretting behaviour of hard coatings under high normal load10.1016/0257-8972(94)90207-0 ↗
16. Solid lubricant materials for high temperatures – A review10.1016/0301-679X(82)90089-5 ↗
17. Wear-resisting oxide films for 900°C
18. Wear engineering oxides/anti-wear oxides10.1016/S0043-1648(98)00181-1 ↗
19. Lubrication using a microstructurally engineered oxide: performance and mechanisms10.1023/A:1019187202237 ↗
20. A crystal chemical approach to the formulation of self-lubricating nanocomposite coatings10.1016/j.surfcoat.2005.08.054 ↗
21. Lubricious oxide coatings for extreme temperature applications: a review10.1016/j.surfcoat.2014.05.064 ↗
22. Tribological and mechanical comparison of sintered and hipped PM212: high temperature self-lubricating composite
23. The effect of counterface on the tribological performance of a high temperature solid lubricant composite from 25 to 650°C10.1016/S0257-8972(96)02959-3 ↗
24. Thermal processing effects on the adhesive strength of PS304 high temperature solid lubricant coatings
25. Oxidation resistant yttrium silicates coating for carbon/carbon composites prepared by a novel in-situ formation method10.1016/j.ceramint.2006.01.007 ↗
26. Preparation of a SiC/cristobalite-AlPO4 multi-layer protective coating on carbon/carbon composites and resultant oxidation kinetics and mechanism10.1016/S1005-0302(10)60168-5 ↗
27. Effect of oxidation inhibitor on the low energy tribological behavior of carbon-carbon composites10.1016/S0008-6223(01)00202-0 ↗
28. W.E. Lee, W.M. Rainforth, Ceramic microstructures: property control by processing, (Springer, London, 1994).
29. Microstructural evolution in lubricious ZnO films grown by pulsed laser deposition10.1016/S0040-6090(99)00880-9 ↗
30. Lubricious zinc oxide films grown by pulsed laser deposition: lateral force microscopy of wear surfaces10.1023/A:1026790330643 ↗
31. Exceptional friction mitigation via subsurface plastic shear in defective nanocrystalline ceramics10.1080/21663831.2014.935968 ↗
32. Tribologically transformed structure in fretting10.1016/S0043-1648(00)00464-6 ↗
33. New insights into the microstructure of the friction surface layer of C/C composites10.1016/j.carbon.2011.06.073 ↗