Rain erosion characteristics of electrodeposited Ni–SiC metal-matrix composite layers
Source abstract
Abstract
Abstract Fibre reinforced plastics (FRP) are finding greater use in aerospace applications. In order to improve the low intrinsic rain erosion resistance of these materials electrodeposited layers consisting of micrometer-sized SiC particles in a Ni matrix were examined. This study presents a microscopic examination of damage caused by water droplet impact at 225 m s −1 , from which it was observed that the SiC particles were selectively removed from the surface of the matrix, causing a slight increase in the surface roughness that tended to a maximum value at 1000–2000 impacts of 2 mm diameter water droplets. The depth-dependent concentration of Si in the Ni matrix was estimated from energy-dispersive X-ray spectroscopy (EDX) measurements by varying the accelerating voltages of a range 5–25 kV and fitting the data using a Monte Carlo simulation method. A layer model was put forward that would account for the observed results, showing that SiC was selectively removed from the upper 0.4 μm of the deposit.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Aerosol Filtration and Electrostatic Precipitation · Surface Modification and Superhydrophobicity · High voltage insulation and dielectric phenomena
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (41)
Show source-provided references
1. Carbon fibre composites poised for dramatic growth10.1016/S0034-3617(09)70148-1 ↗
2. Damage mechanisms in polymers and composites under high-velocity liquid impact
3. The failure of composite materials under high-velocity liquid impact10.1088/0022-3727/9/10/018 ↗
4. High speed liquid impact erosion mechanisms in natural nanocomposites with potential for synthesis for the aerospace industry
5. The erosion of carbon fibre reinforced plastic by repeated liquid impact10.1016/0043-1648(73)90042-2 ↗
6. Indirect damage in composite materials due to raindrop impact10.1016/0043-1648(81)90257-X ↗
7. Galvanisieren kohlenfaserverstärkter Kunstoffe
8. Metallic wear resistant coatings for carbon fibre epoxy composite rolls10.1016/0257-8972(94)01024-D ↗
9. A review of surface engineering issues critical to wind turbine performance10.1016/j.rser.2007.11.009 ↗
10. Case study – alternatives to the use of chromium plating and conversion coatings at McClellan Air Force Base, California
11. Steffani · 1995
12. Non-chromated technology works on aircraft
13. Compliant electrodeposited and electroless nano-structured and nano-composite coatings to replace chromium coatings, Part 1
14. Compliant electrodeposited and electroless nano-structured and nano-composite coatings to replace chromium coatings, Part 2
15. Friction and wear characteristics of electrodeposited nanocrystalline nickel–tungsten alloy films10.1016/j.wear.2007.02.004 ↗
16. Kinetics of the deposition inert particles from electrolytic baths10.1149/1.2404383 ↗
17. Wear characteristics of sediment co-deposited nickel–SiC composite coatings
18. Kinetics of electroplating process of nano-sized ceramic particle/Ni composite10.1016/S0254-0584(01)00564-8 ↗
19. Electrodeposition of Ni–SiC nano-composite coatings and evaluation of wear and corrosion resistance and electroplating characteristics10.1016/j.colsurfa.2007.07.027 ↗
20. Solid particle erosion resistance of thermally sprayed functionally graded coatings for polymer matrix composites10.1016/j.surfcoat.2005.05.038 ↗
21. The deformation and ageing of mild steel: III. Discussion of results10.1088/0370-1301/64/9/303 ↗
22. The cleavage strength of polycrystals
23. A discussion of rain erosion testing at the United States Air Force rain erosion test facility10.1016/0043-1648(95)07139-3 ↗
24. Sol–gel derived erosion protection coatings against damage caused by liquid impact10.1016/j.wear.2006.12.039 ↗
25. M. Grundwürmer, N. Schupp, M. Meyer, J. Wehr, Protection of erosion-stressed aerospace structures through nanoparticle-enhanced inorganic–organic hybrid coatings, Patent WO 2008052510, EADS Deutschland GmbH, 2006.
26. M. Grundwürmer, Development and characterisation of liquid impact resistant sol–gel coatings, PhD Thesis, Technical University of Munich, 2008, p. 171.
27. Fabrication and characterization of Ni–ZrO2 composite nano-coatings by pulse electrodeposition10.1016/j.scriptamat.2005.04.002 ↗
28. Electrodeposition of composite coatings containing nanoparticles in a metal deposit10.1016/j.surfcoat.2005.11.123 ↗
29. M. Grundwürmer, N. Schupp, J. Wehr, Neuartige Prüfmethode zur Simulation von Regenerosion, Patent DE 102007060511, EADS Deutschland GmbH, 2007.
30. A mechanistic investigation of the rain erosion of infrared transmitting materials at velocities to Mach 2
31. The rain erosion resistance of some radome and IRdome materials
32. Rain erosion resistance of IR materials: comparison of rotating arms and MIJA measurements
33. Ministry of Defence · 2006
34. Rain erosion resistance characterizations link between on-ground experiments and in-flight specifications10.1016/j.wear.2004.09.053 ↗
35. Goldstein · 2003
36. X. Llovet Ximenes, Electron induced X-ray emission from solids. Simulation and measurements, PhD Thesis, Dept. Física Aplicada i Optica, University of Barcelona, 1998, p. 124.
37. EDX depth profiling by means of effective layers10.1007/s002160050975 ↗
38. CASINO V2.42—a fast and easy-to-use modeling tool for scanning electron microscopy and microanalysis users10.1002/sca.20000 ↗
39. The effect of second phase volume fraction on the erosion resistance of metal-matrix composites10.1016/S0043-1648(99)00363-4 ↗
40. Wear of titanium carbide reinforced metal matrix composites10.1016/S0043-1648(99)00030-7 ↗
41. Erosion of hard surface coatings for use in offshore gate valves10.1016/j.wear.2004.03.035 ↗