journal article·2018-01Open access

Tribological performance of monolithic copper thin films during nanowear

Bradley M. Schultz, Nan Li, David R. Economy, Julia L. Sharp, Nathan A. Mara, Marian S. Kennedy

Wear· Volume 394-395

Abstract

Abstract Mathematical models suggest that the strain along the film formed by parallel passes of a nanoindentation probe in contact with the film can be either homogenous or heterogeneous, depending on contact pressure and spacing between passes. In this study, a 1 µm copper thin film was worn with a cono-spherical diamond probe with normal loads ranging from 25 to 800 µN and wear box edge lengths of 40, 60, and 80 µm. The nanoindenter counterface was rastered across the surface to mimic dry sliding wear. To determine potential strain field changes, 10-step quasi-static indents (200–2000 µN) were performed using nanoindentation inside the wear boxes created at various loads to determine if a strain field alteration could be observed in changes in hardness of the copper thin film. It was shown that there was a softening effect in the hardness for normal loads
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Metal and Thin Film Mechanics · Diamond and Carbon-based Materials Research · Adhesion, Friction, and Surface Interactions

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (50)

Show source-provided references
1. Nanotribology: friction, wear and lubrication at the atomic scale10.1038/374607a0 ↗
2. Bhushan · 2005
3. Preface to the viewpoint set on: deformation and stability of nanoscale metallic multilayers10.1016/j.scriptamat.2003.11.036 ↗
4. C. Peng, K. Chiang, Overview of multilayered thin film theories for MEMS and electronic packaging applications, in: 2002 Inter Soc. Congerence Therm. Phenom., 2002, pp. 1058–1065.
5. Coefficient of friction and damage to contact area during the early stages of fretting I – glass, copper, or steel against copper
6. Fretting wear of metallic multilayer films10.1016/S0040-6090(03)01089-7 ↗
7. 2001 · Vol. 1
8. Pattern formation during nanowear of gold films
9. An approach to dry friction and wear for small volumes10.1080/01418610208240446 ↗
10. Probing the strain hardening response of small wear volumes with nanoindentation10.1007/s11661-011-0629-8 ↗
11. Tribological and mechanical behavior of nanostructured Al/Ti multilayers10.1016/j.surfcoat.2015.04.039 ↗
12. Wear behavior of Au-ZnO nanocomposite films for electrical contacts10.1007/s10853-014-8326-9 ↗
13. Nanoindentation and nanowear study of Sn and Ni-Sn coatings10.1016/j.triboint.2008.10.001 ↗
14. Characterization of the mechanical behavior of wear surfaces on single crystal nickel by nanomechanical techniques10.1557/jmr.2009.0075 ↗
15. Kondo · 2014
16. Spherical indentation of elastic-plastic solids10.1098/rspa.1999.0423 ↗
17. C.L. Woodcock, D.F. Bahr, N.R. Moody, Plastic zone development around nanoindentations, in: Materials Research Society Symposium Proceedings (Fundamentals of Nanoindentation and Nanotribology II), 2000, p. Q7.14.1–Q7.14.6.
18. Indentation of ceramics with spheres: a century after Hertz10.1111/j.1151-2916.1998.tb02580.x ↗
19. Determination of the effective zero-point and the extraction of spherical nanoindentation stress-strain curves10.1016/j.actamat.2008.03.036 ↗
20. Contact mechanics of coating-substrate systems: Monolayer and multilayer coatings10.1016/j.acme.2012.07.004 ↗
21. Derivation of plastic stress–strain relationship from ball indentations: examination of strain definition and pileup effect10.1557/JMR.2001.0437 ↗
22. Analysis of Berkovich indentation10.1016/0020-7683(95)00033-7 ↗
23. Spherical nanoindentation stress–strain curves10.1016/j.mser.2015.02.001 ↗
24. Prasad · 2006
25. Sliding contact stresses in a two-dimensional layered elastic half-space10.1016/0020-7683(87)90019-9 ↗
26. Sliding contact stress field due to a spherical indenter on a layered elastic half-space10.1115/1.3261591 ↗
27. Explicit equations for the stresses beneath a sliding spherical contact10.1243/PIME_PROC_1983_197_076_02 ↗
28. Goryacheva · 1998
29. Strain hardening around spherical indentations10.1002/1521-396X(200012)182:2<641::AID-PSSA641>3.0.CO;2-U ↗
30. Fischer-Cripps · 2007
31. Johnson · 1987
32. The hardness of solids10.1088/0034-6683/1/3/I01 ↗
33. The determination of yield strength from hardness measurements10.1007/BF02913433 ↗
34. Economy · 2011
35. Underwood · 1970
36. An improved technique for determining hardness and elastic modulus using load and displacement sensing indentation experiments10.1557/JMR.1992.1564 ↗
37. The concept of differential hardness in depth sensing indentation10.1088/1367-2630/5/1/315 ↗
38. Influence of indenter shape on DLC film failure during multiple load cycle nanoindentation10.1179/1743284712Y.0000000039 ↗
39. Plastic strain effect in progressive multi-cycle nano-indentation measurement
40. A model for junction growth of a spherical contact under full stick condition10.1115/1.2772322 ↗
41. Microscopy and microindentation mechanics of single crystal Fe−3 wt. % Si: Part I. Atomic force microscopy of a small indentation10.1557/JMR.1993.1291 ↗
42. Callister · 2010
43. Investigation of room temperature oxidation of Cu in air by Yoneda-XAFS
44. Hertzberg · 2013
45. On the effect of a general residual stress state on indentation and hardness testing10.1016/j.actamat.2008.08.029 ↗
46. Mechanism of creation of compressive residual stress by shot peening10.1016/S0142-1123(98)00002-4 ↗
47. Fischer-Cripps · 2002
48. Effects of the substrate on the determination of thin film mechanical properties by nanoindentation10.1016/S1359-6454(01)00328-7 ↗
49. Linking microstructural evolution and macro-scale friction behavior in metals10.1007/s10853-016-0569-1 ↗
50. Formation of a metallic amorphous layer during the sliding wear of Ti/TiN nanolaminates10.1007/s11249-014-0350-z ↗