Tribological behavior of Mo5Si3 particle reinforced Si3N4 matrix composites

Tateoki Iizuka, Hideki Kita

Wear· Volume 258· Issue 5-6
Publisher page

Abstract

Abstract The tribological behavior of Mo 5 Si 3 particle reinforced silicon nitride composites has been investigated by pin-on-disk wear testing under dry conditions. The friction coefficient of the Si 3 N 4 decreased with the incorporation of submicrometer-sized Mo 5 Si 3 particles and also as the content of Mo 5 Si 3 particles increased. The wear mechanism of the Mo 5 Si 3 –Si 3 N 4 composites consisted of fatigue between the Si 3 N 4 grains and the amorphous grain boundaries, fracture of Si 3 N 4 grains and grain-boundary phases, debonding of the Mo 5 Si 3 particles from the grain boundaries, and tribochemical reactions. Under dry conditions, in air at room temperature, the detached Mo 5 Si 3 particles reacted with oxygen to form MoO 3 and MoO 2 phases at the adherent film of the wear scar and exhibited self-lubricating behavior. When the Mo 5 Si 3 –Si 3 N 4 composites were oxidized at 700 °C in air, solid-lubricant MoO 3 particles were generated on the surface layer. Oxidized Mo 5 Si 3 –Si 3 N 4 composites showed self-lubricating behavior, and the average friction coefficient and wear rate of the oxidized 2.8 wt% Mo 5 Si 3 –Si 3 N 4 composite were 0.43 and 0.72 × 10 −5 mm 3 /N m, respectively, both values ∼30% lower than those for Si 3 N 4 . The formation of MoO 3 particles on the surface of the Mo 5 Si 3 –Si 3 N 4 composites as a result of the oxidation treatment improved the lubrication condition for the wear pairs, and decreased the wear rate, as well as the friction coefficient.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: MXene and MAX Phase Materials · Advanced ceramic materials synthesis · Metal and Thin Film Mechanics

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (25)

Show source-provided references
1. Tribology of ceramics10.1016/0043-1648(90)90075-L ↗
2. Microstructural design of ceramics for optimum wear resistance
3. Skopp · Wear · 1995 · 181–183 · 571
4. Fischer · Wear · 1985 · 105 · 2910.1016/0043-1648(85)90004-3 ↗
5. Nakamura · J. Am. Ceram. Soc. · 2001 · 84 · 257910.1111/j.1151-2916.2001.tb01057.x ↗
6. Influence of porosity on friction and wear of tetragonal zirconia polycrystal10.1111/j.1151-2916.1997.tb02841.x ↗
7. Senda · J. Am. Ceram. Soc. · 1999 · 82 · 150510.1111/j.1151-2916.1999.tb01948.x ↗
8. Bai · Thin Solid Films · 1994 · 249 · 18310.1016/0040-6090(94)90758-7 ↗
10. Kerkwijk · J. Am. Ceram. Soc. · 1999 · 82 · 208710.1111/j.1151-2916.1999.tb02045.x ↗
11. Studt · Tribol. Int. · 1989 · 22 · 11110.1016/0301-679X(89)90171-0 ↗
12. Gates · Tribol. Trans. · 1991 · 34 · 41710.1080/10402009108982052 ↗
13. Bai · Wear · 1993 · 169 · 18110.1016/0043-1648(93)90296-X ↗
14. Iwasa · J. Ceram. Soc. Jpn. · 1985 · 93 · 661
15. Liu · Wear · 1996 · 198 · 14310.1016/0043-1648(96)06946-3 ↗
16. Carrapichano · Wear · 2002 · 253 · 107010.1016/S0043-1648(02)00219-3 ↗
17. Iizuka · J. Ceram. Soc. Jpn. · 2001 · 109 · 69910.2109/jcersj.109.1272_699 ↗
18. Iizuka · J. Am. Ceram. Soc. · 2002 · 85 · 95410.1111/j.1151-2916.2002.tb00198.x ↗
19. Woydt · Tribol. Trans. STLE · 1999 · 42 · 2110.1080/10402009908982185 ↗
20. Orcutt · Wear · 1962 · 5 · 34510.1016/0043-1648(62)90073-X ↗
21. Peterson · ASLE Trans. · 1960 · 2 · 22510.1080/05698195908972374 ↗
22. Ludema · 1995 · 37
23. Hsu · 1990 · 123
24. Johnson · 1985
25. Yao · J. Eur. Ceram. Soc. · 2001 · 21 · 99110.1016/S0955-2219(00)00279-X ↗