Relationship of wear properties to basal-plane texture of worn surface of Mg alloys
Source abstract
Abstract
Abstract The wear properties of pure-Mg, AZ31 extruded alloy, AZ91 cast alloy, and Mg 90.5 Cu 3.25 Y 6.25 (at.%) cast alloy consisting of Mg and long-period-ordered (LPO) phases were investigated by pin-on-disk-type wear tests under dry sliding. The wear loss of the Mg 90.5 Cu 3.25 Y 6.25 cast alloy at high-applied loads over 147 N was less than those of AZ Mg alloys, and about two-thirds of the AZ31 extruded alloy, which indicated that the Mg 90.5 Cu 3.25 Y 6.25 cast alloy has superior wear-resistance. The basal planes (0 0 0 2) and ( 1 0 1 ¯ 1 ) were apparent in the X-ray diffraction patterns of worn surfaces of pure-Mg and Mg alloys. This XRD result indicated that basal planes in both the Mg and LPO phases were aligned to worn surfaces for the pure-Mg and Mg alloys, and this result was also supported by EBSD analysis. Because slip deformation tends to easily occur on the Mg basal plane at a low critical resolved shear stress (CRSS), formation of the basal-plane alignment on the wear surface negatively affects the wear-resistance properties. After the wear test of the Mg 90.5 Cu 3.25 Y 6.25 cast alloy, a kink deformation in the LPO phase was frequently observed in the worn edge section. The kink deformation in the LPO phase contributes to improve wear-resistance properties by suppression of the basal-plane alignment.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Magnesium Alloys: Properties and Applications · Aluminum Alloys Composites Properties · Metal and Thin Film Mechanics
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (22)
Show source-provided references
1. K, Washizu, Development of lightweight engine oil pan made of a heat-resistant magnesium alloy, ALUTOPIA, vol. 30, 2000, pp. 9–16.
2. Issues that influence magnesium use in the automotive industry10.4028/www.scientific.net/MSF.419-422.43 ↗
3. Recent magnesium alloy development for automotive powertrain applications10.4028/www.scientific.net/MSF.419-422.57 ↗
4. Friction and wear of Al2O3, ZrO2 and SiO2 rubbed against pure metals10.1016/0043-1648(92)90176-9 ↗
5. On the wear of aluminium and magnesium metal matrix composites10.1016/0043-1648(93)90338-M ↗
6. The effect of sintering additive on fracture behavior of carbon-whisker-reinforced silicon carbide composites10.1016/j.msea.2007.03.006 ↗
7. Dry sliding wear behavior of hot deformed magnesium AZ61 alloy as influenced by the sliding conditions10.1016/j.msea.2007.03.096 ↗
8. Effect of differential speed rolling on microstructure and mechanical properties of an AZ91 magnesium alloy10.1016/j.jallcom.2007.06.050 ↗
9. Wear behavior of AZ91D magnesium alloy with a nanocrystalline surface layer10.1016/j.surfcoat.2007.10.025 ↗
10. Microstructural evolution during high temperature sliding wear of Mg–3% Al–1% Zn (AZ31) alloy10.1016/j.wear.2009.07.001 ↗
11. Effect of the grain size on friction and wear properties of ZK60 Magnesium alloy10.2472/jsms.51.1154 ↗
12. Sliding wear map for the magnesium alloy Mg–9Al–0.9 Zn (AZ91)10.1016/S0043-1648(00)00495-6 ↗
13. Contribution of crystallographic texturing to the sliding friction behaviour of fcc and hcp metals10.1016/S0043-1648(01)00604-4 ↗
14. Long-period ordered structure in a high-strength nanocrystalline Mg–1at% Zn–2at% Y alloy studied by atomic-resolution Z-contrast STEM10.1016/S1359-6454(02)00191-X ↗
15. Long period stacking structures observed in Mg97Zn1Y2 alloy10.1016/j.scriptamat.2004.04.003 ↗
16. Variation of long-period stacking order structures in rapidly solidified Mg97Zn1Y2 alloy10.1016/j.msea.2004.10.040 ↗
17. Microstructure and mechanical properties of extruded Mg–Zn–Y alloys with 14H long period ordered structure10.2320/matertrans.47.959 ↗
18. Elevated temperature Mg97Y2Cu1 alloy with long period ordered structure10.1016/j.scriptamat.2006.05.011 ↗
19. A high-strength Mg–Ni–Y alloy sheet with a long-period ordered phase prepared by hot-rolling10.1016/j.scriptamat.2008.08.001 ↗
20. Dry sliding wear behavior of magnesium alloys10.1016/j.wear.2007.08.021 ↗
21. Plastic deformation behavior of Mg12YZn with 18R long-period stacking ordered structure10.1016/j.intermet.2009.07.014 ↗
22. Microstructure and Mechanical properties of Mg–Zn–Y rolled sheet with a Mg12ZnY phase10.2320/matertrans.L-M2010816 ↗