Tribological behaviour of enamel coatings
Source abstract
Abstract
Abstract An experimental study has been carried out to evaluate the tribological and mechanical properties of steel hardened with glass-ceramic enamel under ambient conditions. Three types of borosilicate based enamels were fused onto mild steel by the firing process, after a sandblasting and a ground coat to ensure surface integrity between the substrate and the covering coat. The surface roughness, micro hardness, wear track and tribological characteristics of the enamel coating were then characterised by an atomic force microscopy, a Vicker micro-hardness tester, a 3D optical profiler, an EDS/SEM, and a friction and wear testing tribology meter. The tribological differentials of these top coats were examined after sliding against chrome steel, zirconia and silicon nitride. The worn morphologies provided some understandings of the failing mechanism due to friction. During dry sliding with a silicon nitride mating part, the coefficient of friction and loss of enamel enriched with titanium was less than the chrome steel balls, although the zirconia ball succumbed to serious wear. The changes in the worn morphologies and chemical composition under different sliding contacts, and the corresponding wear mechanism were observed, with abrasive wear being dominant.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Metal and Thin Film Mechanics · High-Temperature Coating Behaviors · Advanced materials and composites
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (43)
Show source-provided references
1. Low-melting chemical resistant enamel for steel kitchenware10.1023/A:1023886032228 ↗
2. Maskall · 1986
3. Non-isothermal crystallization kinetic studies on MgO-Al2O3-SiO2-TiO2 glass10.1016/j.jnoncrysol.2007.04.008 ↗
4. Effect of zirconium on grain growth and mechanical properties of a ball-milled nanocrystalline FeNi alloy10.1016/j.jallcom.2012.10.179 ↗
5. Effect of crystallization on the property of hard enamel coating on steel substrate10.1016/j.apsusc.2008.12.007 ↗
6. Effect of thermal treatment on the property of enamel coating on steel substrate
7. The designing of products utilising the special properties of vitreous enamel10.1016/0261-3069(86)90037-3 ↗
8. Chapter 12 - Thermal Conductivity and Heat Transfer in Glass
9. Chapter 11 - Heat Capacity of Glass
10. Chapter 17 - Chemical Durability
11. Corrosion resistance and mechanism of steel rebar coated with three types of enamel10.1016/j.corsci.2012.02.024 ↗
12. Microstructure and corrosion resistance of enamel coatings applied to smooth reinforcing steel10.1016/j.conbuildmat.2012.04.059 ↗
13. Electrochemical behavior of enamel-coated carbon steel in simulated concrete pore water solution with various chloride concentrations10.1016/j.electacta.2012.12.125 ↗
14. Cement-modified enamel coating for enhanced corrosion resistance of steel reinforcing bars10.1016/j.cemconcomp.2012.08.009 ↗
15. Chloride-induced corrosion mechanism and rate of enamel- and epoxy-coated deformed steel bars embedded in mortar10.1016/j.cemconres.2015.12.015 ↗
16. Oxidation and hot corrosion behavior of a novel enamel-Al2O3 composite coating on K38G superalloy10.1016/j.surfcoat.2005.09.004 ↗
17. Effect of ultrafine enamel coating on the oxidation and mechanical property of Ti60 alloy
18. Effect of enamel coating on long-term oxidation of Ti65 alloy10.1504/IJMPT.2004.004267 ↗
19. resistance of enameled surfaces to scratching gouging, and abrasion10.1111/j.1151-2916.1947.tb18875.x ↗
20. Hutchings · 1992
21. Evaluation of the abrasion resistance of enamel coatings10.1016/j.cep.2012.10.009 ↗
22. Influence of mill additives on vitreous enamel properties10.1016/j.matdes.2013.10.059 ↗
23. Abrasion resistance of vitreous enamel coatings in function of frit composition and particles presence10.1016/j.wear.2015.01.058 ↗
24. Abrasion and chemical resistance of composite vitreous enamel coatings with hard particles10.1002/sia.5849 ↗
25. The aesthetic and functional properties of enamel coatings on steel10.1016/j.matdes.2010.04.030 ↗
26. Glass and glass-ceramic coatings, versatile materials for industrial and engineering applications10.1007/BF02704843 ↗
27. K. McKinley, H. Evele, C. Baldwin, Analysis of fracture in porcelain enamels, in: Proceedings of the 22nd International Enamellers Congress, IEI, Cologne - Germany, 2012.
28. Cahn · 1996
29. Effects of RE on the friction and abrasion character of Porcelain Enamel10.4028/www.scientific.net/AMR.538-541.410 ↗
30. Surface integrity and tribological behaviour of hardened steels
31. Preparation and Wear Behavior of Enamel Coating on Ti-6Al-4V ELI Titanium Alloy
32. Improvement in fretting wear and fatigue resistance of Ti-6Al-4V by application of several surface treatments and coatings10.1016/S0257-8972(98)00528-3 ↗
33. Effects of the counterface materials on the tribological characteristics of CNX coating deposited on plasma-nitrided Ti-6Al-4V10.1016/S0921-5093(00)01372-1 ↗
34. The influence of water addition on high-temperature tribological properties of interstitial free steel sliding against different counterparts10.1080/10402004.2017.1400629 ↗
35. Study of the hydrophobic properties of the surface of an enamel material10.4028/www.scientific.net/MSF.789.178 ↗
36. Effect of indication liquids on brittle-fracture properties of vitreous enamel coating
37. Size particle effects on lithium insertion into Sn-doped TiO2 anatase10.1021/cm051445v ↗
38. Controlling the formation of Na2ZrSiO5 in alkali fusion process for zirconium oxychloride production10.1016/j.apt.2015.08.005 ↗
39. Friction and wear behavior of CaO-MgO-Al2O3-SiO2 glass-ceramics prepared by waste casting sands10.4028/www.scientific.net/AMM.217-219.1251 ↗
40. Shear bond strengths between three different yttria-stabilized zirconia dental materials and veneering ceramic and their susceptibility to autoclave induced low-temperature degradation10.1155/2016/9658689 ↗
41. Friction and wear behavior of structural ceramics sliding against zirconia10.1016/j.wear.2006.12.079 ↗
42. Effects of coloring procedures on zirconia/veneer ceramics bond strength10.4047/jap.2014.6.6.451 ↗
43. Shear bond strength of veneering porcelain to zirconia and metal cores10.4047/jap.2009.1.3.129 ↗