journal article·2013-04

Effects of thermal and thermomechanical treatments on sliding wear of graphite crystallised white cast iron

X.J. Gao, Q. Zhang, D.B. Wei, S.H. Jiao, Z.Y. Jiang

Wear· Volume 301· Issue 1-2
Publisher page

Abstract

Abstract The effects of thermal and thermomechanical treatments on sliding wear of graphite crystallised white cast iron (GWCI) were studied. Due to the inherent embrittlement of GWCI, a laminated metal in which the GWCI is cladded by low carbon steel was prepared for this study. Three cylindrical samples (GWCI-A, GWCI-B and GWCI-C) were machined from the same laminate. GWCI-A was kept in as-cast state while GWCI-B and GWCI-C underwent the thermal and thermomechanical treatments, respectively. The pin-on-disc type sliding wear tests were performed on the GWCI layers at room temperature. The microstructures and wear mechanisms were analysed by optical microscope, scanning electron microscope and the Vickers hardness test. Experimental results demonstrated that the GWCI, after laminating with ductile steel, can be deformed at high temperature with crack-free. The thermomechanical treatment produced a finer microstructure and crushed primary carbides in GWCI-C. Both GWCI-B and GWCI-C displayed plenty of secondary carbides in supercooled austenitic matrix, which was more favourable to squeeze the graphite and form the oxide layers than the matrix of martensite plus retained austenite in GWCI-A. The wear resistance of GWCI-C was superior to that of GWCI-A and GWCI-B because the oxidational wear rather than delamination dominated the sliding wear process.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Metal Alloys Wear and Properties · Microstructure and Mechanical Properties of Steels · High Entropy Alloys Studies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (31)

Show source-provided references
1. Sliding wear of graphite crystallised chromium white cast iron10.1016/S0043-1648(01)00600-7 ↗
2. Comparison of wear resistant MMC and white cast iron10.1016/S0043-1648(02)00300-9 ↗
3. Erosive wear of low chromium white cast iron10.1016/0043-1648(93)90466-Y ↗
4. Solidification characteristics of atomized white cast iron powders10.1016/0956-716X(93)90317-L ↗
5. Solidification structure and abrasion resistance of high chromium white irons10.1007/s11661-997-0267-3 ↗
6. Sliding wear behaviour of Cr–Mo–Cu alloy cast irons with and without nano-additives10.1016/j.wear.2011.06.015 ↗
7. Influence of load and speed on wear characteristics of grey cast iron in dry sliding-selection for minimum wear10.1016/0301-679X(85)90006-4 ↗
8. Properties of cross-rolled low alloy white cast iron grinding ball10.1016/S1006-706X(07)60073-9 ↗
9. Superplastic behaviour of fine-grained white cast irons
10. Effect of heat treatment on microstructure and mechanical properties of high boron white cast iron10.1016/j.msea.2010.09.092 ↗
11. The effect of titanium on the wear behaviour of a 16%Cr white cast iron under pure sliding10.1016/j.wear.2006.12.011 ↗
12. Effect of boron on the sliding wear of directionally solidified high-chromium white irons10.1016/j.wear.2008.11.009 ↗
13. Sliding wear of spray-formed high-chromium white cast iron alloys10.1016/j.wear.2005.01.021 ↗
14. Defining a New Era in Physical Simulation and Thermal-Mechanical Testing, 〈http://gleeble.com〉.
15. Wear coefficient of tungsten carbide against hot-work tool steel disc with two different pin settings10.1016/j.wear.2004.01.014 ↗
16. ASTM Standard G99-05, 2010. Standard Test Method for Wear Testing with a Pin-on-Disk Apparatus, ASTM International, West Conshohocken, PA, 〈http://www.astm.org〉.
17. Tribological study of Fe–Cu–Cr-graphite alloy and cast iron railway brake shoes by pin-on-disc technique10.1016/j.wear.2009.12.014 ↗
18. The use of the pin-on-disk tribology test method to study three unique industrial applications10.1016/j.wear.2009.02.026 ↗
19. Influence of hardness on the wear resistance of 17-4 PH stainless steel evaluated by the pin-on-disc testing10.1016/j.jmatprotec.2007.11.251 ↗
20. Influence of the thermomechanical processing on the fracture mechanisms of high strength aluminium/pure aluminium multilayer laminate materials10.1016/j.msea.2008.01.034 ↗
21. Microstructure and properties of iron aluminum alloy/CrMo steel composite prepared by clad rolling10.1016/j.jallcom.2004.02.043 ↗
22. Effect of interfacial bonding strength on tensile ductility of multilayered steel composites10.1016/j.compscitech.2009.04.013 ↗
23. Cui · 2007
24. Abrasive wear of white cast irons10.1016/0043-1648(80)90101-5 ↗
25. The relationship between the abrasive wear resistance, hardness and microstructure of ferritic materials10.1016/0043-1648(74)90101-X ↗
26. Variations in microstructure of high chromium cast irons and resultant changes in resistance to wear, corrosion and corrosive wear10.1016/j.wear.2008.11.025 ↗
27. Hao · 2004
28. Dry rolling-sliding wear of austempered cast iron10.1016/j.wear.2010.12.018 ↗
29. Review of oxidational wear: part I: the origins of oxidational wear10.1016/0301-679X(83)90086-5 ↗
30. Smears of titanium metal10.1038/160260a0 ↗
31. J.B. Robert, Metallurgical cross sectioning of microelectronic packages for optical inspection and electron beam analysis, in: Proceedings of the 29th International Metallurgical Society Convention, Pittsburgh, USA, 1996.