journal article·2005-04

Erosion–corrosion of Fe- and Ni-based tubes and coatings in a fluidized bed test rig during exposure to HCl- and SO2-containing atmospheres

Rikard Norling, Anna Nafari, Anders Nylund

Wear· Volume 258· Issue 9
Publisher page

Abstract

Abstract Tubes made from five commercial alloys (Fe9Cr1Mo, 304L, Esshete 1250, 353 MA and Inconel 625) as well as two coating materials (Inconel 625 and Metco 8443) deposited on low alloyed steel tubes were exposed to different atmospheres in a laboratory fluidized bed test rig at 550 °C for 3 weeks (504 h). The atmospheres were air, air + 50 ppm HCl and air + 50 ppm SO 2 . Excluding the Metco 8443 coating, all materials show the lowest wastage rate in the SO 2 -containing atmosphere. For all exposure conditions, the best overall performance is shown by the Fe9Cr1Mo alloy. The circumferential wastage profiles recorded on tubes exposed in air and air + 50 ppm HCl show an erosion pattern with two maxima (Type A behaviour), while the tubes recorded in the SO 2 -containing atmosphere display only one maximum (Type B behaviour).
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Erosion and Abrasive Machining · High-Temperature Coating Behaviors · Advanced materials and composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (12)

Show source-provided references
1. Effect of process variables on wastage in fluidised bed combustors: criteria for test procedures
2. The circumferential distribution of wastage on in-bed tubes in fluidised bed combustors10.1016/0043-1648(95)07186-5 ↗
3. Summary of results from the Berkely in-bed tube erosion simulator10.1080/09603409.1997.11689558 ↗
4. On the ductile behavior of nominally brittle materials during erosive cutting10.1115/1.3672666 ↗
5. Some principal mechanism in the simultaneous erosion and corrosion attack of metals at high temperatures10.1016/0921-5093(91)90739-A ↗
6. Effect of HCl on the corrosion and wear of in-bed tubes in a laboratory simulated bubbling fluidised bed10.1016/S0043-1648(99)00247-1 ↗
7. Practical experience with wastage at elevated temperatures in coal combustion systems10.1016/0043-1648(95)07189-X ↗
8. Hydrodynamics and steel tube wastage in a fluidised bed at elevated temperature10.1016/j.ces.2003.09.027 ↗
9. Erosion-corrosion of 304 tubes in bubbling fluidised beds at 550°C10.4028/www.scientific.net/MSF.369-372.515 ↗
10. Erosion-corrosion of Fe- and Ni-based alloys at 550°C10.1016/S0043-1648(02)00299-5 ↗
11. Mechanisms in the simultaneous erosion-oxidation attack of nickel and cobalt at high temperature10.1007/BF02646210 ↗
12. Effect of angle of incidence on the combined erosion-oxidation attack of nickel and cobalt10.1007/BF00664339 ↗