Diamond grits reinforced coating on 35CrMnSi coal shearer cutting teeth: Microstructure, wear resistance and service performance in coal extraction
Source abstract
Abstract
Coal shearer cutting teeth is a key components in coal mining, its service life is very important for the productivity and cost in coal mining. In order to improve the wear resistance and service life of 35CrMnSi coal shearer cutting teeth in coal mining, diamond grits reinforced coating was vacuum cladded on 35CrMnSi steel by using Ni–Cr based alloy as a binder. Furthermore, post-heat treatment was performed to eliminate the negative influence of high cladding temperature on the properties of 35CrMnSi steel. The microstructure, phase composition, mechanical properties, reciprocating sliding wear properties, and coal mining application of the coated cutting teeth were investigated. The results show that the coating of about 360 μm thickness is primarily composed of randomly distributed diamond grits that are partially fastened by the Ni–Cr based cladded alloy and metallurgically bonded to the 35CrMnSi steel. Besides, some Cr–C precipitates (Cr 3C 2, Cr 7C 3, Cr 23C 6 ) and CrB precipitates are formed, which can enhance the coating together with the diamond grits. The hardness of 35CrMnSi steel(3.15Gpa) decreases by 10% after cladding(2.18Gpa) but increases by twofold after the post-heat treatment(6.36Gpa). The wear weight losses of the original 35CrMnSi steel, the coating after cladding, and the coating after post-heat treatment are 9.24 mg, 0.49 mg, and 0.12 mg, respectively. The wear rate calculation indicates that the wear resistance of diamond grits reinforced coating before and after post-heat treatment is about 90 times higher than that of uncoated 35CrMnSi steel. The wear mechanism of the coating is mainly abrasive wear, breaking of diamond grits, and plowing of the grits to the Al 2O 3 ball. The industrial tests demonstrate that the service life of 35CrMnSi cutting teeth with diamond grits reinforced coating can be increased by 1.6 times. Moreover, the coating can effectively eliminate sparks generated by high-speed friction. Therefore, diamond grits reinforced coating can significantly improve the service life and production efficiency of the coal shearer cutting teeth.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced materials and composites · Metal Alloys Wear and Properties · Tunneling and Rock Mechanics
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (37)
Show source-provided references
1. The abrasive resistance study about the cutting picker 40Cr of coal cutter10.4028/www.scientific.net/AMM.387.227 ↗
2. Heat treatment technology and property study on 40Cr of shearer picks body10.4028/www.scientific.net/AMR.791-793.782 ↗
3. Study on microstructure and properties of plasma arc surfacing layer for cutting pick10.4028/www.scientific.net/AMM.387.231 ↗
4. Multi-attribute failure analysis of coal cutting picks on longwall shearer machine10.1016/j.engfailanal.2020.105069 ↗
5. Comparison of a cold-sprayed and plasma-sprayed Fe25Cr20Mo1Si amorphous alloy coatings on 40Cr substrates10.1002/maco.202011558 ↗
6. Hardfacing welded ASTM A572-based, high-strength, low-alloy steel: welding, characterization, and surface properties related to the wear resistance10.3390/met9020244 ↗
7. Investigation on fretting Wear performance of laser cladding WC/Co06 coating on 42CrMo steel for hydraulic damper10.1016/j.ijrmhm.2022.106068 ↗
8. Microstructure and wear resistance of in-situ TiC surface composite coating on copper matrix synthesized by SHS and Vacuum-Expendable Pattern Casting10.1016/j.surfcoat.2017.05.080 ↗
9. Friction and wear properties of TiN-TiB2-Ni based composite coatings by argon arc cladding technology10.1016/j.surfcoat.2019.06.015 ↗
10. Dry sliding wear behavior of laser clad WC/NiCrBSi metal matrix composite coatings10.4028/www.scientific.net/AMR.690-693.3327 ↗
11. Adsorption and diffusion behaviors of Ni-based filler elements on diamond surface
12. O. Celep, G. Aydin, I. Karakurt, Diamond recovery from waste sawblades: A preliminary investigation. Proc. IME B J. Eng. Manufact., 227(6), 917–921. https://doi.org/10.1177/0954405412471524.10.1177/0954405412471524 ↗
13. Microstructure and performance of brazed diamonds with Ni–Cr+multilayer graphene composite alloy10.1016/j.jallcom.2019.152630 ↗
14. Microstructures and wear resistance of FeCoCrNi-Mo high entropy alloy/diamond composite coatings by high speed laser cladding10.3390/coatings10030300 ↗
15. Plasma sprayed diamond reinforced molybdenum coatings10.1016/j.jallcom.2018.07.088 ↗
16. Effects of diamond size on the deposition characteristic and tribological behavior of diamond/Ni60 composite coating prepared by supersonic laser deposition10.1016/j.diamond.2015.06.014 ↗
17. Interfacial microstructure and performance of brazed diamond grits with Ni–Cr–P alloy10.1016/j.jallcom.2008.09.134 ↗
18. Fabrication and performance of brazing diamond using large size NiCr alloy as a bonding agent10.1016/j.diamond.2021.108352 ↗
19. Fast salt bath heat treatment for a Bainitic/Martensitic low-carbon low-alloyed steel10.1007/s11661-015-3117-8 ↗
20. Interface microstructure and bonding performance of brazed W-coated diamonds using Ni–Cr alloy10.1016/j.ceramint.2021.12.189 ↗
21. Effects of process parameters on interfacial microstructure, residual stresses, and properties of tunnel furnace brazed diamonds10.1016/j.diamond.2018.04.003 ↗
22. Microstructure and processing performance of brazed diamond drill bits with Ni–Cr + Cu–Ce composite solder10.1016/j.diamond.2019.01.023 ↗
23. Peng Han, Xiaoyang Ding, Interface characteristics and performance of pre-brazed diamond grains with Ni–Cr composite alloy10.1016/j.jallcom.2015.03.269 ↗
24. A thermodynamic study of the chromium-carbon system10.1016/0364-5916(87)90035-6 ↗
25. Microstructure and properties at bonds of diamond grains and NiCr filler alloy by fiber laser brazing10.1016/j.diamond.2022.108969 ↗
26. Study on technique of induction cladding alloy layer in steel tube outer wall and property of alloy layer
27. An improved technique for determining hardness and elastic modulus using load and displacement sensing indentation experiments10.1557/JMR.1992.1564 ↗
28. Magnetron sputtered Cr-Ni-N and Ti-Mo-N films: comparison of mechanical properties10.1016/S0257-8972(01)01250-6 ↗
29. Multicomponent nanostructured films for various tribological applications10.1016/j.ijrmhm.2009.07.014 ↗
30. Can the H/E ratio be generalized as an index for the wear resistance of materials?10.1016/j.matchemphys.2021.125245 ↗
31. Introduction of the ratio of the hardness to the reduced elastic modulus for abrasion
32. Effects of the ratio of hardness to Young's modulus on the friction and wear behavior of bilayer coatings10.1063/1.1811377 ↗
33. The effect of TiN, TiAlN, CrAlN, and TiAlN/TiSiN coatings on the wear properties of AISI H13 steel at room temperature
34. Wear behaviors of HVOF-sprayed NiSiCrFeB, WC-Co/NiSiCrFeB and WC-Co coatings evaluated using a pin-on-disc tester with C45 steel pins
35. Microstructure and tribological performance of thermally sprayed molybdenum coating10.1007/s42250-021-00306-z ↗
36. Oxidation and tribo-oxidation of an alloy steel H13 at elevated temperature
37. Optimizing wear behavior of TiN coated SS 316L against Ti alloy using Response Surface Methodology10.1016/j.matdes.2014.10.051 ↗