Abstract
High strength and translucency are generally not coincident in one restorative material and there is still a continuous development for a better balance between these two properties. Zirconia and lithium-disilicate glass-ceramics are currently the most popular alternatives for monolithic restorations. In this work, the mechanical properties and more important, the slow crack growth (SCG) resistance, which rules long-term durability, were thoroughly studied for three zirconia ceramics stabilized by 3, 4 and 5 mol% yttria in comparison to lithium-disilicate glass-ceramic. Translucency versus strength maps revealed that the more translucent zirconia compositions (i.e. with higher yttria contents) fill the gap between the standard 3 mol% yttria stabilized zirconia (3Y-TZP) and lithium-disilicate. Moreover, increasing yttria content did not always result in lower strength, as values for 3 mol% and 4 mol% yttria were the same. Independent on the yttria contents, all zirconia showed similar relative susceptibility to SCG under static and cyclic conditions and were significantly more SCG-resistant than lithium-disilicate glass ceramic. A concern with higher yttria contents (5 and 4 mol%) however could lie in the higher sensitivity to defects, resulting in a larger scatter in strength. STATEMENT OF SIGNIFICANCE: In addition to the common investigations on the generally reported strength, toughness and translucency, V-KI diagrams (crack velocity versus stress-intensity factor) from fast fracture to threshold for three newly developed zirconia were directly measured by double torsion methods under static and cyclic loading conditions. The crack-growth mechanisms were analyzed in depth. Results were compared with another popular dental ceramic, namely lithium-disilicate glass-ceramic, revealing the pros and cons of polycrystalline and glass-ceramics in terms of long-term durability. This is the first time that V-KI curves are compared for the major ceramic and glass-ceramic used for dental restorations. Strength versus translucency maps for different CAD/CAM dental restorative materials were described, showing the current indication range for zirconia ceramics.
Source: europepmc · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Dental materials and restorations · Advanced ceramic materials synthesis · Glass properties and applications
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (65)
Show source-provided references
1. Zirconia as a ceramic biomaterial10.1016/S0142-9612(98)00010-6 ↗
2. State of the art of zirconia for dental applications10.1016/j.dental.2007.05.007 ↗
3. Current status of zirconia restoration10.1016/j.jpor.2013.09.001 ↗
4. Dentist material selection for single-unit crowns: findings from the National Dental Practice-Based Research Network10.1016/j.jdent.2016.09.010 ↗
5. Ceramics in restorative and prosthetic dentistry10.1146/annurev.matsci.27.1.443 ↗
6. Translucency and biaxial flexural strength of four ceramic core materials10.1016/j.dental.2008.03.010 ↗
7. Novel Zirconia Materials in Dentistry10.1177/0022034517737483 ↗
8. Making yttria-stabilized tetragonal zirconia translucent10.1016/j.dental.2014.08.375 ↗
9. Aging resistance, mechanical properties and translucency of different yttria-stabilized zirconia ceramics for monolithic dental crown applications10.1016/j.dental.2018.03.006 ↗
10. Strength, toughness and aging stability of highly-translucent Y-TZP ceramics for dental restorations10.1016/j.dental.2016.09.025 ↗
11. Cyclic fatigue in water of veneer-framework composites for all-ceramic dental bridges10.1016/j.dental.2006.01.011 ↗
12. ADM guidance-ceramics: fatigue principles and testing10.1016/j.dental.2017.09.006 ↗
13. Chairside CAD/CAM materials. Part 3: Cyclic fatigue parameters and lifetime predictions10.1016/j.dental.2018.03.024 ↗
14. Mechanisms of fatigue-crack propagation in ductile and brittle solids10.1023/A:1018655917051 ↗
15. Fett · 1999
16. Fatigue of zirconia under cyclic loading in water and its implications for the design of dental bridges10.1016/j.dental.2005.12.008 ↗
17. In vitro lifetime of dental ceramics under cyclic loading in water10.1016/j.biomaterials.2006.12.033 ↗
18. Subcritical Crack Propagation in 3Y-TZP Ceramics: Static and Cyclic Fatigue10.1111/j.1151-2916.1999.tb02213.x ↗
19. Crack growth resistance of alumina, zirconia and zirconia toughened alumina ceramics for joint prostheses10.1016/S0142-9612(01)00206-X ↗
20. Lawn · 1993
21. Recent advances in understanding the fatigue and wear behavior of dental composites and ceramics10.1016/j.jmbbm.2018.08.008 ↗
22. Fatigue of dental ceramics10.1016/j.jdent.2013.10.007 ↗
23. Phase separation and hydrothermal degradation of 3 mol% Y2O3-ZrO2 ceramics10.2109/jcersj.113.530 ↗
24. Qualitative X-ray Diffraction Analysis of Metastable Tetragonal (t′) Zirconia10.1111/j.1151-2916.2001.tb00708.x ↗
25. Double-torsion testing a 3Y-TZP ceramic10.1016/0272-8842(95)00076-3 ↗
26. The double-torsion testing technique for determination of fracture toughness and slow crack growth behavior of materials: a review10.1007/s10853-005-5553-0 ↗
27. An Evaluation of the Double Torsion Technique10.1007/s11340-011-9468-1 ↗
28. A Simple Method for Studying Slow Crack Growth
29. Effect of Yttria Content on the Zirconia Unit Cell Parameters10.1111/j.1551-2916.2011.04862.x ↗
30. Phase transitions in zirconium dioxide and related materials for high performance engineering ceramics10.1023/A:1021099308957 ↗
31. Chairside CAD/CAM materials10.1016/j.dental.2016.10.008 ↗
32. Load-bearing capacity of lithium disilicate and ultra-translucent zirconias10.1016/j.jmbbm.2018.08.023 ↗
33. Slow crack-growth behavior of alumina ceramics10.1557/JMR.2000.0024 ↗
34. Cyclic fatigue and resistance-curve behavior of anin situ toughened silicon carbide with AlBC additions10.1016/1359-6454(95)00409-2 ↗
35. Cyclic Fatigue-Crack Growth in a SiC-Whisker-Reinforced Alumina Ceramic Composite: Long- and Small-Crack Behavior10.1111/j.1151-2916.1992.tb04139.x ↗
36. L.M. E., R.R. O., On the Fracture Toughness of Advanced Materials, Advanced Materials 21(20) (2009) 2103-2110.10.1002/adma.200803322 ↗
37. Transformation Toughening in Zirconia-Containing Ceramics10.1111/j.1151-2916.2000.tb01221.x ↗
38. Toughening mechanisms for ceramic materials10.1016/0955-2219(92)90026-A ↗
39. Microstructural mechanisms of cyclic fatigue-crack propagation in grain-bridging ceramics10.1016/S0272-8842(96)00048-X ↗
40. Phenomena and mechanisms of crack propagation in glass-ceramics10.1016/j.jmbbm.2007.11.005 ↗
41. Fracture anisotropy in texturized lithium disilicate glass-ceramics10.1016/j.jnoncrysol.2017.11.040 ↗
42. The phenomena of rupture and flow in solids
43. Effect of Coloring Agent on the Strength and Transmittance of Dental Zirconia Block10.15236/ijcpd.2017.13.4.223 ↗
44. Residual compressive surface stress increases the bending strength of dental zirconia10.1016/j.dental.2016.12.007 ↗
45. Effect of different treatments on the flexural strength of fully versus partially stabilized monolithic zirconia10.1016/j.prosdent.2016.10.031 ↗
46. Evaluation of mechanical and optical behavior of current esthetic dental restorative CAD/CAM composites10.1016/j.jmbbm.2015.10.004 ↗
47. Mechanical properties of zirconia reinforced lithium silicate glass-ceramic10.1016/j.dental.2016.03.013 ↗
48. Flexural resistance of heat-pressed and CAD-CAM lithium disilicate with different translucencies10.1016/j.dental.2016.10.005 ↗
49. The Tetragonal-Monoclinic Transformation in Zirconia: Lessons Learned and Future Trends10.1111/j.1551-2916.2009.03278.x ↗
50. Large increase in fracture resistance of stishovite with crack extension less than one micrometer10.1038/srep10993 ↗
51. Crack propagation and fatigue in zirconia-based composites10.1016/S1359-835X(98)00145-6 ↗
52. Influence of Water Vapor on Crack Propagation in Soda-Lime Glass10.1111/j.1151-2916.1967.tb15145.x ↗
53. A frictional-wear mechanism for fatigue-crack growth in grain bridging ceramics10.1016/0956-7151(93)90145-I ↗
54. Crystallization toughening of a model glass-ceramic10.1016/j.actamat.2014.12.007 ↗
55. Long-term strength of ceramics for biomedical applications10.1002/jbm.b.20039 ↗
56. Lifetime of alumina- and zirconia ceramics used for crown and bridge restorations10.1002/jbm.b.30599 ↗
57. Effect of the microstructure on the lifetime of dental ceramics10.1016/j.dental.2011.04.003 ↗
58. Global description of crack propagation in ceramics10.1016/j.jeurceramsoc.2005.11.004 ↗
59. Impact of oral fluids on dental ceramics: What is the clinical relevance?10.1016/j.dental.2013.08.199 ↗
60. The effect of surface grinding and sandblasting on flexural strength and reliability of Y-TZP zirconia ceramic10.1016/S0109-5641(99)00070-6 ↗
61. Fracture of Ceramics10.1002/adem.200700347 ↗
62. Critical influence of alumina content on the low temperature degradation of 2–3mol% yttria-stabilized TZP for dental restorations10.1016/j.jeurceramsoc.2014.09.018 ↗
63. Grain-boundary structure and microstructure development mechanism in 2–8mol% yttria-stabilized zirconia polycrystals10.1016/j.actamat.2007.11.026 ↗
64. Sintering Kinetics at Constant Rates of Heating: Effect of Al2O3 on the Initial Sintering Stage of Fine Zirconia Powder10.1111/j.1551-2916.2005.00620.x ↗
65. Transparent Tetragonal Yttria-Stabilized Zirconia Ceramics: Influence of Scattering Caused by Birefringence10.1111/j.1551-2916.2010.04322.x ↗