Biomechanical testing and degradation analysis of MgCa0.8 alloy screws: A comparative in vivo study in rabbits
Source abstract
Abstract
The aim of this study was to compare the biomechanical properties of degradable magnesium calcium alloy (MgCa0.8) screws and commonly used stainless steel (S316L) screws and to assess the in vivo degradation behavior of MgCa0.8. MgCa0.8 screws (n=48) and S316L screws (n=32) were implanted into both tibiae of 40 adult rabbits for a follow-up of 2, 4, 6 and 8 weeks. This resulted in a testing group of MgCa0.8 (n=12) and S316L (n=8) screws for each follow-up. Uniaxial pull-out tests were carried out in an MTS 858 Mini Bionix at a rate of 0.1 mm s(-1). For degradation analysis of MgCa0.8 in vivo micro-computed tomography (μCT) was performed to determine the volume of metal alloy remaining. Retrieved MgCa0.8 screws were analysed for degradation by determination of weight changes, scanning electron microscopy and energy dispersive X-ray analyses. No significant differences could be noted between the pull-out forces of MgCa0.8 and S316L 2 weeks after surgery (P=0.121). Six weeks after surgery the pull-out force of MgCa0.8 decreased slightly. In contrast, the S316L pull-out force increased with time. Thus, significantly higher pull-out values were detected for S316L from 4 weeks on (P<0.001). The volume and weight of MgCa0.8 gradually reduced. A corrosion layer, mainly composed of oxygen, magnesium, calcium and phosphorus, formed on the implants. Since MgCa0.8 showed good biocompatibility and biomechanical properties, comparable with those of S316L in the first 2-3 weeks of implantation, its application as a biodegradable implant is conceivable.
Source: europepmc · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Magnesium Alloys: Properties and Applications · Aluminum Alloys Composites Properties · Hydrogen Storage and Materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (40)
Show source-provided references
1. Mechanical factors influencing the holding power of screws in compact bone10.1302/0301-620X.55B3.633 ↗
2. Unalloyed titanium for implants in bone surgery10.1016/S0020-1383(00)80016-9 ↗
3. Stainless steel in bone surgery10.1016/S0020-1383(00)80015-7 ↗
4. Biodegradable implants in traumatology: a review on the state-of-the-art10.1007/BF00443385 ↗
5. Biomaterials in orthopaedics10.1098/rsif.2008.0151 ↗
6. In vivo corrosion and corrosion protection of magnesium alloy LAE44210.1016/j.actbio.2009.10.012 ↗
7. MgZnCa glasses without clinically observable hydrogen evolution for biodegradable implants10.1038/nmat2542 ↗
8. Control of biodegradation of biocompatible magnesium alloys10.1016/j.corsci.2007.01.001 ↗
9. Are resorbable implants about to become a reality?10.1017/S1047951106000011 ↗
10. In vitro corrosion and biocompatibility of binary magnesium alloys10.1016/j.biomaterials.2008.10.021 ↗
11. In vivo evaluation of biodegradable magnesium alloy bone implant in the first 6 months implantation10.1002/jbm.a.32132 ↗
12. In vivo corrosion of four magnesium alloys and the associated bone response10.1016/j.biomaterials.2004.09.049 ↗
13. Degradation behaviour and mechanical properties of magnesium implants in rabbit tibiae10.1007/s10853-009-3936-3 ↗
14. Magnesium and its alloys as orthopedic biomaterials: a review10.1016/j.biomaterials.2005.10.003 ↗
15. Bioresorbable devices made of forged composites of hydroxyapatite (HA) particles and poly-l-lactide (PLLA): Part I. Basic characteristics10.1016/S0142-9612(98)00241-5 ↗
16. Influence of different surface machining treatments of magnesium-based resorbable implants on the degradation behavior in rabbits
17. The development of binary Mg–Ca alloys for use as biodegradable materials within bone10.1016/j.biomaterials.2007.12.021 ↗
18. Investigation on the potential of magnesium alloy AZ31 as a bone implant10.4028/www.scientific.net/MSF.546-549.421 ↗
19. In vitro evaluation of the loosening characteristics of self-tapped and non-self-tapped cortical bone screws10.1097/00003086-198106000-00038 ↗
20. Pullout properties of 3.5-mm AO/ASIF self-tapping and cortex screws in a uniform synthetic material and in canine bone10.1053/jvet.2001.23344 ↗
21. Internal fixation with plates and screws
22. Fertigung von magnesium-implantaten10.37544/1436-4980-2004-11-12-692 ↗
23. Denkena B, Witte F, Podolsky C, Lucas A. Degradable implants made of magnesium alloys. Proceedings of the 5th Euspen international conference, Montpellier, France, 2005.
24. Herstellung resorbierbarer medizinischer implantate aus magnesium [Processing of degradable surgical implants made of magnesium alloys]
25. L’Utilisation du magnesium comme materiel perdu dans l’osteosynthèse
26. Preparation and characterization of a new biomedical magnesium–calcium alloy10.1016/j.matdes.2008.04.017 ↗
27. Development and biocompatibility of a novel corrodible fluoride-coated magnesium–calcium alloy with improved degradation kinetics and adequate mechanical properties for cardiovascular applications10.1002/jbm.a.32582 ↗
28. Comparison of the resorbable magnesium alloys LAE442 und MgCa0.8 concerning their mechanical properties, their progress of degradation and the bone–implant-contact after 12 months implantation duration in a rabbit model10.1002/mawe.200800412 ↗
29. Silicone polymers in controlled drug delivery systems: a review
30. Corrosion resistance of aged die cast magnesium alloy AZ91D10.1016/j.msea.2003.08.060 ↗
31. In vitro corrosion behaviour of Mg alloys in a phosphate buffered solution for bone implant application10.1007/s10856-007-3219-y ↗
32. A method for the study of undecalcified bones and teeth with attached soft tissues10.1111/j.1600-0714.1982.tb00172.x ↗
33. Corrosion mechanisms of magnesium alloys10.1002/(SICI)1527-2648(199909)1:1<11::AID-ADEM11>3.0.CO;2-N ↗
34. Degradable biomaterials based on magnesium corrosion10.1016/j.cossms.2009.04.001 ↗
35. Research on an Mg–Zn alloy as a degradable biomaterial10.1016/j.actbio.2009.06.028 ↗
36. Implant diameter and bone density: effect on initial stability and pull-out resistance
37. Experimental evaluation of the holding power/stiffness of the self-tapping bone screws in normal and osteoporotic bone material10.1016/j.clinbiomech.2005.12.020 ↗
38. Biomechanical analysis of bone mineral density, insertion technique, screw torque, and holding strength of anterior cervical plate screws10.3171/jns.1995.83.2.0324 ↗
39. In vitro and in vivo corrosion measurements of magnesium alloys10.1016/j.biomaterials.2005.07.037 ↗
40. In vivo corrosion behavior of Mg–Mn–Zn alloy for bone implant application10.1002/jbm.a.31273 ↗