journal article·2013-04

Microstructure and tribological properties of reactive hot pressed TiN–TiB2 composites incorporated with or without MoSi2 from room temperature to 800°C

Zhen-Lin Yang, Jia-Hu Ouyang, Zhan-Guo Liu, Xue-Song Liang, Yu-Jin Wang

Wear· Volume 301· Issue 1-2
Publisher page

Abstract

Abstract TiN–TiB 2 composites incorporated with or without MoSi 2 have been prepared by the reactive hot pressing method, using Ti, BN or MoSi 2 powders as the starting materials. The influence of MoSi 2 addition on tribological properties of TiN–TiB 2 composites have been evaluated by using a ball-on-disk friction and wear tester in sliding against alumina ball from room temperature to 800 °C. The wear performance depends mainly upon temperature as well as the applied load. At room temperature and 10 N load, the TiN–TiB 2 ceramic has a wear rate of 1.6×10 –6 mm 3 N –1 m –1 , however, the TiN–TiB 2 –MoSi 2 composite exhibits a wear rate of 1.5×10 –4 mm 3 N –1 m –1 under identical wear condition. At room temperature, the material removal of composites results from brittle fracture and abrasive wear during wear tests. The addition of MoSi 2 can improve the oxidation resistance of TiN–TiB 2 ceramic at high temperatures as it oxidizes to produce a protective SiO 2 layer, which forms an effective barrier layer to restrain from further oxidation. At 800 °C and 10 N load, the wear rate of TiN–TiB 2 –MoSi 2 composite is 1.7×10 –6 mm 3 N –1 m –1 , which is only one fifth as much as the TiN–TiB 2 ceramic. The low wear rate of TiN–TiB 2 –MoSi 2 composite at 800 °C is attributed to high oxidation resistance, the formation of dense SiO 2 scale and self-healing of microcracks.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · MXene and MAX Phase Materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (19)

Show source-provided references
1. The densification and mechanical properties of a TiC and TiB2 hardmetal sintered with a reactive alloy binder10.1002/pssa.2211530109 ↗
2. Simultaneous spark plasma synthesis and densification of TiC–TiB2 composites10.1111/j.1551-2916.2005.00832.x ↗
3. Dense in situ TiB2/TiN and TiB2/TiC ceramic matrix composites: reactive synthesis and properties10.1016/S0921-5093(97)00835-6 ↗
4. Synthesis of dense TiB2–TiN nanocrystalline composites through mechanical and field activation10.1111/j.1151-2916.2001.tb00818.x ↗
5. Reactive hot pressing of titanium nitride–titanium diboride composites at moderate pressures and temperatures10.1111/j.1151-2916.2004.tb06333.x ↗
6. Reactive electric-discharge sintering of TiN–TiB210.1007/s11106-007-0081-x ↗
7. Characterization of structure and properties of TiN–TiB2 nano-composite prepared by ball milling and high pressure heat treatment10.1016/j.jallcom.2007.02.052 ↗
8. Synthesis and consolidation of TiN/TiB2 ceramic composites via reactive spark plasma sintering10.1016/j.jallcom.2010.10.198 ↗
9. Wear mechanisms of TiN–TiB2 ceramic in sliding against alumina from room temperature to 700°C10.1016/j.ceramint.2010.05.019 ↗
10. Friction and wear properties of reactive hot-pressed TiB2–TiN composites in sliding against Al2O3 ball at elevated temperatures10.1016/j.wear.2010.11.057 ↗
11. Isothermal oxidation behavior of reactive hot-pressed TiN–TiB2 ceramics at elevated temperatures10.1016/j.matdes.2010.06.041 ↗
12. Improvement in oxidation resistance of TiB2 by formation of protective SiO2 layer on surface10.1557/JMR.2001.0023 ↗
13. A model for the oxidation of ZrB2, HfB2 and TiB210.1016/j.actamat.2007.07.027 ↗
14. Mechanical behavior of MoSi2 and MoSi2 composites10.1016/0921-5093(94)03246-7 ↗
15. Frictional properties of sintered TiN–TiB2 and Ti(CN)–TiB2 ceramics at high temperature10.1111/j.1151-2916.1987.tb05014.x ↗
16. Microstructure and mechanical properties of in situ produced TiC/TiB2/MoSi2 composites10.1111/j.1551-2916.2005.00279.x ↗
17. Effect of MoSi2 content on the lubricated sliding–wear resistance of ZrC–MoSi2 composites10.1016/j.jeurceramsoc.2010.11.017 ↗
18. E.L. Courtright, Oxygen Permeability for Selected Ceramic Oxides in the Range 1200°C–1700°C, DTIC Document, 1991, pp. 22–31.
19. Oxidation-based materials selection for 2000°C+hypersonic aerosurfaces: theoretical considerations and historical experience10.1023/B:JMSC.0000041686.21788.77 ↗