Laser additive manufacturing of biodegradable magnesium alloy WE43: A detailed microstructure analysis

Florian Bär, Leopold Berger, Lucas Jauer, Güven Kurtuldu, Robin Schäublin, Johannes H. Schleifenbaum, Jörg F. Löffler

Acta Biomaterialia· Volume 98
Publisher page

Abstract

WE43, a magnesium alloy containing yttrium and neodymium as main alloying elements, has become a well-established bioresorbable implant material. Implants made of WE43 are often fabricated by powder extrusion and subsequent machining, but for more complex geometries laser powder bed fusion (LPBF) appears to be a promising alternative. However, the extremely high cooling rates and subsequent heat treatment after solidification of the melt pool involved in this process induce a drastic change in microstructure, which governs mechanical properties and degradation behaviour in a way that is still unclear. In this study we investigated the changes in the microstructure of WE43 induced by LPBF in comparison to that of cast WE43. We did this mainly by electron microscopy imaging, and chemical mapping based on energy-dispersive X-ray spectroscopy in conjunction with electron diffraction for the identification of the various phases. We identified different types of microstructure: an equiaxed grain zone in the center of the laser-induced melt pool, and a lamellar zone and a partially melted zone at its border. The lamellar zone presents dendritic lamellae lying on the Mg basal plane and separated by aligned Nd-rich nanometric intermetallic phases. They appear as globular particles made of Mg3Nd and as platelets made of Mg41Nd5 occurring on Mg prismatic planes. Yttrium is found in solid solution and in oxide particles stemming from the powder particles' shell. Due to the heat influence on the lamellar zone during subsequent laser passes, a strong texture developed in the bulk material after substantial grain growth. STATEMENT OF SIGNIFICANCE: Additively manufactured magnesium alloys have the potential of providing a major breakthrough in bone-reconstruction surgery by serving as biodegradable porous scaffold material. This study is the first to report in detail on the microstructure development of the established magnesium alloy WE43 fabricated by the additive manufacturing process of Laser Powder Bed Fusion (LPBF). It presents unique microstructural features which originate from the laser-melting process. An in situ transmission electron microscopy heating experiment further demonstrates the development of two distinct intermetallic phases in additively manufactured WE43 alloys. While one forms already during solidification, the other precipitates due to the ongoing heat treatment during LPBF processing.
Source: europepmc · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Magnesium Alloys: Properties and Applications · Titanium Alloys Microstructure and Properties · Hydrogen Storage and Materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (60)

Show source-provided references
1. Magnesium and its alloys as orthopedic biomaterials: a review10.1016/j.biomaterials.2005.10.003 ↗
2. Biodegradable magnesium alloys for orthopaedic applications: a review on corrosion, biocompatibility and surface modifications10.1016/j.msec.2016.06.020 ↗
3. Comparison of magnesium alloys and poly-l-lactide screws as degradable implants in a canine fracture model10.1002/jbm.b.33470 ↗
4. Biocompatibility and efficiency of biodegradable magnesium-based plates and screws in the facial fracture model of beagles10.1016/j.joms.2018.01.015 ↗
5. Biocompatibility and degradation properties of WE43 Mg alloys with and without heat treatment: In vivo evaluation and comparison in a cranial bone sheep model10.1016/j.jcms.2017.09.016 ↗
6. M. Schildwächter, BIOTRONIK Announces CE Mark for Magmaris, the First Clinically-Proven Bioresorbable Magnesium Scaffold, https://www.magmaris.com/en/Newsroom/June-15-2016. (2016).
7. Biodegradable magnesium-based screw clinically equivalent to titanium screw in hallux valgus surgery: short term results of the first prospective, randomized, controlled clinical pilot study10.1186/1475-925X-12-62 ↗
8. Differences in microstructure and properties between selective laser melting and traditional manufacturing for fabrication of metal parts: a review10.1007/s11465-015-0341-2 ↗
9. Selective laser melted titanium implants: a new technique for the reconstruction of extensive zygomatic complex defects10.1186/s40902-015-0001-9 ↗
10. Sintering of commercially pure titanium powder with a Nd:YAG laser source10.1016/S1359-6454(02)00567-0 ↗
11. Parametric analysis of thermal behavior during selective laser melting additive manufacturing of aluminum alloy powder10.1016/j.matdes.2014.07.006 ↗
12. Microstructural features of Sc- and Zr-modified Al-Mg alloys processed by selective laser melting
13. Microstructure and mechanical properties of as-processed scandium-modified aluminium using selective laser melting10.1016/j.cirp.2016.04.057 ↗
14. Rapid prototyping: Porous titanium alloy scaffolds produced by selective laser melting for bone tissue engineering10.1089/ten.tec.2008.0288 ↗
15. Layer manufacturing of magnesium and its alloy structures for future applications10.1080/17452751003718629 ↗
16. Microstructure and mechanical properties of selective laser melted magnesium10.1016/j.apsusc.2011.03.004 ↗
17. Experimental investigation on selective laser melting of bulk net-shape pure magnesium10.1080/10426914.2015.1025963 ↗
18. Influence of element vaporization on formability, composition, microstructure, and mechanical performance of the selective laser melted Mg–Zn–Zr components10.1016/j.matlet.2015.05.074 ↗
19. Laser rapid solidification improves corrosion behavior of Mg-Zn-Zr alloy10.1016/j.jallcom.2016.09.019 ↗
20. Selective Laser Melting of magnesium alloys, eCM Meeting Abstracts
21. Additively manufactured biodegradable porous magnesium10.1016/j.actbio.2017.12.008 ↗
22. Additive manufactured WE43 magnesium: a comparative study of the microstructure and mechanical properties with those of powder extruded and as-cast WE43
23. Effect of energy input on formability, microstructure and mechanical properties of selective laser melted AZ91D magnesium alloy10.1016/j.msea.2014.05.092 ↗
24. Effects of processing parameters on properties of selective laser melting Mg-9%Al powder mixture10.1016/j.matdes.2011.06.061 ↗
25. ASTM B951-11 (2018) Standard Practice for Codification of Unalloyed Magnesium and Magnesium-Alloys, Cast and Wrought, West Conshohocken, PA, 2018. https://doi.org/10.1520/B0080.10.1520/B0080 ↗
26. Recent advances on the development of magnesium alloys for biodegradable implants10.1016/j.actbio.2014.07.005 ↗
27. Progress of biodegradable metals10.1016/j.pnsc.2014.08.014 ↗
28. In vivo study of a biodegradable orthopedic screw (MgYREZr-alloy) in a rabbit model for up to 12 months10.1177/0885328212472215 ↗
29. On the biodegradation performance of an Mg-Y-RE alloy with various surface conditions in simulated body fluid10.1016/j.actbio.2008.07.034 ↗
30. Effect of Y on the bio-corrosion behavior of extruded Mg–Zn–Mn alloy in Hank's solution10.1016/j.msec.2009.09.014 ↗
31. The influence of yttrium (Y) on the corrosion of Mg-Y binary alloys10.1016/j.corsci.2010.07.019 ↗
32. Composition of corrosion layers on a magnesium rare-earth alloy in simulated body fluids10.1002/jbm.a.31887 ↗
33. Rokhlin · 2003
34. Additive manufacturing of magnesium alloys, eCM Meeting Abstracts
35. Microstructure of WE43 casting magnesium alloys
36. Characterisation of strengthening precipitate phases in a Mg–Y–Nd alloy10.1016/S1359-6454(00)00013-6 ↗
37. J.-F. Nie, Precipitation and hardening in magnesium alloys, in: 2012, pp. 3891–3939. https://doi.org/10.1007/s11661-012-1217-2.10.1007/s11661-012-1217-2 ↗
38. B. Predel, Mg-Nd (Magnesium-Neodymium), in: Madelung O. (eds) Li-Mg – Nd-Zr. Landolt-Börnstein – Group IV Physical Chemistry (Numerical Data and Functional Relationships in Science and Technology), Springer-Verlag, Berlin, Heidelberg, 1987, https://doi.org/10.1007/10522884_1986.10.1007/10522884_1986 ↗
39. The formation and structure of precipitates in a dilute magnesium-neodymium alloy10.1016/0022-5088(73)90007-6 ↗
40. In situ heat treatment in selective laser melted martensitic AISI 420 stainless steels10.1016/j.matdes.2015.08.045 ↗
41. More features, more tools, more CrysTBox10.1107/S1600576717006793 ↗
42. EMS - a software package for electron diffraction analysis and HREM image simulation in materials science10.1016/0304-3991(87)90080-5 ↗
43. The crystal structures of magnesium-rich compounds in the systems La-Mg, Ce-Mg, and Nd-Mg
44. Phase relationships in the neodymium-magnesium alloy system10.1007/BF02647869 ↗
45. GdMg5: a complex structure with a large cubic cell10.1107/S0108270186097019 ↗
46. Precipitation in magnesium alloy WE54 during isothermal ageing at 250 C10.1016/S1359-6462(99)00084-6 ↗
47. Magnetic interactions and crystal field in RMg3 compounds (R = Ce, Pr, Nd)10.1016/0304-8853(81)90054-8 ↗
48. Intermetallic compounds of rare-earth and 3d transition metals10.1088/0034-4885/40/10/002 ↗
49. Compounds with the alpha-Mn superstructure in the rare earth-magnesium system
50. Dantzig · 2009
51. B. Predel, Gd-Mg (Gadolinium-Magnesium): Datasheet from Landolt-Börnstein – Group IV Physical Chemistry Volume 5F: “Ga-Gd – Hf-Zr” in Springer Materials, Springer-Verlag, Berlin/Heidelberg, 1996, https://doi.org/10.1007/10501684_1427.10.1007/10501684_1427 ↗
52. K. Neh, M. Ullmann, R. Kawalla, Twin-roll-casting and hot rolling of magnesium alloy WE43, in: 2014, pp. 1553–1558, https://doi.org/10.1016/j.proeng.2014.10.189.10.1016/j.proeng.2014.10.189 ↗
53. P. Franke, D. Neuschütz, eds., “Binary Systems. Part 4: Binary Systems from Mn-Mo to Y-Zr”, Springer-Verlag, Berlin/Heidelberg, 2006, https://doi.org/10.1007/10757285_12.10.1007/b76778 ↗
54. Y. Zhao, G. Wu, Q. Lu, J. Wu, R. Xu, K.W.K. Yeung, et al., Improved surface corrosion resistance of WE43 magnesium alloy by dual titanium and oxygen ion implantation, in: 2013, pp. 407–411, https://doi.org/10.1016/j.tsf.2012.05.046.10.1016/j.tsf.2012.05.046 ↗
55. Nucleation in undercooled liquids10.1016/0025-5416(84)90206-4 ↗
56. Orientation selection in dendritic evolution10.1038/nmat1693 ↗
57. α-Mg primary phase formation and dendritic morphology transition in solidification of a Mg-Nd-Gd-Zn-Zr casting alloy10.1016/j.actamat.2016.06.035 ↗
58. Dendritic morphology of α-Mg during the solidification of Mg-based alloys: 3D experimental characterization by X-ray synchrotron tomography and phase-field simulations10.1016/j.scriptamat.2011.07.040 ↗
59. Characterisation of the 3-D dendrite morphology of magnesium alloys using synchrotron X-ray tomography and 3-D phase-field modelling10.1016/j.actamat.2015.03.044 ↗
60. Dendritic solidification of magnesium alloy AZ9110.1007/BF02656439 ↗