Metallic zinc implanted into the abdominal aorta of rats out to 6months has been demonstrated to degrade while avoiding responses commonly associated with the restenosis of vascular implants. However, major questions remain regarding whether a zinc implant would ultimately passivate through the production of stable corrosion products or via a cell mediated fibrous encapsulation process that prevents the diffusion of critical reactants and products at the metal surface. Here, we have conducted clinically relevant long term in vivo studies in order to characterize late stage zinc implant biocorrosion behavior and products to address these critical questions. We found that zinc wires implanted in the murine artery exhibit steady corrosion without local toxicity for up to at least 20months post-implantation, despite a steady buildup of passivating corrosion products and intense fibrous encapsulation of the wire. Although fibrous encapsulation was not able to prevent continued implant corrosion, it may be related to the reduced chronic inflammation observed between 10 and 20months post-implantation. X-ray elemental and infrared spectroscopy analyses confirmed zinc oxide, zinc carbonate, and zinc phosphate as the main components of corrosion products surrounding the Zn implant. These products coincide with stable phases concluded from Pourbaix diagrams of a physiological solution and in vitro electrochemical impedance tests. The results support earlier predictions that zinc stents could become successfully bio-integrated into the arterial environment and safely degrade within a time frame of approximately 1-2years. Staement of significance Previous studies have shown zinc to be a promising candidate material for bioresorbable endovascular stenting applications. An outstanding question, however, is whether a zinc implant would ultimately passivate through the production of stable corrosion products or via a cell mediated tissue encapsulation process that prevented the diffusion of critical reactants and products at the metal surface. We found that zinc wires implanted in the murine artery exhibit steady corrosion for up to at least 20months post-implantation. The results confirm earlier predictions that zinc stents could safely degrade within a time frame of approximately 1-2years.
Source: europepmc · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Magnesium Alloys: Properties and Applications · Trace Elements in Health · Bone Tissue Engineering Materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (60)
Show source-provided references
1. A randomized comparison of coronary-stent placement and balloon angioplasty in the treatment of coronary artery disease10.1056/NEJM199408253310802 ↗
2. A comparison of balloon-expandable-stent implantation with balloon angioplasty in patients with coronary artery disease10.1056/NEJM199408253310801 ↗
3. Coronary stents: a materials perspective10.1016/j.biomaterials.2006.11.042 ↗
4. Morphological predictors of restenosis after coronary stenting in humans10.1161/01.CIR.0000019071.72887.BD ↗
5. Incomplete stent apposition and very late stent thrombosis after drug-eluting stent implantation10.1161/CIRCULATIONAHA.106.658237 ↗
6. The incidence and clinical impact of stent strut fractures developed after drug-eluting stent implantation10.1016/j.ijcard.2007.02.033 ↗
7. Bioresorbable scaffold technologies10.1253/circj.CJ-10-1135 ↗
8. Bioabsorbable coronary stents10.1161/CIRCINTERVENTIONS.109.859173 ↗
9. A biodegradable poly-l-lactic acid coronary stent in the porcine coronary artery10.1111/j.1540-8183.1999.tb00673.x ↗
10. A biodegradable stent based on poly (L-lactide) and poly (4-hydroxybutyrate) for peripheral vascular application: preliminary experience in the pig10.1177/152660280701400518 ↗
11. A biodegradable slotted tube stent based on poly (L-lactide) and poly (4-hydroxybutyrate) for rapid balloon-expansion10.1007/s10439-007-9376-9 ↗
12. Initial and 6-month results of biodegradable poly-l-lactic acid coronary stents in humans10.1161/01.CIR.102.4.399 ↗
13. Biocorrosion of magnesium alloys: a new principle in cardiovascular implant technology?10.1136/heart.89.6.651 ↗
14. Degradable biomaterials based on magnesium corrosion10.1016/j.cossms.2009.04.001 ↗
15. Iron–manganese: new class of metallic degradable biomaterials prepared by powder metallurgy10.1179/174329008X284868 ↗
16. Fe-Mn alloys for metallic biodegradable stents: degradation and cell viability studies10.1016/j.actbio.2009.11.025 ↗
17. Long-term biocompatibility of a corrodible peripheral iron stent in the porcine descending aorta10.1016/j.biomaterials.2006.05.029 ↗
18. A simplified in vivo approach for evaluating the bioabsorbable behavior of candidate stent materials10.1002/jbm.b.31922 ↗
19. Biodegradable metals for cardiovascular stents: from clinical concerns to recent Zn-alloys10.1002/adhm.201501019 ↗
20. Effects of alloying elements (Mn Co, Al, W, Sn, B, C and S) on biodegradability and in vitro biocompatibility of pure iron
21. A novel approach to temporary stenting: degradable cardiovascular stents produced from corrodible metal—results 6–18 months after implantation into New Zealand white rabbits10.1136/heart.86.5.563 ↗
22. Long-term in vivo corrosion behavior, biocompatibility and bioresorption mechanism of a bioresorbable nitrided iron scaffold10.1016/j.actbio.2017.03.020 ↗
23. In vivo corrosion and corrosion protection of magnesium alloy LAE44210.1016/j.actbio.2009.10.012 ↗
24. Biodegradable magnesium scaffolds: Part I: appropriate inflammatory response10.1002/jbm.a.31170 ↗
25. Implant-derived magnesium induces local neuronal production of CGRP to improve bone-fracture healing in rats10.1038/nm.4162 ↗
26. Corrosion fatigue behaviors of two biomedical Mg alloys – AZ91D and WE43 – in simulated body fluid10.1016/j.actbio.2010.07.026 ↗
27. In vitro degradation and mechanical integrity of calcium-containing magnesium alloys in modified-simulated body fluid10.1016/j.biomaterials.2008.02.003 ↗
28. Magnesium alloys as body implants: fracture mechanism under dynamic and static loadings in a physiological environment10.1016/j.actbio.2011.10.031 ↗
29. Control of biodegradation of biocompatable magnesium alloys10.1016/j.corsci.2007.01.001 ↗
30. In vivo study of nanostructured diopside (CaMgSi2O6) coating on magnesium alloy as biodegradable orthopedic implants10.1016/j.apsusc.2014.05.130 ↗
31. Mg-Zr-Sr alloys as biodegradable implant materials10.1016/j.actbio.2012.04.028 ↗
32. Mechanical properties, in vitro corrosion and biocompatibility of newly developed biodegradable Mg-Zr-Sr-Ho alloys for biomedical applications
33. MgZnCa glasses without clinically observable hydrogen evolution for biodegradable implants10.1038/nmat2542 ↗
34. Safety and performance of the drug-eluting absorbable metal scaffold (DREAMS) in patients with de-novo coronary lesions: 12 month results of the prospective, multicentre, first-in-man BIOSOLVE-I trial10.1016/S0140-6736(12)61765-6 ↗
35. Safety and performance of the second-generation drug-eluting absorbable metal scaffold in patients with de-novo coronary artery lesions (BIOSOLVE-II): 6 month results of a prospective, multicentre, non-randomised, first-in-man trial10.1016/S0140-6736(15)00447-X ↗
36. Sustained safety and performance of the second-generation drug-eluting absorbable metal scaffold in patients with de novo coronary lesions: 12-month clinical results and angiographic findings of the BIOSOLVE-II first-in-man trial10.1093/eurheartj/ehw196 ↗
37. Materials and manufacturing technologies available for production of a pediatric bioabsorbable stent10.1155/2013/137985 ↗
38. Zinc exhibits ideal physiological corrosion behavior for bioabsorbable stents10.1002/adma.201300226 ↗
39. Structural characteristics and in vitro biodegradation of a novel Zn-Li alloy prepared by induction melting and hot rolling
40. Zn-Li alloy after extrusion and drawing: structural, mechanical characterization, and biodegradation in abdominal aorta of rat10.1016/j.msec.2017.02.167 ↗
41. Evaluation of wrought Zn–Al alloys (1, 3, and 5 wt% Al) through mechanical and in vivo testing for stent applications
42. Metallic zinc exhibits optimal biocompatibility for bioabsorbable endovascular stents10.1016/j.msec.2015.07.022 ↗
43. In vitro cytotoxicity, adhesion, and proliferation of human vascular cells exposed to zinc10.1021/acsbiomaterials.6b00035 ↗
44. Zinc toxicity10.1093/ajcn/51.2.225 ↗
45. Corrosion characteristics dictate the long-term inflammatory profile of degradable zinc arterial implants10.1021/acsbiomaterials.6b00591 ↗
46. Rates of in vivo (arterial) and in vitro biocorrosion for pure magnesium10.1002/jbm.a.35179 ↗
47. Importance of oxide film in endovascular biodegradable zinc stents10.1680/jsuin.16.00014 ↗
48. Preparation of amorphous calcium-magnesium phosphates at pH 7 and characterization by X-ray absorption and fourier transform infrared spectroscopy10.1016/0022-0248(88)90455-1 ↗
49. Magnesium in the murine artery: probing the products of corrosion10.1016/j.actbio.2013.11.021 ↗
50. Raman and infrared spectroscopic study of the vivianite-group phosphates vivianite, baricite and bobierrite10.1180/0026461026660077 ↗
51. Preparation and characterization of magnesium/carbonate co-substituted hydroxyapatites10.1023/A:1015793927364 ↗
52. Phase and thermal stability of nanocrystalline hydroxyapatite prepared via microwave heating10.1016/j.tca.2006.04.013 ↗
53. How useful is SBF in predicting in vivo bone bioactivity?10.1016/j.biomaterials.2006.01.017 ↗
54. Self-repairing oxides to protect zinc: review, discussion and prospects10.1016/j.corsci.2013.01.011 ↗
55. Corrosion of zinc as a function of pH
56. Zinc transport in mammalian cells10.1152/ajpcell.1996.270.2.C401 ↗
57. Mammalian zinc transport, trafficking, and signals10.1074/jbc.R600011200 ↗
58. Long-term in vivo degradation behaviour and biocompatibility of the magnesium alloy ZEK100 for use as a biodegradable bone implant10.1016/j.actbio.2012.08.028 ↗
59. A surface-eroding poly(1,3-trimethylene carbonate) coating for fully biodegradable magnesium-based stent applications: toward better biofunction, biodegradation and biocompatibility10.1016/j.actbio.2013.02.041 ↗
60. Cui · 2004