Fatigue behaviors of HP-Mg, Mg–Ca and Mg–Zn–Ca biodegradable metals in air and simulated body fluid
Source abstract
Abstract
Unlabelled The dynamic loading in human body, along with the corrosive body fluid, presents a great challenge for the practical use of biodegradable magnesium implants. In this study, a high purity magnesium (99.99wt.%) and two typical promising biodegradable magnesium alloys (binary Mg-1Ca and ternary Mg-2Zn-0.2Ca) were chosen as the experimental materials. Their dynamic mechanical performances were comparatively evaluated by carrying out fatigue tests in air and in simulated body fluid (SBF). The fatigue strengths of HP-Mg, Mg-1Ca and Mg-2Zn-0.2Ca were all around 90MPa in air, however, they decreased to 52MPa, 70MPa and 68MPa in SBF at 4×10(6)cycles, respectively. The fatigue cracks initiated from the microstructural defects when tested in air, but nucleated from surface corrosion pits when tested in SBF. Cyclic loading significantly increased the corrosion rates of all the experimental materials compared to that in static SBF. Moreover, based on our findings, the fatigue failure processes and interactions between material, corrosion and cyclic loading were systematically discussed. Statement of significance Fatigue strength and life are vital parameters to the design of metallic implant devices. For the corrosion fatigue of biomedical magnesium alloys, we reported the corrosion fatigue behavior of AZ91D and WE43 in SBF (Acta Biomaterialia, 6 (2010) 4605-4613), and till now there is no other reports to our knowledge. We spent 3years to finish the fatigue testing and get S-N curves for three more magnesium biomaterials, and our significant finding is that the fatigue strengths of HP-Mg, Mg-1Ca and Mg-2Zn-0.2Ca are all around 90MPa in air but 52MPa, 70MPa and 68MPa in SBF at 4×10(6)cycles, which will provide the first-hand data for the future magnesium implants design.
Source: europepmc · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Magnesium Alloys: Properties and Applications · Orthopaedic implants and arthroplasty · Aluminum Alloys Composites Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (60)
Show source-provided references
1. Biodegradable metals10.1016/j.mser.2014.01.001 ↗
2. Biodegradable magnesium-based screw clinically equivalent to titanium screw in hallux valgus surgery: short term results of the first prospective, randomized, controlled clinical pilot study10.1186/1475-925X-12-62 ↗
3. Safety and performance of the second-generation drug-eluting absorbable metal scaffold in patients with de-novo coronary artery lesions (BIOSOLVE-II): 6month results of a prospective, multicentre, non-randomised, first-in-man trial10.1016/S0140-6736(15)00447-X ↗
4. Magnesium: an update on physiological, clinical and analytical aspects10.1016/S0009-8981(99)00258-2 ↗
5. Progress and challenge for magnesium alloys as biomaterials10.1002/adem.200800035 ↗
6. Stress shielding and bone resorption in shoulder arthroplasty10.1067/mse.2003.22 ↗
7. Enhanced antimicrobial properties, cytocompatibility, and corrosion resistance of plasma-modified biodegradable magnesium alloys10.1016/j.actbio.2013.10.012 ↗
8. In vivo stimulation of bone formation by aluminum and oxygen plasma surface-modified magnesium implants10.1016/j.biomaterials.2013.08.052 ↗
9. Unique antitumor property of the Mg–Ca–Sr alloys with addition of Zn10.1038/srep21736 ↗
10. Reasons for removal of rigid internal fixation devices in craniofacial surgery10.1097/00001665-199801000-00009 ↗
11. The effects of rigid fixation on craniofacial growth of rhesus monkeys10.1097/00006534-199401000-00001 ↗
12. Safety and performance of the drug-eluting absorbable metal scaffold (DREAMS) in patients with de-novo coronary lesions: 12month results of the prospective, multicentre, first-in-man BIOSOLVE-I trial10.1016/S0140-6736(12)61765-6 ↗
13. Cranio-orbital reconstruction: safety and image quality of metallic implants on CT and MRI scanning10.1097/00006534-199410000-00004 ↗
14. Understanding magnesium corrosion—a framework for improved alloy performance10.1002/adem.200310405 ↗
15. Cracking of magnesium-based biodegradable implant alloys under the combined action of stress and corrosive body fluid: a review
16. Magnesium alloys as body implants: fracture mechanism under dynamic and static loadings in a physiological environment10.1016/j.actbio.2011.10.031 ↗
17. What is fatigue damage? A view point from the observation of low cycle fatigue process10.1016/j.ijfatigue.2004.10.009 ↗
18. Corrosion fatigue behaviors of two biomedical Mg alloys – AZ91D and WE43 – in simulated body fluid10.1016/j.actbio.2010.07.026 ↗
19. Corrosion fatigue behavior of extruded magnesium alloy AZ61 under three different corrosive environments10.1016/j.ijfatigue.2008.02.012 ↗
20. Fatigue of biomaterials: a review10.1016/S0142-1123(00)00052-9 ↗
21. Fatigue-life assessment and validation techniques for metallic vascular implants10.1016/j.biomaterials.2009.10.028 ↗
22. Failure of orthopedic implants: three case histories10.1016/1044-5803(91)90012-S ↗
23. Premature fracture of a stainless steel 316L orthopaedic plate implant by alternative episodes of fatigue and cleavage decoherence10.1016/j.engfailanal.2006.11.010 ↗
24. In-body corrosion fatigue failure of a stainless steel orthopaedic implant with a rare collection of different damage mechanisms10.1016/j.engfailanal.2006.11.037 ↗
25. Failure analysis of a commercially pure titanium plate for osteosynthesis10.1016/S1350-6307(02)00067-5 ↗
26. Corrosion fatigue fracture of magnesium alloys in bioimplant applications: a review10.1016/j.engfracmech.2014.08.009 ↗
27. Fatigue strength of a magnesium MA2-1 alloy after equal-channel angular pressing10.1134/S0036029510090120 ↗
28. Recent advances on the development of magnesium alloys for biodegradable implants10.1016/j.actbio.2014.07.005 ↗
29. Aluminum as a risk factor for Alzheimer’s disease10.1590/S0104-11692008000100023 ↗
30. Evaluation of short-term effects of rare earth and other elements used in magnesium alloys on primary cells and cell lines10.1016/j.actbio.2009.09.024 ↗
31. Comparative study of fluoride conversion coatings formed on biodegradable powder metallurgy Mg: the effect of chlorides at physiological level10.1016/j.msec.2011.01.010 ↗
32. Assessing the degradation performance of ultrahigh-purity magnesium in vitro and in vivo10.1016/j.corsci.2014.09.008 ↗
33. The development of binary Mg–Ca alloys for use as biodegradable materials within bone10.1016/j.biomaterials.2007.12.021 ↗
34. Corrosion resistance and surface biocompatibility of a microarc oxidation coating on a Mg–Ca alloy10.1016/j.actbio.2010.11.034 ↗
35. Development of biodegradable Mg–Ca alloy sheets with enhanced strength and corrosion properties through the refinement and uniform dispersion of the Mg2Ca phase by high-ratio differential speed rolling10.1016/j.actbio.2014.09.029 ↗
36. Electrochemical characteristics of bioresorbable binary MgCa alloys in Ringer’s solution: revealing the impact of local pH distributions during in-vitro dissolution10.1016/j.msec.2015.11.069 ↗
37. (last accessed on May 12, 2016).
38. ASTM-E8-04 · 2004
39. ASTM-E466-96 · 2002
40. How useful is SBF in predicting in vivo bone bioactivity?10.1016/j.biomaterials.2006.01.017 ↗
41. ASTM G31-72 · 2004
42. The effects of calcium and yttrium additions on the microstructure, mechanical properties and biocompatibility of biodegradable magnesium alloys10.1007/s10853-010-4843-3 ↗
43. Comment on Mg–Zn (magnesium–zinc)10.1007/BF02667700 ↗
44. Ternary compounds and relative phase equilibria in the Mg-rich side of the Mg–Zn–Ca system
45. The origins of high hardening and low ductility in magnesium10.1038/nature15364 ↗
46. Texture weakening and ductility variation of Mg–2Zn alloy with CA or RE addition10.1016/j.msea.2015.08.025 ↗
47. Corrosion fatigue behavior of extruded AZ80, AZ61, and AM60 magnesium alloys in distilled water10.1007/s11223-008-0034-8 ↗
48. Corrosion fatigue of a magnesium alloy in modified simulated body fluid10.1016/j.engfracmech.2014.07.007 ↗
49. The role of twinning–detwinning on fatigue fracture morphology of Mg–3%Al–1%Zn alloy10.1016/j.msea.2008.04.056 ↗
50. Enhanced very high cycle fatigue performance of extruded Mg–12Gd–3Y–0.5Zr magnesium alloy10.1016/j.msea.2010.12.092 ↗
51. Effect of twinning, slip, and inclusions on the fatigue anisotropy of extrusion-textured AZ61 magnesium alloy10.1016/j.msea.2011.05.047 ↗
52. Corrosion mechanism applicable to biodegradable magnesium implants10.1016/j.mseb.2010.12.017 ↗
53. Degradable biomaterials based on magnesium corrosion10.1016/j.cossms.2009.04.001 ↗
54. Neuropathology of aluminum toxicity in rats (glutamate and GABA impairment)10.1016/S1043-6618(02)00336-5 ↗
55. Effect of different Ti–6Al–4V surface treatments on osteoblasts behaviour10.1016/S0142-9612(01)00266-6 ↗
56. Effect of long-term intake of Y3+ in drinking water on gene expression in brains of rats10.1016/S1002-0721(06)60126-9 ↗
57. Fatigue of magnesium alloys10.1002/adem.200400021 ↗
58. Dieter · 1988
59. Biodegradable behaviour and fatigue life of ZEK100 magnesium alloy in simulated physiological environment10.1111/ffe.12262 ↗
60. Corrosion fatigue behavior of extruded magnesium alloy AZ80-T5 in a 5% NaCl environment10.1016/j.engfracmech.2010.03.032 ↗