Breakeven Point in Ultimate Thickness Between Moisture-Reduced Shrinkage and Thickness Recovery of Densified Softwood Species: Part 1: At Room Temperature
Source abstract
Abstract
Thermo-hygro-mechanical (THM) densification technique has been used to increase the density and mechanical properties of underutilized softwoods. One potential application of the densified softwoods is the substitute of hardwood flooring. This technique is usually employed to mechanically compress the softened wood in the radial direction with the assistance of a high temperature greater than 100°C. Use of high temperature shows that the THM densification process consumes a lot of thermal energy, losing the economic competitivity in comparison with the hardwood floorings. From the energysaving point of view, the authors tried to densify two softwood species at three temperatures of 20°C, 50°C, and 90°C with various compression ratios (CRs), followed by air-drying (AD) the densified wood specimens at room temperature. It was discovered that the decrease of MC would result, during the AD conditioning, in shrinkage of densified wood, which could offset part of the thickness recovery of densified wood. However, this phenomenon was not well addressed. This study was aimed at discussing the effect of shrinkage on the thickness recovery ratio (TRR) of densified softwoods. To ignore the influence of temperature on the shrinkage capability of wood because of the decomposition of hemicellulose, only the data of densified wood specimens compressed and posttreated at room temperature were analyzed in this study. Two softwood species used were eastern white pine (Pinus strobus) and balsam fir (Abies balsamea). The CRs ranged from 0.05 CR and 0.65 CR. The major findings were: 1) the final thickness of densified wood was a result of “recovery” containing elastic deformation and viscoelastic deformation, and “shrinkage” of cell walls; 2) the relationship of TRR of densified pine or fir and CR followed an exponential increase trend at 20°C; 3) after AD conditioning, the breakeven point in thickness between moisture-reduced shrinkage and visco-elastic recovery when the CRs of densified pine and fir at 20°C were 0.12 and 0.13, respectively.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Wood Treatment and Properties · Bamboo properties and applications · Tree Root and Stability Studies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (16)
Show source-provided references
1. Fang CH, Mariotti N, Cloutier A, Koubaa A, Blanchet P (2012) Densification of wood veneers by compression combined with heat and steam. Eur J Wood Wood Prod 70:155-163.10.1007/s00107-011-0524-4 ↗
2. Gong M, Lamason C, Li L (2010) Interactive effect of surface densification and post heat-treatment on aspen wood. J Mater Process Technol 210(2):293-296.10.1016/j.jmatprotec.2009.09.013 ↗
3. Gong M, Nakatani M, Yang Y, Afzal M (2006) Maximum ratios of softwoods produced in eastern Canada. Proc. 9th World Conference on Timber Engineering, 6-10 August 2006, Portland, OR. CD-ROM.
4. Ito Y, Tanahashi M, Shigematsu M, Shinoda Y, Ohta C (1998a) Compressive molding of wood by high-pressure steam-treatmeant: Part 1. Development of compressively molded squares from thinning. Holzforschung 52:211-216.10.1515/hfsg.1998.52.2.211 ↗
5. Kamke FA, Kutnar A (2010) Transverse compression behavior of wood in saturated steam at 150-170°C. Wood Fiber Sci 42(3):377-387.
6. Kelley S, Rials TG, Glasser WG (1987) Relaxation behavior of the amorphous components of wood. J Mater Sci 22:617-624.10.1007/BF01160778 ↗
7. Kutnar A, Kamke FA (2012) Compression of wood under saturated steam, superheated steam, and transient conditions at 150°C, 160°C, and 170°C. Wood Sci Technol 46: 73-88.10.1007/s00226-010-0380-0 ↗
8. Li L, Gong M, Yuan N, Li D (2012) Recovery of mechanically induced residual stresses in densified softwoods created during a densification process. Wood Fiber Sci 44(4):1-9.
9. Navi P, Gigardet F (2000) Effects of thermo-hydro mechanical treatment on the structure and properties of wood. Holzforschung 54:287-293.10.1515/HF.2000.048 ↗
10. NorimotoM(1993) Large compressive deformation in wood. Mokuzai Gakkaishi 39(8):867-874 (In Japanese with abstract in English).
11. OriginLab Corporation (2010) OriginPro 8 SR4. OriginLab Corporation, Northampton, MA.
12. Popescu MC, Lisa G, Froidevaus J, Navi P, Popescu CM (2014) Evaluation of the thermal stability and set recovery of thermo-mechanically treated lime (Tilia cordata) wood. Wood Sci Technol 48:85-97.10.1007/s00226-013-0588-x ↗
13. Rautkari L, Honkanen J, Hill CAS, Ridley-Ellis D, Hughes M (2014) Mechanical and physical properties of thermally modified Scots pine wood in high pressure reactor under saturated steam at 120, 150, and 180°C. Eur J Wood Wood Prod 72:33-41.10.1007/s00107-013-0749-5 ↗
14. Rautkari L, Properzi M, Pichelin F, Hughees M (2010) Properties and set-recovery of surface densified Norway spruce and European beech. Wood Sci Technol 44:679-691.10.1007/s00226-009-0291-0 ↗
15. Scharfetter H (1990) Thickness stability of particleboard. Int J Adhes Adhes 1:93-95.10.1016/0143-7496(80)90064-0 ↗
16. Welzbacher CR, Wehsener J, Rapp AO, Haller P (2008) Thermo-mechanical densification combined with thermal modification of Norway spruce (Picea abies Karst) in industrial scale-dimensional stability and durability aspects. Holz Roh Werkst 66:39-49.10.1007/s00107-007-0198-0 ↗