journal article·2011-03

Moisture-driven fracture in solid wood

Finn Larsen, Sigurdur Ormarsson, John Forbes Olesen

Publisher page

Abstract

Abstract Moisture-induced fractures in solid timber create considerable problems for both building industries and sawmills. Cracks caused by kiln-drying of solid timber are extremely difficult to predict. This paper reports on experiments concerned with methods of reducing cracks in wood and with the cracking behaviour of Norway spruce discs. The spruce was dried from green moisture content down to equilibrium moisture content at 23°C and 64% relative humidity. Moisture-related strains and crack development were measured using a digital image correlation system, Aramis. The moisture gradient in the longitudinal direction had a major influence on crack behaviour and was quite pronounced in discs more than 30 mm thick, but much more limited in discs only 15 mm thick. Although the thicker discs often cracked very early in the drying process, many of these cracks became invisible later on in the drying process, suggesting that sealing the ends of timber logs while in the green moisture state could considerably reduce the development of end-cracks. The initial moisture content and the shrinkage properties of the wood varied markedly from pith to bark. The importance of taking material inhomogeneities into account when modelling crack propagation in solid wood is emphasized.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Wood Treatment and Properties · Tree Root and Stability Studies · Lignin and Wood Chemistry

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (9)

Show source-provided references
1. Aramis 2007 . Aramis v6 user manual . GOM mbH, GOM optical measuring techniques.http://www.gom.com
2. Dahlblom , O. , Petersson , H. & Ormarsson , S. 1999 . Characterization of shrinkage . European project FAIR CT 96-1915 , Improved spruce timber utilization ( Final Rep. sub-task AB1.5. Division of Structural Mechanies, Lund Institute of Technology, Lund University, Sweden ).
3. Krabbenhøft , K. 2003 . Moisture transport in wood. A study of physical–mathematical models and their numerical implementation . PhD thesis (Chapters 4 and 5), Technical University of Denmark, Copenhagen .
4. 10.1080/0737393080194469710.1080/07373930801944697 ↗
5. 10.1007/BF0070278910.1007/BF00702789 ↗
6. 10.1007/s00226005012610.1007/s002260050126 ↗
7. 10.1515/hfsg.1995.49.4.36310.1515/hfsg.1995.49.4.363 ↗
8. Valentin , G. H. , Boström , L. Gustafsson P. J. , Ranta-Maunus , A. & Gowda , S 1991 . Application of fracture mechanics to timber structures . RILEM state-of-the-art report (Res. Notes 1262), Technical Research Centre of Finland, Espoo, Finland .
9. 10.1080/0737393000891780410.1080/07373930008917804 ↗