journal article·2013-11

Effect of biologically relevant ions on the corrosion products formed on alloy AZ31B: An improved understanding of magnesium corrosion

Yongseok Jang, Boyce Collins, Jagannathan Sankar, Yeoheung Yun

Acta Biomaterialia· Volume 9· Issue 10
Publisher page

Abstract

Simulated physiological solutions mimicking human plasma have been utilized to study the in vitro corrosion of biodegradable metals. However, corrosion and corrosion product formation are different for different solutions with varied responses and, hence, the prediction of in vivo degradation behavior is not feasible based on these studies alone. This paper reports the role of physiologically relevant salts and their concentrations on the corrosion behavior of a magnesium alloy (AZ31B) and subsequent corrosion production formation. Immersion tests were performed for three different concentrations of Ca(2+), HPO4(2-), HCO3(-) to identify the effect of each ion on the corrosion of AZ31B assessed at 1, 3 and 10 days. Time-lapse morphological characterization of the samples was performed using X-ray computed tomography and scanning electron microscopy. The chemical composition of the surface corrosion products was determined by electron dispersive X-ray spectroscopy and X-ray diffraction. The results show that: (1) calcium is not present in the corrosion product layer when only Cl(-) and OH(-) anions are available; (2) the presence of phosphate induces formation of a densely packed amorphous magnesium phosphate corrosion product layer when HPO4(2-) and Cl(-) are present in solution; (3) octacalcium phosphate and hydroxyapatite (HAp) are deposited on the surface of the magnesium alloy when HPO4(2-) and Ca(2+) are present together in NaCl solution (this coating limits localized corrosion and increases general corrosion resistance); (4) addition of HCO3(-) accelerates the overall corrosion rate, which increases with increasing bicarbonate concentration; (5) the corrosion rate decreases due to the formation of insoluble HAp on the surface when HCO3(-), Ca(2+), and HPO4(2-) are present together.
Source: europepmc · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Magnesium Alloys: Properties and Applications · Corrosion Behavior and Inhibition · Hydrogen Storage and Materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (47)

Show source-provided references
1. Magnesium alloys as implant materials – principles of property design for Mg–RE alloys10.1016/j.actbio.2009.09.010 ↗
2. Degradable metallic biomaterials: design and development of Fe–Mn alloys for stents10.1002/jbm.a.32224 ↗
3. First-principles studies on alloying and simplified thermodynamic aqueous chemical stability of calcium-, zinc-, aluminum-, yttrium- and iron-doped magnesium alloys10.1016/j.actbio.2009.08.016 ↗
4. In vitro and in vivo corrosion measurements of magnesium alloys10.1016/j.biomaterials.2005.07.037 ↗
5. Degradable biomaterials based on magnesium corrosion10.1016/j.cossms.2009.04.001 ↗
6. Ion release from magnesium materials in physiological solutions under different oxygen tensions10.1007/s10856-011-4490-5 ↗
7. Revolutionizing biodegradable metals10.1016/S1369-7021(09)70273-1 ↗
8. The electrochemical corrosion of pure magnesium in 1N NaCl10.1016/S0010-938X(96)00172-2 ↗
9. Corrosion product formation during NaCl induced atmospheric corrosion of magnesium alloy AZ91D10.1016/j.corsci.2006.08.004 ↗
10. Corrosion of high purity Mg, AZ91, ZE41 and Mg2Zn0.2Mn in Hank’s solution at room temperature10.1016/j.corsci.2010.10.008 ↗
11. Waizy H, Weizbauer A, Moderjewski C, Witte F, Windhagen H, Lucas et al. A. In vitro corrosion of ZEK100 plates in Hank’s balanced salt solution. BioMedical Engineering Online 2012;11/12:1-14; http://www.biomedical-engineering-online.com/content/11/1/12.10.1186/1475-925X-11-12 ↗
12. Corrosion behavior of biomedical AZ91 magnesium alloy in simulated body fluids10.1557/jmr.2007.0233 ↗
13. Composition of corrosion layers on a magnesium rare-earth alloy in simulated body fluids10.1002/jbm.a.31887 ↗
14. Corrosion process of pure magnesium in simulated body fluid10.1016/j.matlet.2007.11.045 ↗
15. Biodegradation kinetics of modified magnesium-based materials in cell culture medium10.1016/j.corsci.2011.01.014 ↗
16. Chemical surface alteration of biodegradable magnesium exposed to corrosion media10.1016/j.actbio.2011.03.004 ↗
17. Influence of chloride, sulfate and bicarbonate anions on the corrosion behavior of AZ31 magnesium alloy10.1016/j.jallcom.2010.02.088 ↗
18. Influence of aggressive ions on the degradation behavior of biomedical magnesium alloy in physiological environment10.1016/j.actbio.2008.05.014 ↗
19. Anodic behavior of Mg in HCO3-/CO32- buffer solution. Quasi-steady measurements10.1016/0013-4686(92)87014-Q ↗
20. Effect of inorganic salts, amino acids and proteins on the degradation of pure magnesium in vitro10.1016/j.msec.2008.12.015 ↗
21. Electrochemical behavior of AZ91D magnesium alloy in phosphate medium – part I. Effect of pH10.1007/s10800-008-9696-y ↗
22. Gamble · 1967
23. Anion-exchange properties of hydrotalcite-like compounds10.1346/CCMN.1983.0310409 ↗
24. First principles study of the structure and chemistry of Mg-based hydrotalcite-like anionic clays10.1021/jp026339k ↗
25. Characterization of Mg, Al-hydrotalcite conversion film on Mg alloy and Cl− and CO32- anion-exchangeability of the film in a corrosive environment10.1016/j.scriptamat.2007.02.020 ↗
26. Study of the corrosion mechanism of the in situ grown Mg–Al–CO32- hydrotalcite film on AZ31 alloy10.1016/j.corsci.2012.08.026 ↗
27. A reexamination of hydrotalcite crystal chemistry10.1021/jp960039j ↗
28. Hydrotalcite decomposition mechanism: a clue to the structure and reactivity of spinel-like mixed oxides10.1021/jp960040i ↗
29. The influence of carbon dioxide on the atmospheric corrosion of some magnesium alloys in the presence of NaCl10.1149/1.1452115 ↗
30. In situ growth of Mg–Al hydrotalcite conversion film on AZ31 magnesium alloy10.1016/j.corsci.2011.06.003 ↗
31. Study of the in situ growth mechanism of Mg–Al hydrotalcite conversion film on AZ31 magnesium alloy10.1016/j.corsci.2012.05.022 ↗
32. Influence of chloride ion concentration and temperature on the corrosion of Mg–Al alloys in salt fog10.1016/j.corsci.2010.01.020 ↗
33. A corrosion study of the main constituent phases of AZ91 magnesium alloys10.1016/S0010-938X(03)00109-4 ↗
34. The corrosion of pure magnesium in aerated and deaerated sodium sulphate solutions10.1016/S0010-938X(00)00095-0 ↗
35. Influence of microstructure and composition on the corrosion behavior of Mg/Al alloys in chloride media10.1016/j.electacta.2008.06.001 ↗
36. Understanding magnesium corrosion; a framework for improved alloy performance10.1002/adem.200310405 ↗
37. A chemical conversion hydroxyapatite coating on AZ60 magnesium alloy and its electrochemical corrosion behaviour10.1016/S1452-3981(23)16961-6 ↗
38. The influence of NaCl and CO2 on the atmospheric corrosion of magnesium alloy AZ9110.1002/maco.200390130 ↗
39. Corrosion of magnesium in humid air10.1016/j.corsci.2003.09.010 ↗
40. Biomimetic calcium phosphate coating on Ti6Al4V: a crystal growth study of octacalcium phosphate and inhibition by Mg2+ and HCO3-10.1016/S8756-3282(99)00145-3 ↗
41. Molecular mechanisms of dental enamel formation10.1177/10454411950060020701 ↗
42. Microstructure of hydroxyapatite- and octacalcium phosphate-coatings formed on magnesium by a hydrothermal treatment at various pH values10.1016/j.actamat.2010.09.041 ↗
43. Bone-like matrix formation on magnesium and magnesium alloys10.1007/s10856-007-3172-9 ↗
44. Biological performance of uncoated and octacalcium phosphate-coated Ti6Al4V10.1016/j.biomaterials.2004.02.026 ↗
45. Biomimetic calcium phosphate coating on Ti wires versus flat substrates: structure and mechanism of formation10.1007/s10856-009-3906-y ↗
46. Calcium phosphate coatings on magnesium alloys for biomedical applications: a review10.1016/j.actbio.2011.10.016 ↗
47. Precipitation of magnesium apaptite on pure magnesium surface during immersing in Hank’s solution10.2320/matertrans.42.1317 ↗