Abstract

This study evaluated the effect of solvent polarity on the photostability of teak extractives and their potential application in wood protection. Using the Soxhlet extraction method, three teak extractives – labeled as petroleum ether extractives (PeE), absolute ethanol extractives (EtE) and hot water extractives (HWE) – were prepared and applied as natural coatings to the surface of Chinese fir (Cunninghamia lanceolata (Lamb.) Hook.). The effect of solvent polarity on the ultraviolet (UV) resistance of teak extractives was evaluated by comparing the surface color, gloss, and chemical changes on fir samples treated with three extractives during UV exposure. UV-accelerated weathering tests demonstrated that the EtE-treated coating exhibited optimal photostability, showing the smallest total color change among the three coatings. In contrast, PeE-coated surfaces exhibited declining gloss during UV exposure, whereas both EtE and HWE coatings showed increasing trends. Although compositional differences led to distinct chemical evolution pathways during UV exposure, all three extractive-based coatings effectively inhibited lignin photodegradation in Chinese fir wood. This study compared the photostability of teak extractive coatings prepared with different solvents, establishing a solvent selection framework and providing mechanistic insights for subsequent research on plant-derived wood coatings.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Wood Treatment and Properties · Cultural Heritage Materials Analysis · Wood and Agarwood Research

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Beihua University

Northeast Forestry University

Kyushu University

Funding

Beihua University

References (70)

Show source-provided references
1. 10.1016/j.apsusc.2006.08.02910.1016/j.apsusc.2006.08.029 ↗
2. Anderson, E.L., et al., 1991. Infrared studies of wood weathering. Part I: softwoods. Applied Spectroscopy, 45 (4), 641–647.10.1366/0003702914336930 ↗
3. 10.1080/17480272.2022.205358610.1080/17480272.2022.2053586 ↗
4. 10.1016/j.polymdegradstab.2020.10941510.1016/j.polymdegradstab.2020.109415 ↗
5. 10.1520/G0154-2310.1520/G0154-23 ↗
6. 10.1007/s00107-011-0551-110.1007/s00107-011-0551-1 ↗
7. 10.4067/S0718-221X201600500002510.4067/S0718-221X2016005000025 ↗
8. 10.1016/j.jclepro.2016.11.07410.1016/j.jclepro.2016.11.074 ↗
9. 10.1007/s00226-018-0996-z10.1007/s00226-018-0996-z ↗
10. 10.1007/s00226-019-01084-110.1007/s00226-019-01084-1 ↗
11. 10.3390/polym1323408510.3390/polym13234085 ↗
12. 10.1016/j.polymdegradstab.2010.06.01210.1016/j.polymdegradstab.2010.06.012 ↗
13. 10.1016/j.polymdegradstab.2014.03.03610.1016/j.polymdegradstab.2014.03.036 ↗
14. 10.12326/j.2096-9694.202104610.12326/j.2096-9694.2021046 ↗
15. 10.1016/j.jphotobiol.2016.02.03010.1016/j.jphotobiol.2016.02.030 ↗
16. 10.1016/S0141-3910(03)00051-X10.1016/S0141-3910(03)00051-X ↗
17. 10.1016/S0040-4020(97)00460-210.1016/S0040-4020(97)00460-2 ↗
18. 10.1007/BF0260840410.1007/BF02608404 ↗
19. 10.1016/j.trac.2009.03.01010.1016/j.trac.2009.03.010 ↗
20. 10.1007/BF0024443710.1007/BF00244437 ↗
21. 10.3964/j.issn.1000-0593(2022)01-0056-0610.3964/j.issn.1000-0593(2022)01-0056-06 ↗
22. 10.3390/f1510178210.3390/f15101782 ↗
23. 10.1155/2022/634933210.1155/2022/6349332 ↗
24. 10.1002/jms.437910.1002/jms.4379 ↗
25. 10.1002/pol.1975.17013060710.1002/pol.1975.170130607 ↗
26. Hon, D.N.-S., Ifju, G., and Feist, W.C., 1980. Characteristics of free radicals in wood. Wood and Fiber Science, 12 (2), 121–130.
27. 10.1007/s00107-020-01603-z10.1007/s00107-020-01603-z ↗
28. 10.1007/s10086-008-1024-y10.1007/s10086-008-1024-y ↗
29. 10.3390/coatings1009087710.3390/coatings10090877 ↗
30. 10.1007/s13595-014-0428-710.1007/s13595-014-0428-7 ↗
31. Kirker, G.T., et al., 2013. Transferable durability: enhancing decay resistance of non-durable species with extractives from durable wood species. Section 1 Biology, 1–12. https://research.fs.usda.gov/treesearch/43782.
32. 10.1080/0277381000934963810.1080/02773810009349638 ↗
33. 10.1021/acssuschemeng.3c0081110.1021/acssuschemeng.3c00811 ↗
34. 10.15376/biores.12.3.4500-451410.15376/biores.12.3.4500-4514 ↗
35. Li, H., et al., 2019. Study of the discoloration behaviour of teak wood (Tectona grandis Linn. fil.) caused by simulated sunlight. Wood Research, 64 (4), 625–636.
36. 10.3390/polym1104070910.3390/polym11040709 ↗
37. 10.1155/2018/182916010.1155/2018/1829160 ↗
38. 10.51850/wrj.2021.12.1.10-1710.51850/wrj.2021.12.1.10-17 ↗
39. 10.3390/ijms23241573510.3390/ijms232415735 ↗
40. 10.1016/j.porgcoat.2023.10742810.1016/j.porgcoat.2023.107428 ↗
41. 10.1016/j.conbuildmat.2023.13192310.1016/j.conbuildmat.2023.131923 ↗
42. 10.1021/acssuschemeng.1c0541510.1021/acssuschemeng.1c05415 ↗
43. 10.1016/S1011-1344(02)00412-810.1016/S1011-1344(02)00412-8 ↗
44. 10.1002/col.2024810.1002/col.20248 ↗
45. 10.1038/s41598-023-41494-710.1038/s41598-023-41494-7 ↗
46. 10.1155/2015/63183510.1155/2015/631835 ↗
47. 10.12841/wood.1644-3985.373.0910.12841/wood.1644-3985.373.09 ↗
48. 10.1002/(SICI)1097-4628(19990321)71:12<1969::AID-APP6>3.0.CO;2-D10.1002/(SICI)1097-4628(19990321)71:12<1969::AID-APP6>3.0.CO;2-D ↗
49. 10.1016/j.polymdegradstab.2004.09.00710.1016/j.polymdegradstab.2004.09.007 ↗
50. 10.1016/j.polymdegradstab.2005.02.00910.1016/j.polymdegradstab.2005.02.009 ↗
51. 10.1016/j.porgcoat.2020.10566510.1016/j.porgcoat.2020.105665 ↗
52. 10.1016/j.indcrop.2021.11360610.1016/j.indcrop.2021.113606 ↗
53. 10.1007/s00107-023-02034-210.1007/s00107-023-02034-2 ↗
54. 10.1021/ba-1984-0207.ch00210.1021/ba-1984-0207.ch002 ↗
55. 10.4067/S0718-221X201700500001210.4067/S0718-221X2017005000012 ↗
56. 10.13360/j.issn.2096-1359.20190704110.13360/j.issn.2096-1359.201907041 ↗
57. 10.1007/s00107-017-1228-110.1007/s00107-017-1228-1 ↗
58. Salgado L.C. 2021. Study of the valorization of teak (Tectona grandis) by-product from a sawmill by a continuous process under subcritical water. PhD thesis. Institut National Polytechnique de Toulouse – INPT. https://theses.hal.science/tel-04171178
59. 10.1016/j.polymdegradstab.2012.01.01310.1016/j.polymdegradstab.2012.01.013 ↗
60. 10.1016/j.microc.2024.11078810.1016/j.microc.2024.110788 ↗
61. 10.1016/j.apsusc.2006.12.00510.1016/j.apsusc.2006.12.005 ↗
62. 10.1007/s00107-006-0127-710.1007/s00107-006-0127-7 ↗
63. 10.1007/s00226-015-0771-310.1007/s00226-015-0771-3 ↗
64. 10.1016/j.measurement.2018.05.10210.1016/j.measurement.2018.05.102 ↗
65. 10.1007/s10311-020-01067-w10.1007/s10311-020-01067-w ↗
66. 10.1007/s00107-003-0425-210.1007/s00107-003-0425-2 ↗
67. 10.5152/forestist.2018.00710.5152/forestist.2018.007 ↗
68. 10.3390/molecules2509218910.3390/molecules25092189 ↗
69. 10.3969/j.issn.0253-2417.2018.05.01110.3969/j.issn.0253-2417.2018.05.011 ↗
70. 10.1016/j.jclepro.2020.12477010.1016/j.jclepro.2020.124770 ↗