journal article·2017-01Open access

Wood defects during industrial-scale production of thermally modified Norway spruce and Scots pine

Michael Altgen, Stergios Adamopoulos, Holger Militz

Abstract

This research investigates wood defects, particularly the formation of surface cracks, during the production of thermally modified wood and its exposure to cyclic moisture changes. Boards of Norway spruce and Scots pine originating from different steps within the production of ThermoWood® were collected and wood defects were investigated at macroscopic and microscopic scale. Subsequently, the wood was exposed to capillary wetting cycles to record its sensitivity towards cracking. After the modification process, typical anatomical defects of conventional kiln-drying became more frequent and severe, with the magnitude being to some extent depending on the presence of defects in the raw material. At microscopic scale, damages to ray parenchyma and epithelial cells as well as longitudinal cracks within the cell walls of earlywood tracheids were evident in thermally modified wood. Despite a lower water uptake and higher dimensional stability, thermally modified wood was more sensitive to surface cracking during wetting cycles than unmodified wood, i.e. at the outside face of outer boards (near bark). For limiting surface cracking of thermally modified wood during service life, the use of high-quality raw material, the exposure of the inside face of the boards (near pith) and the application of a surface coating are considered beneficial.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Wood Treatment and Properties · Lignin and Wood Chemistry · Tree Root and Stability Studies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (33)

Show source-provided references
1. 10.1007/s00226-010-0315-910.1007/s00226-010-0315-9 ↗
2. Boonstra M. · Maderas Ciencia i tecnología · 2006 · 8 · 193
3. Boonstra M. · Maderas Ciencia i tecnología · 2006 · 8 · 209
4. 10.1080/1748027080194543910.1080/17480270801945439 ↗
5. 10.1051/forest:200704810.1051/forest:2007048 ↗
6. 10.1007/978-90-481-9550-310.1007/978-90-481-9550-3 ↗
7. Chang S. T. · Wood and Fiber Science · 1982 · 14 · 104
8. Eaton R. A. · 1993
9. 10.1007/s00107005040410.1007/s001070050404 ↗
10. Forest Products Laboratory. (1957) Shrinking and Swelling of Wood in Use (Madison, WI: United States Department of Agriculture, Forest Service, Forest Products Laboratory), Report No. 736, 19 pp.
11. 10.1016/j.polymdegradstab.2005.04.04210.1016/j.polymdegradstab.2005.04.042 ↗
12. 10.1515/HF.2003.08310.1515/HF.2003.083 ↗
13. ISO 4628-4 · Paints and Varnishes – Evaluation of Degradation of Coatings – Designation of Quantity and Size of Defects, and of Intensity of Changes – Part 4: Assessement of Degree of Cracking · 1982
14. 10.1108/0369942001031780710.1108/03699420010317807 ↗
15. 10.1007/s00107-001-0261-110.1007/s00107-001-0261-1 ↗
16. 10.1016/j.biortech.2007.03.03810.1016/j.biortech.2007.03.038 ↗
17. 10.1007/BF0077954710.1007/BF00779547 ↗
18. Lamb F. M. · 1992
19. 10.1007/s00226-010-0389-410.1007/s00226-010-0389-4 ↗
20. Mayes D. · 2003
21. 10.1007/s00107-005-0063-y10.1007/s00107-005-0063-y ↗
22. Morén, T. (1993) Creep, deformation and moisture redistribution during air convective wood drying and conditioning: air convective wood drying and conditioning. Ph.D. thesis, Luleå University of Technology.
23. 10.1007/s00107-004-0554-210.1007/s00107-004-0554-2 ↗
24. 10.1007/s00107005015610.1007/s001070050156 ↗
25. 10.1007/BF0299054110.1007/BF02990541 ↗
26. 10.1080/1748027060064440710.1080/17480270600644407 ↗
27. Schniewind A. P. · Forest Products Journal · 1963 · 13 · 475
28. Syrjänen, T. and Kangas, E. (2000) Heat Treated Timber in Finland. Document No. IRG/WP 00-40158 (Kona, HI: International Research Group on Wood Protection).
29. 10.1007/s00107005028710.1007/s001070050287 ↗
30. Tsoumis G. T. · 2009
31. Ward J. C. · Dry Kiln Operator's Manual USDA Agriculture Handbook AH-188 · 2001 · 179
32. Welzbacher, C. and Rapp, A. (2002) Comparison of Thermally Modified Wood Originating from Four Industrial Scale Processes – Durability. Document No. IRG/WP 02-40229 (Cardiff: International Research Group on Wood Protection).
33. Yildiz, S. (2002) Effects of Heat Treatment on Water Repellence and Anti Swelling Efficiency of Beech Wood. Document No. IRG/WP 02-40223 (Cardiff: International Research Group on Wood Protection).