Superheated steam treatment of rubberwood to enhance its mechanical, physiochemical, and biological properties
Source abstract
Abstract
This research was aimed to investigate mechanical properties, color and cell-wall components changes, and durability of pre-dried rubberwood (Hevea brasiliensis) after superheated steam (SS) treatment. Wood samples were treated at different SS temperatures (140–180°C) for 1–3 h. The highest compression strength parallel-to-grain, hardness and impact strength were found for samples treated at 160°C for 3 h (30.7% higher than untreated), at 150°C for 1 h (26.6% higher than untreated) and at 150°C for 2 h (52.6% higher than untreated), respectively. The surface color became darker after each treatment in comparison with the untreated wood. The number of accessible hydroxyl groups decreased and the relative cellulose crystallinity increased with SS temperature, indicating decreased hygroscopicity of the treated wood. Also, SEM micrographs of wood surface showed consistent decrease in starch particles with treatment temperature. Both decay and termite resistances of treated rubberwood improved with treatment temperature. All the analyzes showed that dried rubberwood treated with SS had some improvements in the mechanical properties, decreased hygroscopicity, and increase resistance to decay.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Wood Treatment and Properties · Natural Fiber Reinforced Composites · Lignin and Wood Chemistry
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Department of Chemical Engineering, Faculty of Engineering, Prince of Songkla University, Hat Yai, Thailand
References (30)
Show source-provided references
1. 10.1007/s00226-006-0110-910.1007/s00226-006-0110-9 ↗
2. ASTM D143 · 2000
3. ASTM D-1413 (2007) Standard Test Method for Wood Preservatives by Laboratory Soil-Block Cultures. American Society for Testing and Materials, USA.
4. ASTM D3345-08 (1999) Standard Test Method for Laboratory Evaluation of Wood and Other Cellulosic Materials for Resistance to Termites. American Society for Testing and Materials, USA.
5. Ates S. · BioResources · 2009 · 4 · 103210.15376/biores.4.3.1032-1043 ↗
6. Aydemir D. · BioResources · 2011 · 6 · 130810.15376/biores.6.2.1308-1321 ↗
7. 10.1016/j.biortech.2008.03.06910.1016/j.biortech.2008.03.069 ↗
8. 10.1016/j.biortech.2010.06.11910.1016/j.biortech.2010.06.119 ↗
9. 10.26525/jtfs2018.30.3.38439210.26525/jtfs2018.30.3.384392 ↗
10. 10.1080/17480272.2013.85369210.1080/17480272.2013.853692 ↗
11. Esteves B. · Maderas. Ciencia y tecnología · 2013 · 15 · 245
12. Fabiyi J.S. · Maderas. Ciencia y tecnología · 2015 · 17 · 5
13. Gawron J. · Wood Research · 2011 · 56 · 213
14. 10.1080/0737393090353016210.1080/07373930903530162 ↗
15. 10.1590/0104776020162201210110.1590/01047760201622012101 ↗
16. ISO 3350 (1975) Wood-Determination of Static Hardness.
17. ISO 3787 (1976) Wood Tests Methods – Determination of Ultimate Stress in Compression Parallel to Grain.
18. 10.1016/j.biortech.2013.06.11010.1016/j.biortech.2013.06.110 ↗
19. 10.1080/17480272.2013.86925610.1080/17480272.2013.869256 ↗
20. 10.3390/ma510191010.3390/ma5101910 ↗
21. 10.15376/biores.10.1.1198-121210.15376/biores.10.1.1198-1212 ↗
22. 10.1080/1748027090332614010.1080/17480270903326140 ↗
23. Patcharawijit A. · Drying Technology
24. Percin O. · Wood Research · 2016 · 61 · 443
25. Schneid E. · Maderas. Ciencia y Tecnología · 2014 · 16 · 413
26. Sik H. · Journal of Tropical Forest Science · 2009 · 21 · 181
27. 10.5539/jas.v2n1p4810.5539/jas.v2n1p48 ↗
28. 10.1007/s10086-011-1173-210.1007/s10086-011-1173-2 ↗
29. Umar I. · Journal of Tropical Forest Science · 2016 · 28 · 88
30. 10.1080/07373937.2011.57480510.1080/07373937.2011.574805 ↗