Geometric changes of TMP fibres due to thermo-hydrolytic disintegration of waste MDF evaluated by three fibre analysers
Source abstract
Abstract
Thermo-hydrolytic disintegration of medium-density fibreboard (MDF) is a promising method for recovering fibres. This process, however, may affect the geometry and size distribution of the applied fibres initially obtained by thermomechanical pulping (TMP), and thus, the properties of MDF produced thereof. Optical methods based on image acquisition are increasingly common for geometrical characterisation to assess fibre quality. In this study, we analysed the size distribution of recovered fibres (RF) obtained by thermo-hydrolytic disintegration of urea–formaldehyde-bonded waste MDF and subsequent hammer-milling by using three optical fibre analysers, FibreShape Pro, QICPIC and Valmet FS5, while comparing them to virgin fibres (VF). The analysers use different evaluation methods and therefore gave different absolute values. Thus, size distributions could not be directly compared. Nevertheless, the results provided an indication of the changes that occurred during the manufacturing and recycling process. The RF displayed a similar fibre geometry to the VF, in spite of process-related shortening. Mean fibre length and length-based distribution of the VF were always greater than those of the RF, while fibre width of the hammer-milled RF was slightly greater than that of the VF. The analysers, however, provided substantially different results, especially between FibreShape Pro and QICPIC, although the general tendencies observed for the process-related changes were consistent. It can be concluded that the thermo-hydrolytic disintegration applied to the UF-bonded MDF did not cause any substantial changes in fibre geometry (i.e. fibre shortening). All fibre analysers are capable of detecting these changes, but the absolute values provided can vary widely between the instruments.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Natural Fiber Reinforced Composites · Fiber-reinforced polymer composites · Recycling and Waste Management Techniques
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
University of Goettingen
Linnaeus University
Swedish University of Agricultural Sciences
Fraunhofer-Institut für Holzforschung WKI
References (52)
Show source-provided references
1. Beele P.M. 2009. Demonstration of end uses for recovered MDF fibre. WRAP (Waste and Resources Action Programme) (Final report No. MDD005). Banbury UK.
2. Benthien, J.T., et al., 2014. Effect of fiber size distribution on medium-density fiberboard properties caused by varied steaming time and temperature of defibration process. Wood and Fiber Science, 46, 175–185.
3. 10.1007/s00107-016-1094-210.1007/s00107-016-1094-2 ↗
4. 10.1007/s00107-021-01739-610.1007/s00107-021-01739-6 ↗
5. 10.21926/rpm.210302910.21926/rpm.2103029 ↗
6. 10.3923/jas.2007.1043.104710.3923/jas.2007.1043.1047 ↗
7. 10.1007/s00107010021010.1007/s001070100210 ↗
8. 10.1007/s00107010021110.1007/s001070100211 ↗
9. FAO 2019. Global forest products facts and figures 2018. Rome: FAO – Food and Agriculture Organization of the United Nations.
10. FAO 2020. FAOSTAT – forestry production and trade [WWW Document]. http://www.fao.org/faostat/en/#data/FO (accessed 9.17.20).
11. Groom L. Mott L. and Shaler S. 1999. Relationship between fiber furnish properties and structural performance of MDF. 33rd International Particleboard/Composite Material Symposium 1999 13–15 April 1999 Pullman Washington USA.
12. Guay D. et al. 2005. Comparison of fiber length analyzers. In: Proceedings of 2005 TAPPI Practical Papermaking Conference. Tappi Press pp. 30–38.
13. Gusovius H.J. et al. 2006. New quantitative image analysis method for the characterization of mineral and fibrous materials. XXIII International Mining Processing Congress. Presented at the XXIII International Mining Processing Congress Istanbul Turkey.
14. 10.1007/s12649-021-01391-410.1007/s12649-021-01391-4 ↗
15. Hirn, U., and Bauer, W., 2006. A review of image analysis based methods to evaluate fiber properties. Lenzing Berichte, 86, 96–105.
16. 10.1007/s00107-021-01698-y10.1007/s00107-021-01698-y ↗
17. 10.1080/17480272.2018.142714410.1080/17480272.2018.1427144 ↗
18. ISO 13322-1 2014. Particle size analysis – image analysis methods – part 1: static image analysis methods.
19. ISO 13322-2 2014. Particle size analysis – image analysis methods – part 2: dynamic image analysis methods.
20. ISO 9276-1 2004. Representation of results of particle size analysis – part 1: graphical representation.
21. ISO 9276-6 2008. Representation of results of particle size analysis – part 6: descriptive and quantitative representation of particle shape and morphology.
22. Kearley V. and Goroyias G. 2004. Wood panel recycling at a semi-industrial scale. In: Proceedings of the 8th European Panel Products Symposium Llandudno Wales UK 1–18.
23. 10.1016/j.compositesa.2011.07.01210.1016/j.compositesa.2011.07.012 ↗
24. Liiri, O., Kivisto, A., and Saarinen, A., 1977. Einfluss von Holzart, Spangröße und Bindemittel auf die Festigkeit und die Quellung von Spanplatten mit höheren elastomechanischen Eigenschaften. Holzforschung und Holzverwertung, 29, 117–122.
25. 10.1080/02773813.2017.131674110.1080/02773813.2017.1316741 ↗
26. 10.1016/j.wasman.2006.11.01610.1016/j.wasman.2006.11.016 ↗
27. Michanickl A. and Boehme C. 2003. Method for recovering chips and fibers of bonded wood materials involves passing of steam through a vessel with such materials which have been soaked with a heated impregnation solution. European Union Patent No: DE10144793 WO03026859. DE10144793 WO03026859.
28. Mitchell A. and Stevens G. 2009. Life cycle assessment of closed loop MDF recycling: Microrelease trial (No. GR185). WRAP – Waste and Resources Action Programme Banbury UK.
29. 10.1007/s00107-018-1291-210.1007/s00107-018-1291-2 ↗
30. 10.1017/S143192760488432010.1017/S1431927604884320 ↗
31. Nakos P. Athanassiadou E. and Coutinho J.M.A. 2005. Production of high added value products from resin-bonded waste composite wood products. United States Patent No: US6841101B2. US6841101B2.
32. New A.J. 2012. Recycling technology. European Union Patent No: EP2516730A1. EP2516730A1.
33. 10.1007/s00107-023-01937-410.1007/s00107-023-01937-4 ↗
34. Ohlmeyer M. et al. 2015. Effects of refining parameters on fibre quality measured by fibre cube. In: Proceedings of the International Panel Products Symposium. Biocomposites Centre Bangor 17–25.
35. 10.3183/npprj-2016-31-04-p548-56010.3183/npprj-2016-31-04-p548-560 ↗
36. Plinke, B., et al., 2016. Optische Größenvermessung von Holzpartikeln für die WPC-Herstellung – Vergleich dreier Messverfahren (Optical measurement of wood particles for WPC – comparison of three methods). Holztechnologie, 57, 43–50.
37. Plinke, B., Schirp, A., and Weidenmüller, I., 2012. Review: Methoden der Holzpartikelgrößenmessung – Von der technologischen Fragestellung zur aussagefähigen Statistik (Methods of wood particle size measurements - From the technical questions to informative statistics). Holztechnologie, 53, 11–17.
38. Riddiough S. 2002. Wood panel recycling: an introduction to the fibersolve process. In: Proceedings of the 6th Panel Products Symposium. Llandudno Wales UK 159–166.
39. 10.1007/s00107-009-0376-310.1007/s00107-009-0376-3 ↗
40. Rowell, R.M., et al., 1993. Opportunities for composites from recycled waste wood-based resources: a problem analysis and research plan. Forest Product Journal, 43, 55–63.
41. Sandison M. 2002. Method for the recovery of wood fiber from compressed fiberboard scrap US6413364 United States Patent No: US6413364B1.
42. 10.3390/fib1107006410.3390/fib11070064 ↗
43. 10.1016/j.compositesa.2014.03.00310.1016/j.compositesa.2014.03.003 ↗
44. Schmid H.G. and Schmid G.P. 2006. Characterisation of high aspect ratio objects using the powdershape quantitative image analysis system. Presented at the European Congress and Exhibition on Powder Metallurgy (EURO PM) Ghent Belgium 2006.
45. 10.1007/s00107005045510.1007/s001070050455 ↗
46. 10.1007/978-981-10-0234-2_210.1007/978-981-10-0234-2_2 ↗
47. 10.1007/s10570-020-03226-210.1007/s10570-020-03226-2 ↗
48. Teuber L. 2016. Evaluation of particle and fibre degradation during processing of wood plastic composites (WPC) using dynamic image analysis. PhD thesis at Georg-August University of Goettingen Goettingen.
49. 10.1016/j.compositesa.2016.02.02810.1016/j.compositesa.2016.02.028 ↗
50. 10.15376/biores.9.4.7554-756510.15376/biores.9.4.7554-7565 ↗
51. Witt W. Köhler U. and List J. 2004. Direct imaging of very fast particles opens the application of the powerful (dry) dispersion for size and shape characterization. Sympatec GmbH System-Partikel-Technik Clausthal-Zellerfeld Germany.
52. Witt W. Köhler U. and List J. 2007. Current limits of particle size and shape analysis with high speed image analysis. PARTEC2007.