Osteogenic and pH stimuli-responsive self-healing coating on biomedical Mg-1Ca alloy
Source abstract
Abstract
Various coatings have been used to slow down the corrosion rate of biomedical magnesium alloys. However, these coatings usually act only as passive barriers. It is much more desirable to endow such coatings with active, biocorrosion-responsive self-repairing capacity. In the present work, a self-healing coating system (denoted as "silk-PA") was constructed in the form of a sandwich architecture of fluoride precoating (bottom), silk-phytic acid (PA) coating (middle), and silk fibroin coating (top). Here, PA was loaded in the middle coating as a corrosion inhibitor by harnessing its strong chelating ability toward dissolving Mg2+ and Ca2+ ions. The self-healing property was evaluated by scratch and SVET tests, and the corrosion resistance was evaluated by in vitro immersion and electrochemical measurements. The results showed that the silk-PA manifested intriguing self-healing capacity with pH responsiveness, hence profiting the corrosion resistance of the Mg-1Ca alloy. The biocompatibility and osteogenic activity of the coating system were further evaluated using MC3T3-E1 cells, and it demonstrated favorable responses in multiple cellular behaviors, i.e., adherence, spreading, proliferation, and differentiation. These findings open new opportunities in the study of self-healing coatings for protection against corrosion in biomedical Mg alloys. STATEMENT OF SIGNIFICANCE: In the present study, a self-healing coating system with pH stimuli-responsiveness and osteogenic activity was fabricated on Mg-1Ca alloy by integrating a silk fibroin barrier coating, a silk fibrin/phytic acid composite coating, and a fluoride precoating. This coating system demonstrated interesting self-healing ability as compared to traditional surface modification layers. Furthermore, the self-healing ability enhanced the corrosion resistance of biomedical magnesium alloys, while effective compositions of the coating system endowed the substrate with osteogenic activity. This work provides some new insights into smart surface modification for biomedical Mg alloys.
Source: europepmc · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Magnesium Alloys: Properties and Applications · Bone Tissue Engineering Materials · Aluminum Alloys Composites Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (63)
Show source-provided references
1. Current status on clinical applications of magnesium-based orthopaedic implants: a review from clinical translational perspective10.1016/j.biomaterials.2016.10.017 ↗
2. Magnesium biomaterials: past, present and future10.1179/1743278212Y.0000000034 ↗
3. In vitro studies of biomedical magnesium alloys in a simulated physiological environment: a review10.1016/j.actbio.2010.12.004 ↗
4. In vitro and in vivo corrosion measurements of magnesium alloys10.1016/j.biomaterials.2005.07.037 ↗
5. Reprint of: the history of biodegradable magnesium implants: a review10.1016/j.actbio.2015.07.017 ↗
6. Potentiostatic deposition process of fluoride conversion film on AZ31 magnesium alloy in 0.1M KF solution10.1016/j.electacta.2013.04.161 ↗
7. In vivo comparative property study of the bioactivity of coated Mg-3Zn-0.8Zr alloy10.1016/j.msec.2013.04.006 ↗
8. Corrosion resistance of a composite polymeric coating applied on biodegradable AZ31 magnesium alloy10.1016/j.actbio.2013.02.036 ↗
9. A surface-eroding poly(1,3-trimethylene carbonate) coating for fully biodegradable magnesium-based stent applications: toward better biofunction, biodegradation and biocompatibility10.1016/j.actbio.2013.02.041 ↗
10. The effects of pulse electrodeposition parameters on morphology and formation of dual-layer Si-doped calcium phosphate coating on AZ31 alloy10.1016/j.ceramint.2014.09.003 ↗
11. In vitro and in vivo biocompatibility and corrosion behaviour of a bioabsorbable magnesium alloy coated with octacalcium phosphate and hydroxyapatite10.1016/j.actbio.2014.09.026 ↗
12. Micro-arc oxidization of a novel Mg–1Ca alloy in three alkaline KF electrolytes: corrosion resistance and cytotoxicity10.1016/j.apsusc.2013.11.038 ↗
13. Structure and properties of compound coatings on Mg alloys by micro-arc oxidation/hydrothermal treatment10.1016/j.jallcom.2015.02.008 ↗
14. A layer-by-layer approach to natural polymer-derived bioactive coatings on magnesium alloys10.1016/j.actbio.2013.05.013 ↗
15. Nanocontainer-enhanced self-healing for corrosion-resistant Ni coating on Mg alloy10.1021/acsami.7b12036 ↗
16. Influence of functionalization of nanocontainers on self-healing anticorrosive coatings10.1021/acsami.5b08028 ↗
17. Influence of embedded nanocontainers on the efficiency of active anticorrosive coatings for aluminum alloys part II: influence of nanocontainer position10.1021/am302141y ↗
18. Regenerative nano-hybrid coating tailored for autonomous corrosion protection10.1002/adma.201501044 ↗
19. Developments in smart anticorrosive coatings with multifunctional characteristics10.1016/j.porgcoat.2017.06.013 ↗
20. Monodisperse polymeric core-shell nanocontainers for organic self-healing anticorrosion coatings10.1002/admi.201300019 ↗
21. Acid and alkaline dual stimuli-responsive mechanized hollow mesoporous silica nanoparticles as smart nanocontainers for intelligent anticorrosion coatings10.1021/nn4053233 ↗
22. A critical appraisal of the potential of self healing polymeric coatings10.1016/j.porgcoat.2011.06.016 ↗
23. Self-healing anticorrosion coatings based on pH-sensitive polyelectrolyte/inhibitor sandwichlike nanostructures10.1002/adma.200800705 ↗
24. Self-healing plasma electrolytic oxidation coatings doped with benzotriazole loaded halloysite nanotubes on AM50 magnesium alloy10.1016/j.corsci.2016.06.016 ↗
25. Layer-by-layer assembly of a self-healing anticorrosion coating on magnesium alloys10.1021/acsami.5b08577 ↗
26. Inhibitor encapsulated, self-healable and cytocompatible chitosan multilayer coating on biodegradable Mg alloy: a pH-responsive design10.1039/C6TB00117C ↗
27. Localized corrosion of the Mg alloys with inhibitor-containing coatings: SVET and SIET studies10.1016/j.corsci.2015.10.015 ↗
28. Silica mesoporous thin films as containers for benzotriazole for corrosion protection of 2024 aluminium alloys10.1016/j.apsusc.2015.03.191 ↗
29. Self-healing property of hydroxyapatite and octacalcium phosphate coatings on pure magnesium and magnesium alloy10.1016/j.corsci.2015.08.001 ↗
30. Corrosion resistance and antibacterial properties of polysiloxane modified layer-by-layer assembled self-healing coating on magnesium alloy10.1016/j.jcis.2018.04.071 ↗
31. Osteogenic signaling on silk-based matrices10.1016/j.biomaterials.2016.04.020 ↗
32. Structures, mechanical properties and applications of silk fibroin materials10.1016/j.progpolymsci.2015.02.001 ↗
33. Silk proteins for biomedical applications: bioengineering perspectives10.1016/j.progpolymsci.2013.09.002 ↗
34. In vivo bioresponses to silk proteins10.1016/j.biomaterials.2015.08.039 ↗
35. Silk as a potential candidate for bone tissue engineering10.1016/j.jconrel.2015.07.031 ↗
36. Controlling silk fibroin particle features for drug delivery10.1016/j.biomaterials.2010.02.024 ↗
37. Review physical and chemical aspects of stabilization of compounds in silk10.1002/bip.22026 ↗
38. Effect of PLLA coating on corrosion and biocompatibility of zinc in vascular environment10.1680/jsuin.17.00011 ↗
39. Silk as a biocohesive sacrificial binder in the fabrication of hydroxyapatite load bearing scaffolds10.1016/j.biomaterials.2014.05.013 ↗
40. Bioinspired and biomimetic AgNPs/gentamicin-embedded silk fibroin coatings for robust antibacterial and osteogenetic applications10.1021/acsami.7b06757 ↗
41. A silk-based coating containing GREDVY peptide and heparin on Mg–Zn–Y–Nd alloy: improved corrosion resistance, hemocompatibility and endothelialization10.1039/C7TB02784B ↗
42. Microstructure and corrosion resistance of phytic acid conversion coatings for magnesium alloy10.1016/j.apsusc.2008.06.199 ↗
43. In vitro corrosion and biocompatibility study of phytic acid modified WE43 magnesium alloy10.1016/j.apsusc.2011.11.087 ↗
44. Crack self-healing of phytic acid conversion coating on AZ31 magnesium alloy by heat treatment and the corrosion resistance10.1016/j.apsusc.2014.06.104 ↗
45. Corrosion resistance and cytotoxicity of a MgF2coating on biomedical Mg-1Ca alloy via vacuum evaporation deposition method10.1002/sia.5257 ↗
46. Materials fabrication from Bombyx mori silk fibroin10.1038/nprot.2011.379 ↗
47. Synthesis and in vitro degradation evaluation of the nano-HA/MgF2 and DCPD/MgF2 composite coating on biodegradable Mg–Ca–Zn alloy10.1016/j.surfcoat.2013.02.007 ↗
48. Silk fibroin as a novel coating material for controlled release of theophylline
49. Water-insoluble silk films with silk I structure10.1016/j.actbio.2009.10.041 ↗
50. Corrosion resistance and surface biocompatibility of a microarc oxidation coating on a Mg-Ca alloy10.1016/j.actbio.2010.11.034 ↗
51. Development of magnesium-based biodegradable metals with dietary trace element germanium as orthopaedic implant applications10.1016/j.actbio.2017.10.004 ↗
52. Layer-by-layer polyelectrolyte/inhibitor nanostructures for metal corrosion protection10.1021/am1002712 ↗
53. Self-healing and antifouling multifunctional coatings based on pH and sulfide ion sensitive nanocontainers10.1002/adfm.201203180 ↗
54. The effect of polymer morphology on the performance of a corrosion inhibiting polypyrrole/aluminum flake composite pigment10.1016/j.electacta.2013.03.128 ↗
55. Biomedical coatings on magnesium alloys - a review10.1016/j.actbio.2012.04.012 ↗
56. Dual modulation of bone formation and resorption with zoledronic acid-loaded biodegradable magnesium alloy implants improves osteoporotic fracture healing: an in vitro and in vivo study10.1016/j.actbio.2017.10.033 ↗
57. One-step electrodeposition of self-assembled colloidal particles: a novel strategy for biomedical coating10.1021/la5010177 ↗
58. Controlled release and corrosion protection by self-assembled colloidal particles electrodeposited onto magnesium alloys10.1039/C4TB01683A ↗
59. Effect of metallic ions on silk formation in the mulberry silkworm, Bombyx mori10.1021/jp050883m ↗
60. An investigation into the effect of potassium ions on the folding of silk fibroin studied by generalized two-dimensional NMR-NMR correlation and Raman spectroscopy10.1111/j.1742-4658.2007.06191.x ↗
61. Self-healing mechanisms in smart protective coatings: a review10.1016/j.corsci.2018.08.005 ↗
62. Enhanced corrosion resistance of phytic acid coated magnesium by stearic acid treatment10.1016/S1003-6326(13)62588-1 ↗
63. Corrosion resistance of a self-healing micro-arc oxidation/polymethyltrimethoxysilane composite coating on magnesium alloy AZ3110.1016/j.corsci.2017.01.025 ↗