journal article·2013-03

Evaluation of the photo stabilising efficiency of clear coatings comprising organic UV absorbers and mineral UV screeners on wood surfaces

Boris Forsthuber, Christian Schaller, Gerhard Grüll

Wood Science and Technology· Volume 47· Issue 2
Publisher page

Abstract

A study of the surface discolouration of clear coated wood during artificial and outdoor weathering and its prevention using clear coatings comprising organic UV absorbers (UVA) and mineral UV screeners was carried out. It was shown that the use of UVA and UV screeners in clear coatings was very effective in reducing photodegradation of the wood surface. Preliminary irradiation trials with Xenon arc light showed that the UV screener TiO₂ led to the least discolouration of the coated wood surface, closely followed by UVA of the hydroxyphenyl-s-triazine class (HPT). The artificial and outdoor weathering trials indicated that UVA of the HPT class stabilised the colour of the wood surface better than UVA of the 2-(2-hydroxyphenyl)-benzotriazole class (BTZ). Comparison of different artificial weathering methods indicated that Xenon arc light weathering showed the best match to the proceeding discolouration of the clear coated wood panels during outdoor weathering.
Source: europepmc · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Building materials and conservation · Conservation Techniques and Studies · Infrastructure Maintenance and Monitoring

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (34)

Show source-provided references
1. Allen NS, Edge M, Ortega A, Liauw CM, Stratton J, Mc Intyre RB (2002) Behaviour of nanoparticle (ultrafine) titanium dioxide pigments and stabilisers on the photooxidative stability of water based acrylic and isocyanate based acrylic coatings. Polym Degrad Stab 78:467–47810.1016/S0141-3910(02)00189-1 ↗
2. Aloui F, Ahajji A, Irmouli Y, George B, Charrier B, Merlin A (2007) Inorganic UV absorbers for the photostabilisation of wood-clearcoating systems: comparison with organic UV absorbers. Appl Surf Sci 253:3737–374510.1016/j.apsusc.2006.08.029 ↗
3. Andrady AL, Hamid SH, Hu X, Torikai A (1998) Effects of increased solar ultraviolet radiation on materials. J Photochem Photobiol, B 46:96–10310.1016/S1011-1344(98)00188-2 ↗
4. Avar L, Bechtold K (1999) Studies on the interaction of photoreactive light stabilizers and UV-absorbers. Prog Org Coat 35:11–1710.1016/S0300-9440(99)00031-4 ↗
5. Ayadi N, Lejeune F, Charrier F, Charrier B, Merlin A (2003) Color stability of heat-treated wood during artificial weathering. Holz Roh Werkst 61:221–22610.1007/s00107-003-0389-2 ↗
6. Chou PL, Chang JT, Yeh TF, Chang ST (2008) Characterizing the conservation effect of clear coatings on photodegradation of wood. Bioresour Technol 99:1073–107910.1016/j.biortech.2007.02.027 ↗
7. Creemers J, de Meijer M, Zimmermann T, Sell J (2002) Influence of climatic factors on the weathering of coated wood. Holz Roh Werkst 60:411–42010.1007/s00107-002-0338-5 ↗
8. Da Silva Braga M (2005) Schutz von Holz- und TMP-Holzstoff-Oberflächen vor lichtinduzierter Vergilbung durch chemische Modifikation des Lignins. Dissertation, Philipps-Universität Marburg
9. Deka M, Petric M (2008) Photodegradation of water borne acrylic coated modified and non-modified wood during artificial light exposure. Bioresour 2:346–36210.15376/biores.3.2.346-362 ↗
10. Derbyshire H, Miller ER (1981) The photodegradation of wood during solar irradiation.1. Effects on the structural integrity of thin wood strips. Holz Roh Werkst 39:341–35010.1007/BF02608404 ↗
11. Derbyshire H, Miller ER, Turkulin H (1995) Investigations into the photodegradation of wood using microtensile testing 1. The application of microtensile testing to measurement of photodegradation rates. Holz Roh Werkst 53:339–34510.1007/s001070050103 ↗
12. Evans PD, Thay PD, Schmalzl KJ (1996) Degradation of wood surfaces during natural weathering. Effects on lignin and cellulose and on the adhesion of acrylic latex primers. Wood Sci Technol 30:411–42210.1007/BF00244437 ↗
13. Evans PD, Chowdhury MJ, Mathews B, Schmalzl K, Ayer S, Kiguchi M, Yutaka K (2005) Weathering and surface protection of wood. In: Kutz M (ed) Handbook of environmental degradation or materials. William Andrew Publishing, New York, pp 277–29710.1016/B978-081551500-5.50016-1 ↗
14. Fengel D, Wegener G (1989) Wood Chemistry, ultrastructure, reactions. Gruyter, Berlin
15. Forsthuber B, Grüll G (2010) The effects of HALS in the prevention of photodegradation of acrylic clear topcoats and wooden surfaces. Polym Degrad Stab 95:746–75510.1016/j.polymdegradstab.2010.02.016 ↗
16. Heinskill J (1994) Möglichkeiten der UV-Stabilisierung farbloser Holz-Außenanstriche. Farbe und Lack 100:1011–1015
17. Hon DNS, Ifju G (1978) Measuring penetration of light into wood by detection of photoinduced free-radicals. Wood Sci 11:118–127
18. Jacques LFE (2000) Accelerated and outdoor/natural exposure testing of coatings. Prog Polym Sci 25:1337–136210.1016/S0079-6700(00)00030-7 ↗
19. Kamdem DP, Grelier S (2002) Surface roughness and color change of copper-amine treated red maple (acer rubrum) exposed to artificial ultraviolet light. Holzforschung 56:473–47810.1515/HF.2002.073 ↗
20. Kataoka Y, Kiguchi M (2001) Depth profiling of photo-induced degradation in wood by FT-IR microspectroscopy. J Wood Sci 47:325–32710.1007/BF00766722 ↗
21. Kataoka Y, Kiguchi M, Williams RS, Evans PD (2007) Violet light causes photodegradation of wood beyond the zone affected by ultraviolet radiation. Holzforschung 61:23–2710.1515/HF.2007.005 ↗
22. Kuo ML, Hu NH (1991) Ultrastructural-changes of photodegradation of wood surfaces exposed to UV. Holzforschung 45:347–35310.1515/hfsg.1991.45.5.347 ↗
23. Ljuljka B (1971) Der Einfluß von Licht auf lackierte Holzoberflächen. Holz Roh Werkst 29:224–23110.1007/BF02615035 ↗
24. Müller U, Rätzsch M, Schwanninger M, Steiner M, Zöbl H (2003) Yellowing and IR-changes of spruce wood as result of UV-irradiation, J Photochem. Photobiol, B 69:97–10510.1016/S1011-1344(02)00412-8 ↗
25. Oltean L, Teischinger A, Hansmann C (2008) Wood surface discolouration due to simulated indoor sunlight exposure. Holz Roh Werkst 66:51–5610.1007/s00107-007-0201-9 ↗
26. Pospísil J, Nespurek S (2000) Photostabilization of coatings. Mechanisms and performance. Prog Polym Sci 25:1261–133510.1016/S0079-6700(00)00029-0 ↗
27. Schaller C, Rogez D (2007) New approaches in wood coating stabilization. J Coat Technol Res 4(4):401–40910.1007/s11998-007-9049-5 ↗
28. Schaller C, Rogez D, Braig A (2008) Hydroxyphenyl-s-triazines: advanced multipurpose UV-absorbers for coatings. J Coat Technol Res 5:25–3110.1007/s11998-007-9025-0 ↗
29. Schnabel T, Zimmer B, Petutschnigg JA (2009) On the modelling of colour changes of wood surfaces. Holz Roh Werkst 67:141–14910.1007/s00107-008-0293-x ↗
30. Suits LD, Hsuan YG (2003) Assessing the photodegradation of geosynthetics by outdoor exposure and laboratory weatherometer. Geotext Geomembranes 21:111–12210.1016/S0266-1144(02)00068-7 ↗
31. Tolvaj L, Faix O (1995) Artificial aging of wood monitored by DRIFT spectroscopy and CIE L*a*b* color measurements. Holzforschung 49:397–40410.1515/hfsg.1995.49.5.397 ↗
32. Tolvaj L, Mitsui K (2005) Light source dependence of the photodegradation of wood. J Wood Sci 51:168–47310.1007/s10086-004-0693-4 ↗
33. Tolvaj L, Mitsui K (2010) Correlation between hue angle and lightness of light irradiated wood. Polym Degrad Stab 95:638–64210.1016/j.polymdegradstab.2009.12.004 ↗
34. Valet A (1996) Lichtschutzmittel für Lacke. Vincentz, Hannover