journal article·2010-08Open access

Exploratory study on the impregnation of Scots pine sapwood (Pinus sylvestris L.) and European beech (Fagus sylvatica L.) with different hot melting waxes

G. Scholz, A. Krause, H. Militz

Wood Science and Technology· Volume 44· Issue 3

Abstract

Scots pine sapwood ( Pinus sylvestris L.) and beech ( Fagus sylvatica L.) were impregnated with five waxes. The experiments indicate deep penetration into pine sapwood. Besides the viscosity, an influence of the wax polarity is presumed. Wax penetrates pine wood deeply via the cross-section, but not sufficiently enough to impregnate longer construction elements. However, the radial wax uptake exceeds the uptake via the tangential orientation and guarantees complete soaking of the sapwood tissue. The lateral wax penetration within beech is quite low and irregular. In addition to the temperature, a prolonged process procedure is decisive for an increasing wax uptake. As such, beech wood vessel elements seem to be fully impregnable via the longitudinal surface after a longer process procedure.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Plant Water Relations and Carbon Dynamics · Forest ecology and management · Tree-ring climate responses

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (30)

Show source-provided references
1. Atkins PW (1993) Einführung in die Physikalische Chemie. VCH, Weinheim
2. Bellmann H (1987) Zur Bedeutung der Holzfeuchte bei der Kesseldrucktränkung von Nadelhölzern. Holz-Zbl. (126) 1857, 1858, 1862; (143) 2201–2203 (151) 2312, 2314, 2316
3. Borgin K, Corbett K (1970) The stability and weathering properties of wood treated with various waxes. Plast Paint Rubber 14:69–72
4. Braun HJ (1970) Funktionelle Histologie der sekundären Sproßachse. Das Holz. Handbuch der Pflanzenanatomie, vol. 9, part 1. Bornträger, Berlin Stuttgart
5. Bub-Bodmar F, Tilger B (1922) Die Konservierung des Holzes. Parey, Berlin
6. Buro A, Buro EA (1959) Beitrag zur Kenntnis der Eindringwege für Flüssigkeiten in Kiefernholz. Holzforschung 13:71–7710.1515/hfsg.1959.13.3.71 ↗
7. Feist WC, Mraz EA (1978) Protecting millwork with water repellents. Forest Prod J 28:31–35
8. Fengel D, Wegener G (2003) Wood-chemistry, Ultrastructure, reactions. Remagen, Kessel
9. Grosser D (1977) Die Hölzer Mitteleuropas. Springer, Berlin10.1007/978-3-642-66576-9 ↗
10. Hackbarth W (1978) Untersuchungen über einige Grundlagen der Kesseldruck-Imprägnierung von Fichtenholz. Holz Roh- Werkst 33:97–9910.1007/BF02607014 ↗
11. Illmann G, Schmidt H, Brotz W, Michalczyk G, Payer W, Dietsche W, Hohner G, Wildgruber J (1983) Wachse. In: Bartholomé E, Ullmann F (eds) Ullmanns Enzyklopädie der technischen Chemie, Verlag Chemie, vol 24. Wachse bis Zündhölzer, Weinheim
12. Ivanovszky L (1965) Strukturmodelle der Wachse. Fette Seifen Anstrichm 67:762–76910.1002/lipi.19650671006 ↗
13. Kollmann F (1951) Technologie des Holzes und der Holzwerkstoffe, vol 1. Springer, Berlin Göttingen München
14. Liese W (1957) Der Feinbau der Hoftüpfel bei den Laubhölzern. Holz Roh Werkst 15:449–45310.1007/BF02613207 ↗
15. Middleton TM, Butterfield BG (1990) Vessel length distribution in the stems of three New Zealand species of Nothofagus. Wood Sci Technol 24:17–2210.1007/BF00225305 ↗
16. Militz H, Mai C (2008) Holzvergütung. In: Wagenführ A, Scholz F (eds) Taschenbuch der Holztechnik, Hanser, pp 485–500
17. Mundigler N, Rettenbacher M (2005) Natwood technology—A material thermal wood modification. In: Hill CAS, Militz H (eds) Proceedings of the second European conference on wood modification, Göttingen, pp 270–275
18. Murmanis L, Chudnoff M (1979) Lateral flow in beech and birch as revealed by the electron microscope. Wood Sci Technol 13:79–8710.1007/BF00368601 ↗
19. Scheiding W (2007) Weiterentwicklung eines Verfahrens zur Herstellung von wachsimprägniertem Thermoholz; Untersuchung der Holzeigenschaften und Ableitung von Einsatzmöglichkeiten, Final report, DBU-AZ 22257
20. Scholz G, Krause A, Militz H (2009) Capillary water uptake and mechanical properties of wax soaked Scots Pine. In: Englund F, Hill CAS, Militz H, Segerholm BK (eds) Proceedings of the fourth European conference on wood modification, Stockholm, pp 209–212
21. Scholz G, Van den Bulcke J, Boone M, Zauer M, Bäucker E, Militz H (2010a) Investigation on wax impregnated wood. Part 1: microscopic observations and 2D X-ray imaging of distinct wax types. Holzforschung, in press10.1515/hf.2010.091 ↗
22. Scholz G, Krause A, Militz H (2010b) Beeinflussung der Holzfestigkeit durch Wachstränkung. Holztechnologie 51:30–35
23. Sell J (1977) Hydrophobierende Holzimprägnierung—Wirkungsweise, Eigenschaften, Anwendungsmöglichkeiten. Holz Roh Werkst 35:75–7810.1007/BF02608139 ↗
24. Siau JF (1984) Transport processes in wood. Springer, Berlin10.1007/978-3-642-69213-0 ↗
25. Skene DS, Balodis V (1968) A study of vessel length in Eucalyptus obliqua L′Herit. J Experimental Bot 19:825–83010.1093/jxb/19.4.825 ↗
26. Suchsland O (1958) Über das Eindringen des Leimes bei der Holzverleimung und die Bedeutung der Eindringtiefe für die Fugenfestigkeit. Holz Roh- Werkst 16:101–10810.1007/BF02615415 ↗
27. Unger A, Schniewind AP, Unger W (2001) Conservation of wood artifacts. Natural science and archeology. Springer, Berlin10.1007/978-3-662-06398-9 ↗
28. Wagenführ R (1984) Anatomie des Holzes. VEB, Leipzig
29. Wagenführ R (2007) Holzatlas. Hanser, Leipzig
30. Wittmann J (2000) Physik in Wald und Flur. Deubner, Köln